The watchmakers' hand book
The Project Gutenberg eBook of The watchmakers' hand book This eBook is for the use of anyone anywhere in the United States and most other parts of the world at no cost and with almost no restrictions whatsoever. You may copy it, give it away or re-use it under the terms of the Project Gutenberg License included with this eBook or online at www.gutenberg.org. If you are not located in the United States, you will have to check the laws of the country where you are located before using this eBook. Title: The watchmakers' hand book intended as a workshop companion for those engaged in watchmaking and allied mechanical arts Author: Claudius Saunier Editor: Henry G. Abbott Release date: September 10, 2025 [eBook #76850] Language: English Original publication: Chicago: Geo. K. Hazlitt & Co., 1892 Other information and formats: www.gutenberg.org/ebooks/76850 Credits: Aaron Adrignola, Sharon Joiner, A Marshall and the Online Distributed Proofreading Team at https://www.pgdp.net (This book was produced from images made available by the HathiTrust Digital Library.) *** START OF THE PROJECT GUTENBERG EBOOK THE WATCHMAKERS' HAND BOOK ***
The Project Gutenberg eBook of The watchmakers' hand book
This eBook is for the use of anyone anywhere in the United States and
most other parts of the world at no cost and with almost no restrictions
whatsoever. You may copy it, give it away or re-use it under the terms
of the Project Gutenberg License included with this eBook or online
at www.gutenberg.org. If you are not located in the United States,
you will have to check the laws of the country where you are located
before using this eBook.
Title: The watchmakers' hand book
intended as a workshop companion for those engaged in watchmaking and allied mechanical arts
Author: Claudius Saunier
Editor: Henry G. Abbott
Release date: September 10, 2025 [eBook #76850]
Language: English
Original publication: Chicago: Geo. K. Hazlitt & Co., 1892
Other information and formats: www.gutenberg.org/ebooks/76850
Credits: Aaron Adrignola, Sharon Joiner, A Marshall and the Online Distributed Proofreading Team at https://www.pgdp.net (This book was produced from images made available by the HathiTrust Digital Library.)
*** START OF THE PROJECT GUTENBERG EBOOK THE WATCHMAKERS' HAND BOOK ***
TRANSCRIBER’S NOTE
Italic text is denoted by _underscores_.
Bold text is denoted by =equal signs=.
Underlined text is denoted by __double underscores__.
Overlined text is denoted by @at symbols@. Overlines from square and
cube root notations (²√ and ³√, respectively) have been omitted.
Footnote anchors are denoted by [number], and the footnotes have been
placed at the end of the chapter.
A superscript is denoted by ^x or ^{xx}, for example und^r or 36^{th}.
Some minor changes to the text are noted at the end of the book.
This edition of the book did not include a Table of Contents. For
the convenience of the reader one has been created here:
Preface.
Index.
Part I. Arithmetic, Geometry, Drawing, Etc.
Arithmetic.
Some Signs Employed in Calculations.
Powers and Roots.
Proportion.
Elements of Practical Geometry.
Geometrical Drawing.
Drawing Instruments.
Geometrical Drawings.
the Micrometrical Dividing Table.
Other Methods of Dividing Into Equal Parts.
to Subdivide a Circle.
Time.
Part II. Materials Employed in Horology.
Iron.
Cast Iron.
Steel.
General Observations.
Special Observations.
Determination of the Qualities of Steel.
Preparations of Steel.
Hardening.
Tempering.
to Whiten and Blue Steel.
Case-hardening.
Influence of Foreign Metals and Metalloids on the
Qualities of Iron and Steel.
Copper.
Zinc.
Brass.
Hammer Hardening of Brass.
to Anneal Brass.
Cast Brass.
Tin.
Bronze.
Sterro.
Lead.
Nickel.
German Silver.
Gold.
Silver.
Aluminium and Aluminium Bronze.
Mercury.
Platinum.
Palladium.
Characteristic Properties of Alloys.
Soldering.
Methods of Soldering.
Bronzing.
Gilding.
Acids and Salts.
Oil.
Alcohol.
Benzine, Etc.
Polishing Materials.
Preparation of Polishing Materials.
Smoothing.
Smoothing of Brass.
Smoothing of Steel.
Polishing.
to Polish Steel.
Cement, Wax, Resin, Etc.
Enamel.
Precious Stones.
Working in Precious Stones.
Part III. Health and Manipulation.
Preservation of Health.
the Sight.
the Body in General.
Use of the File and Graver.
to File Flat and Square With Both Hands at Once.
to File Flat With One Hand.
to Turn Cylindrical Pivots, Etc., and Square Shoulders.
Part IV. Tools and Appliances.
Workshop Fittings.
the Lathe.
the Foot Wheel.
the Bench.
Idlers.
Chucks.
the Slide Rest.
Gravers and Other Hand-turning Tools.
Drills.
Lathe Attachments.
Miscellaneous Small Tools.
Accessories and Miscellaneous Operations to Be Performed in the
Universal Head.
to Center an Object.
Uprighting and Drilling.
Production of Screw Threads. Screw Plates and Taps.
Taps.
Methods of Tapping Holes.
Rapid Mode of Making a Screw.
Screw-head Tools.
Tools For Cutting and Rounding-up the Teeth of Wheels.
Wheel-cutting Engine.
Cutters For Forming the Teeth of Brass Wheels.
Mill Cutters For Steel.
Tool For Making Cutters.
Tools For Correcting the Form of Teeth.
to Test the Accuracy of Certain Tools.
Part V. Repairing and Examining Watches.
Method.
External Examination of the Watch.
to Examine a Geneva Movement.
Accessories For Beginners.
Cleaning the Watch.
Putting the Watch Together.
to Examine English Or American Movements.
to Rapidly Time a Watch Or Clock.
Timing in Positions. Horizontal and Vertical.
Note on the Proportions of Balances.
Demagnetizing.
Part VI. Practical Recipes.
the Plate.
the Barrel. Including Arbor, Stopwork, Mainspring, Etc.
the Mainspring.
the Fusee.
Chain.
Wheels.
Pinions.
Set-hands Square.
Pivots.
Bushing Pivot Holes, Etc.
Depths.
on the Application of the Geometrical Laws of Depths to Practice.
Pallets.
Cylinder.
Balance Spring.
Dial Plate.
Metal Dials.
Hands.
Glasses.
Broaching.
Solid and Hollow Squares.
to Straighten a Rod, Plate Or Wheel.
American Watch Tool Co.
STONEY BATTER WORKS,
Chymistry District, WALTHAM, MASS.
[Illustration]
MAKERS OF THE CELEBRATED
WEBSTER-WHITCOMB LATHE
AND ATTACHMENTS.
Do not be deceived by an “IMITATION” when you can get the
Genuine Webster-Whitcomb for $36.00.
By the introduction of special and costly tools we have brought the
price of Lathes down from $80.00 in 1876, to $36.00 in 1894. Who has
done more for the craft than we?
SEND for Price List and NOTE reductions.
Remember our full address.
BENJ. ALLEN & CO.
141-143 STATE ST., CHICAGO, ILL.
Watch Materials, Tools and
__Jewelers’ Supplies__.
THE MOST COMPLETE STOCK.
LOWEST PRICES. BEST GOODS.
[Illustration: DIAMOND PIN TONGUES
Extra Quality
Manufactured Expresssly for
BENJ. ALLEN & CO,
141 & 143 State Street Chicago, Ill.]
“Diamond” Brand Pin Tongues, put up in neat box, partitioned off, each
size separate, warranted the best and stiffest Pins in the market, per
gross - =$1.00=.
_All Orders Filled Accurately and
Without Delay._
SEND FOR ILLUSTRATED CATALOGUE.
Watches, Clocks, Diamonds,
Jewelry and Silverware.
THE
WATCHMAKERS’ HAND BOOK
INTENDED AS A WORKSHOP COMPANION FOR THOSE ENGAGED
IN WATCHMAKING AND ALLIED MECHANICAL ARTS
BY CLAUDIUS SAUNIER
ILLUSTRATED AMERICAN EDITION
REVISED AND ENLARGED BY
HENRY G. ABBOTT
WITH SPECIAL REFERENCE TO THE WANTS OF AMERICAN WORKMEN
CHICAGO:
GEO. K. HAZLITT & CO., PUBLISHERS.
1894.
COPYRIGHTED 1892, BY GEO. K. HAZLITT & CO.
PREFACE.
M. Saunier’s writings occupy an unique position in Europe, as works of
reference for all who are engaged in watchmaking, and it may not be out
of place to observe that the American edition of his treatise promises
to take a similar place among English-speaking communities.
A glance at the index will show that the information given is
essentially practical in its character, and such as will be of use to
the watchmaker in his daily work. The volume is thus in no sense an
abridgment of the original edition, but on the contrary, it contains
much more matter than the original work.
In recent years the work of the ordinary watch repairer has undergone
considerable change. The apprenticeship he serves, if indeed it can be
called a real apprenticeship, is shorter than formerly. The immense
number of badly constructed watches that he is called upon to put in
going order for a trifling remuneration, compels him to replace the
older methods of procedure by others, whenever by so doing time can
be saved. From this point of view, then, the value of the present
Hand Book can hardly be over-estimated, since it contains, in a
readily accessible form, many details as to the working of metals, and
descriptions of various practical operations, new and improved forms of
tools, etc.
But the volume will be found of daily use to a wider circle of workers
than those above referred to. We believe that there is hardly a
branch of the watchmaking trade which may not benefit by the numerous
practical details that are given; indeed, although the work is
specially designed for the use of watchmakers, a great portion of it
will be seen to be no less applicable to other mechanical arts.
M. Saunier’s original works, the _Guide-Manuel de l’Horloger_, and
_Recueil des Procedes Pratiques_, which appeared as separate volumes,
have been incorporated in this American edition, a large amount of
additional information being at the same time added. As the second
contained many details that more properly belonged to the first, and
_vice versa_, it has been thought desirable to remodel the whole, and,
as will be seen from an examination, the six parts that constitute the
work are distinct in their character.
With a view to further facilitate the use of this Hand Book as a work
of daily reference, an unusually full index has been added, which the
reader is recommended in all cases to consult, and no effort has been
spared to make the cross references in the body of the work as complete
as possible.
It seems desirable here to give some explanation in regard to several
of the practical methods described. Every watchmaker will at once
recognize that recipes are included which are of the nature of
makeshifts, and that it would in many cases be better to replace a
piece by a new one rather than to repair it in the manner indicated.
But, on the other hand, it has been felt that the work will often be
appealed to by those who, from various circumstances, may be prevented
from making or procuring a new part that will suit the watch under
repair, while those who are not so situated will have no difficulty in
deciding for themselves as to which method to adopt.
The original work of M. Saunier, and the English edition, both had the
illustrations in the back of the work, which necessitated considerable
inconvenience when consulting them. In this edition we have ventured
to insert the illustrations in the text that describes them. The
antiquated tools, like the bow, bow-lathe, the turns and mandril,
have been omitted, and the modern foot-wheel, lathe and accessories
substituted.
HENRY G. ABBOTT
INDEX.
_NOTE—The references are in all cases to the pages, not to the
paragraphs._
A
Accuracy of tools, to test, 366
” ” rules, to test, 33
Acids, 127
Adjusting rod, to use, 433
Agate, 164
Akerman on hardening, 77
Alcohol, 132
” and glycerine on oilstones, 192
Alloys, 57
” properties of, 108
” that melt at certain temperatures, 82
Alum, 128
Aluminium, 103, 110
” bronze, 104, 110
” solders, 113, 116
Amalgams, 105
American chucks, 224
Ammonium, chloride of, 128
Angle of cutting edges, 235
Angles of escapement, to measure, 465
” measurement of, 26
” to construct equal, 44
” to subdivide, 44
Annealing brass, 96
” steel, 72
Anvil, to harden face of, 88
Appliances for watchmakers, 189
Aqua Regia, 127
Arbor, barrel, to make, 409, 420
” ” ” repair, 428
” ” ” true, 429
” chuck for wheel-cutting, 224, 337
” to straighten, 505
” nut, to drill, 425
” ” diameter of, 425
” set-hands, to adjust, 451
” ” ” tighten, 294
Area, measurement of, 25
Arithmetic, importance of, 17
Arithmetical ratio, 22
Automatic blow-pipe, 201
Ayr stone, 135
Axis of crystallization, 166
B
Back rests, 253
Balance, pivots, form of, 400
” poise of, 401
” protector, 265
” spring stud index, 280
” to make plain, 436
” vibrations of, 460
Balances, proportions of, 401
Balance spring, action of, 473
” ” collet tool, 286, 474
” ” gauge, 475
” ” to center, 377
” ” ” clean, 384
” ” ” draw, 47
” ” ” flatten, 477
” ” ” select, 478
” ” ” weaken, 477
Balance-springs, palladium, 107
” ” platinum, 107
Balas ruby, 162
Bands, 219
Barrel-arbor, to make, 409, 420
” ” ” repair, 428
” ” ” true, 429
” cover, to make, 410
” going, to put together, 385
” hole to bush, 412
” hook, to fix, 411
” clock, to make, 420
” to examine, 379
” ” make, 409
” ” oil, 388
” ” repair, 379, 412
” ” true, 379, 413
” ” upright, 413
Bars, to make, 409
Baths for hardening, 78
Beaupuy burnishers and files, 195
Beat block, 266
Beginners, aids for, 381
Bell-metal, 98
Belts for lathes, 219
Bench, 189, 221
Bent pivot, to redress, 454
Benzine, 133, 384
Berlioz rounding-up cones, 362
Berzelius pastile, 498
Black polish on steel, 154
Bleaching silver dials, 487
Blow-pipes, 199
Blow-pipe, gas, 201
” automatic, 201
Blue polishing stone, 135
Blueing steel, 86
Board, arrangements of, 177, 189
“Body” of steel, 70
Borax as flux for soldering, 128
Bouchons, movable, 456
” to make, 298, 456
” ” rivet, 456
Brass, 90, 110
” cast, 86, 110
” dials, to silver, 491
” etc., drill blade for, 241
” influence of impurities on, 91
” plates, to harden, 92
” rods, to harden, 95
” to anneal, 96
” ” bronze, 121
” ” polish, 149
” ” select, 91
” ” smooth, 139
” wheel teeth, observations on cutting, 346
” wheels, to polish, 149, 135
Brazing, 119
Breguet spring, to set, 476
Broaches, 199
Broaching, 499
” a hole round, 499
Brocot method of hardening brass rods, 95
Broken screw extractor, 262
” ” to remove with alum, 128
Bronze, 98, 110
” aluminium, 103, 110
” to render malleable, 98
Bronzing, 120
Brush, to clean with, 383
Brushes, preparation of, 382
Buff leather, 133
Burnishers, 198
” Beaupuy, 195
” to re-face, 198
Burnishing brass wheels, 135, 149
Burnt iron, 58
Bushing barrel holes, 412
” pivot-holes, 456
C
Caliper, figure-of-8, 197
” for heights, etc., 197
” micrometer, 270
” pallet, 466
” rest, jeweling, 249
” vernier, 278
Camphorated oil, 131
Cannon pinion, to tighten, 449
Carbon in cast iron and steel, 60
Carnelian, 164
Case hardening, 88
Case, to examine, 389
Cast brass, 90
” iron, 60
” steel, 61
Castings, malleable, 61
Catgut bands, to join, 219
Cement, application of, 156
” steel, 62
Center of circle, to find, 44
Centers, to test truth of, 366
” various, 266
Center wheel, 379
” ” to oil, 388
Centering attachments, 253
” from circumference, 307
” in wax, 157, 314
” methods of, 305
” rods, 285, 385
Chain, fusee, to ease, 434
Chain hook, to rivet, 434
Chalk for cleaning, 382
Chamfering tools, 281, 283
Charcoal for polishing, 133
” used for smoothing, 133
Chinese bronzing, 121
Chloride of ammonium, 128
” of zinc as flux for soldering, 118
Chrysolite, 163
Chucks, 224
Circle, divisions of, 24
” sub-division of, 52
” to find center of, 44
Circular oil stones, 191
Circumference, ratio to diameter, 25
” to center from, 307
Cleaning brushes, 383
” files, 193
” gold or gilt objects, 125
” metal dials, 491
” nickel movements, 101
” rough steel, 75
” watches, 382
Clock barrel, to make, 420
” dials, to clean, 491
” hands, to blue, 86
” pinions, to polish, 443
” to time rapidly, 394
Closing barrel holes, etc., 295
Cocks, to make, 409
Colcothar of vitriol, 135
Cold gilding without mercury, 122
” hammering, 74, 92
Collet, balance spring, tool, 286
Coloring gold dials, 493
Compass, proportional, 37
Compasses, 196
Conductivity, 110, 112
Copper, 89
” alloys with gold, 102
” to bronze, 120
Cord of lathe, 219
Countershaft, 220
Counting vibrations, 394
Cover of barrel, groove for, 410
” ” ” to make, 410
Crocus, 135
Crossing out a wheel, 435
Crossings of wheel, to mark, 298
” to renew broken, 440
Crystallization, axis of, 166
Cube root, 20
Curb, to adjust, 415
Cutters, to adjust form of, 353
” for jewels, 165
” ” making grooves, etc., 312
” ” slide rest, 286
” ” steel wheels, 347
” ” teeth, various kinds, 339
” rose and star, 349
” rounding up, to make, 331
” tool for making wheels, 353
” to sharpen slide rest, 287
” wheel, to make, 339
Cutting a file, 194
” edge, angles of, 235
” faces of gravers, forms of, 239
” glass, 498
” wheels, observations on, 310, 348
Cylinder escape wheel, to test, 290
” to oil, 388
” ” pivot a, 454
” ” polish mechanically, 468
D
Dead smoothing, 143
” surface of gold, to restore, 126
Decantation, 136
Definitions, geometrical, 23
Degrees of circle defined, 24
Demagnetizing watches, 403
Density, 108
Depth caliper, 197
Depths, application of laws of, 458, 460
” in stem-wind work, 462
” theoretical and practical, 458, 460
” to ease, 365
” ” secure good, 457
” visible and invisible, to test, 377
Depthing tool, to test accuracy of, 368
Design, to transfer, 30
Dial, enamel, to cut hole in, 484
” ” ” drill, 480
” ” ” reduce diameter of, 486
” ” ” remove figure from, 486
” plate, to cut, 479
” to file hole in, 481
” ” remove enamel from back of, 482
Dials, enamel for, 160
” fixed by feet, 483
” ” ” screws, 482
” gold, to restore, 493
” metal, to clean, 491
” silver, to restore, 487
” to paint hours on, 495
” ” repair, 161
Diamond, 161
” drill, to use, 169
” ” and gravers, 162, 173
” for polishing, 162
” powder, drilling with, 168
” ” to prepare, 135
Diamantine for polishing, 134, 154
Diameter, ratio to circumference, 25
Dies for screw-making, 315
” ” wheel-making, 438
Dividing plate, 298
” scales, etc., 48
” table, micrometrical, 48
Dome, freedom of, 389
Douzieme gauge, 196
Draw-plate, 298
Drawing, geometrical, 28, 40
” instruments, 32
” scales, 33
” to reduce a, 40
Drawn steel, advantages of, 71
Drifting, 296, 415, 502
Drifts, to make, 296, 422
Drill, diamond, 162, 173
” rest, 267
Drilling a barrel-arbor, 423
” enamel dial, 480
” glass, 498
” in the lathe, 308
” lubricants for, 480
” precautions in, 242, 244
” tool, to test accuracy of, 366
” with diamond powder, 168
Drills for oil-cups, 281
” to make, 244
” ” mount diamond, 173
” various, 241
Duplex ruby-roller, to make, 173
E
Elasticity of steel, 70, 84
Electro-gilding, 124
Elements of practical geometry, 23
Elevation defined, 28
Ellipse, to draw, 46
Emery, 134
” paper, to make, 134
” wheels and sticks, 134
Enamel, 159
” false, 161
” to apply cold, 160
” ” remove from back of dial, 482
” dial, to cut hole in, 484
” ” ” drill, 480
” ” ” erase figure from, 486
” ” ” reduce diameter of, 486
” dials fixed by feet, 483
” ” ” by screws, 482
Endshake, 375
Endstone, to fix, 159
” ” make, 171
Engine, wheel-cutting, 330
English movement, to examine, 389
Engraved design, to transfer, 30
Epicycloidal depths, 459
Equaling file, to cut, 194
Erasing figure from enamel dial, 486
Escapements, action of, 376
” gauges for, 465
” play of pivots in, 452
” to examine, 391
” ” measure angles of, 465
” ” oil, 387
Escapewheel, clip for holding, 289
” to test, 290
” cock passage, to turn, 312
Essences for cleaning, 133, 384
Examining watches, 371, 389
Expansion, 109
Extracting broken screws, 128, 262, 317
” square root of numbers, 21
Eyesight, to preserve, 175
F
Face-plate, 257
” universal, 257
False ruby, 163
Figure-of-8 calliper, 197
File, to cut equaling, 194
” ” round-up teeth with, 363
” use of, 178, 193
Files, Beaupuy, 195
” to clean, 193
” ” renew, 193
” ” set in handles, 193
Filing block, 269
” fixture, 268
” flat, 179
” rest, 269
” square by hand, 179, 182, 500
Finger-piece, to make, 418
Flat filing, 179
” ” device for, 182
” polishing, tool for, 302
Fletcher furnaces, 201
Fluxes for soldering, 117
Foot-wheel, 218
Fourth wheel, uprighting of, 379
Fraise, Ingold, 362
Freedom of various parts, 378, 375, 391
Frosted surface on steel, to produce, 144
Frosting silver dial, 487
Furnace temperatures, table of, 78
Furnaces, wind and muffle, 201
Fusee, advantages of, 432
” to adjust, 433
” ” snail, 145
” watch, to examine, 389
Fusion, points of, 110, 112
G
Gauges, 196
” for balance-springs, 475
” ” escapements, 465
” movement, table of, 462
” registering, 274
” staff, 275
Geneva movement, to examine, 374
Geometrical drawing, 28
” proportion, 22
” ratio, 20
Geometry, elements of practical, 23
” importance of, 17
German silver, 100, 110
Gilding, 122
” bath, to prepare, 124
Gilt objects, to clean, 125
Glass, to cement, 157
” ” cut, 498
” ” drill, 498
” use of, 175
Glue, application of, 156
Glycerine and alcohol on oilstones, 191
Gold, 101, 110
” to clean, 126
” ” deaden surface, 126
” ” prepare in powder, 128
” copper alloys, 102
” ” dials, to restore, 493
” solders, 114, 116
” springs, 102, 478
Graduations of scales, etc., 49
Grain of steel, 68
Graining prior to gilding, 125
” steel, 144
Grammaire, 298
Gravers, diamond, 162
” to mount diamond, 162
” use of, 178
” various, 238
Grinder, traverse spindle, 258
Grindstone, 192
Groove, circular, to cut, 311
” for barrel-cover, to make, 410
” straight, to make, 312
” to turn, 312
H
Hairspring, _see_ Balance spring.
” stud index, 280
Hairspringing collet tool, 286
Hammer hardening, 68, 74, 92
Hand fitting pliers, 288
” holder, 287
” to enlarge hole in, 287
” ” set in position, 497
” turning tools, 238
Hands, freedom of, 373
” to blue, 86
” ” to redden, 497
” ” tighten, 287
Handles, to set tools in, 198
Hard steel, to drill, 243
” ” ” turn, 185
Hardening brass, 92
” gold spring, 478
” solutions, 77
” steel, methods of, 77
” ” precautions in, 79
” ” temperature for, 68, 81
Hardness of jewels, to test, 166
” ” steel, 82
” scale of, 111
Health, preservation of, 175
Heat, mode of applying, to temper, 84
” of furnaces, table of, 78
Homogeneity of steel, 68
Hone slates, 134
Holder, escape wheel, 289
” for watch-hand, 287
Holes, methods of tapping, 323
Hook, chain, to rivet, 484
” to fix in barrel, 411
Hooks for catgut bands, 219
Hooked gravers, 288
Hours, to paint on dials, 495
” wheel, freedom of, 374
Hydrochloric acid, 127
” ” flux for soldering, 118
Hydrofluoric acid, 127
Hydrogen in palladium, 107
I
Idlers, 222
Impurities in brass, their influence, 90
” ” steel ” ”, 88
Index, to ease, 478
Ingold fraise, 362
Inks for painting dials, 496
Instruments, drawing, 82
Involute depths, 458
Iridium, alloy with platinum, 107
Iron, cast, 60, 110
” for soldering, 118
” its properties and uses, 57
” oxides of, for polishing, 185
” to case harden, 88
” ” distinguish from steel, 57
” ” restore, 59
” wrought, 57, 110
J
Jewel in pallet, to advance, 463
” resetting tool, 299
” setting, cutters for, 137
” to find axis of, 166
” holes, thickness of, 400
” ” to make, 168
” ” ” set, 171, 298
” ” ” smooth and polish, 169
Jeweling caliper rest, 249
Jewelry, alloys used for, 102
” to clean after soldering, 126
Jewels, 161
” to select, 166
” working in, 165
K
Keyless pinion, to drift, 503
” winding depths, 392, 462
” ” wheel, to make, 441
” work, need of oil, 383
” ” to examine, 392
L
Lamps, 190
Laps for jewelers, 165
Lathe, 210
” attachments, 247
” belts, 219
” care of, 213
” simple form of, 211
” for jewel making, 165
” large size, 216
” to center rods in, 285, 305
” band, 219
Lead, 99, 110
” use of, in brass, 90
Leaves of pinions, to polish, 445
Leclerre’s vibration counter, 395
Left-handed screws, to make, 320
Lever escapement, to examine, 391
Lift, to measure, 465
Lines, to connect up, 45
” ” draw parallel, 43
” ” subdivide, 43
Liquation, 92
Local time, 54
Locking stones, to make, 172
Longitude, value in time, 55
Lubrication of whetstones, 191
M
Magnetism, to remove, 403
Mainspring, setting up, 385
” to blue, 86
” ” make eye, 431
” ” reduce height of, 432
” ” select, 432
Malleability, etc., of steel, 70
Malleable bronze, 98
” castings, 61
” nickel, 100
Materials used in horology, 57
Measurement, exact, 38
” of angles, 26
” ” triangles, squares, etc., 26
” ” various solid bodies 28
Melting points, 110, 112
Mercury, 105, 110
” to purify, 106
Metals, 57
” to cement, 156
Methylated spirit, 132
Micrometers, 196, 270
Micrometer screw, 39, 48
Micrometrical dividing table, 48
Mill cutters for steel teeth, 347
Milling fixture, 258
Minute wheel, freedom of, 374
” ” to cut, 310
Mixed oils, 131
Mortar for making diamond powder 138
Motion work, to examine, 374
Motive force, effect of variations in, 402
Movement, to examine English and American, 389
Movement, to examine Geneva, 374
Muffle furnace, 201
N
Natural steel, 62, 65
Nickel, 99, 110
” movements, 100
” to surface, 147
” ” render malleable, 100
” silver, 100, 110
Nitric acid, 127
O
Oil, 128
” application of, 387
” necessary in keyless work, 393
” retention of, at center pivots, 378, 386
” ” ” on acting surfaces, 132
” tests of quality of, 129
” to secure permanency in, 130
Oil-cup chamferers, 281
Oil-cups, observations on, 282
” to polish, 153
Oilsinks, 131
Oilstone, 135, 190
Oilstones, circular, 191
Oilstone dust, to prepare, 137
Oriental chrysolite, 163
” ruby, 162
” sapphire, 163
Oxides of iron for polishing, 135
P
Paillard’s balance-springs, 108
Painting dials, 495
Palladium, 107
” balance-springs, 108
Pallets, 463
Pallet-opening calliper, 466
” stone, to alter, 464
” ” ” cement, 159
” ” ” make, 172
” ” ” move, 463
Pallets, verge, to open or close, 467
” ” ” measure, 466
Paper used in cleaning watches, 385
Parallel lines, to draw, 42
Parallelogram, 27
Pendulum, counting vibrations of, 394
” spring, _see_ Balance-spring.
” vibrations of, 460
Permanency in oil, to secure, 130
Perpendicular, to erect, 41
Petroleum, use for cleaning, 384
Pewter, composition of, 99
Physical properties of alloys, 108
Pickling dials, 488
Pinion, cannon, to tighten, 449
” hollow, to replace pivot of, 453
” leaves, to polish, 445
” riveting tool, 294
” to drift keyless, 297
” ” increase or decrease, 444
Pinions, etc., cutters for, 349
” high and low numbered, 460
” sizes of, 443
” to make, 442
Pivot-holes, cleaning, 382
Pivot polisher, 250
” to bush, 456
Pivots, balance, length of, 377
” ” form of, 400
” center, 378
” play of, 378, 452
” replacing broken, 453
” to polish mechanically, 454
” ” redress bent, 454
” ” turn, 183
Pivoting a cylinder, 454
Plate, watch, to make, 407
Plates, brass, to harden, 92
” for screw-making, 315
” to straighten, 504
Plating, gold, 124
” silver dials, 491
Platinum, 106
” balance-springs, 108
” to solder, 131
Pliers, 196
” hand-fitting, 288
Poise of balance, 401
Polish, black, on steel, 154
Polisher, form of, 155
Polishing brass, 149
” circular grooves, 428
” cylinder lips, tool for, 468
” escape-wheel teeth, 153
” flat objects, 302
” jewel-holes, 168
” machine for pinions, 445
” materials, 133
” pivots in lathe, 454
” powders, to prepare, 136
” ratchet teeth, 427
” sinks and oil-cups, 153
” steel, 153
” stones, Cadot’s, 136
Positions, timing in, 399
Post, to adjust, 415
Powers of numbers, 20
Precious stones, 161
” ” working in, 164
Preservation of health, 175
Prime numbers, 18
Proportion of numbers, 22
” ” balances, 401
Proportional compass, 37
Protractor, 33
Puddled steel, 62
Pulleys, 222
Pumice-stone, 135
Punch, centering, 285
” riveting, 198
Putty powder, 135
R
Radius defined, 24
Railway time, 55
Ratchet, to renew barrel-arbor, 425
” ” smooth, 140
” ” snail, 141
” teeth, to cut in lathe, 310
” to polish, 427
Ratio, 25
Receipts for watchmakers, 407
Red-stuff, 135
Re-facing burnishers, 198
Registering gauge, 273
Regulating a clock, 398
” ” watch, 396
Renewing files, 193
Repairing watches, 371
Resetting jewels, 300
Resin as flux for soldering, 117
Resist for use in gilding, 125
Retention of oil on acting surfaces, 132
Riveting stake and punch, 198
Rods, brass, to harden, 95
” to straighten, 504
Roller remover, 264
” to make duplex, 173
Roots of numbers, 20
Rose cutters, 349, 357
Rottenstone, 135
Rouge, 135
Rough steel, to clean, 75
Roughing files, 193
Round hole, to broach, 499
Rounding-up attachment, 259
” ” cones, 362
” ” cutters, to make, 331
” ” teeth by hand, 363
” ” tools, 330, 359
Rubitine, 134
Ruby, 162
” false, 163
” roller, to make duplex, 173
Rust, to remove and to prevent, 58
S
Sal-amoniac as flux for soldering, 128
Salts, 128
Sapphire, 163
Sapphirine, 134
Scale, to remove, from steel, 75
Scales used in drawing, 33
Scratch-brushing, 125
Screw dies, 315
” head sinking tools, 260
” ” to smooth, polish and slit, 143, 301
” micrometer, 39
” plates, to make, 316
” ” and taps, 315
” rapid mode of making, 326
Screws, double and treble threaded, 381
” left-handed, 320
” to blue, 86
” ” make internal and external, 315
” ” extract broken, 128, 262, 317
” tray for, 381
Sealing-wax as cement, 155
Seconds circle, to fix, 484
” ” ” make hole for, 484
Sector, 36
Semi-cylindrical drill, 245
Series of holes, to drill, 309
Set-hands arbor, to adjust, 451, 294
” nut, to make, 449
” square, to make, 422, 449, 500
Setting jewel-holes, 171
” ” cutters for, 236
Set-square, to center with, 286
Sharpening cutters, 237
Shear steel, 62, 66
Shellac as cement, 155
Shoulders, cutters for making, 236
” gravers for turning, 239
” to polish square, 155
” ” turn square, 183
Sight, to preserve, 175
Signs used in calculations, 19
Silver, 103, 110
” dial, to restore, 487
” German or nickel, 100, 110
” solders, 114
” solution for dials, 490
” for plating, to apply, 492
” ” ” ” prepare, 491
Sinks in watch plate, 131, 281
” to polish, 153
Sinking tools, 281
Slates, hone, 134
Slide rest, 233
” cutters, 236
” ” to sharpen, 237
” turning with, 234
Sliding tongs, 196
Smoothing brass wheels, 149
” metallic surfaces, 139
Snailing, circular, 141
” steel, 145
” tool for, 146
Soap, application of, 383
Solders for various metals, 113
” hard and soft, 113
Soldering, 112
” fluid, 118
” fluxes used in, 117
” iron, 118
” methods of, 115
” to clean jewelry after, 126
Solid content, measurement of, 28
” geometry, 23
” squares, 500
Specific gravity, 110, 111
” heat, 110, 111
Spelter solders, 114
Spinel ruby, 162
Spiral, to draw, 47
Split chucks, 224
Spotting, circular, 141
” machine, 141
Spring, balance, 473
Springs, to blue, 86
Square hole, to drift a, 502
” measurement of, 26
” root, 21
” set hands, to make, 422, 449, 500
” shoulders, to turn, 183
” to file by hand, 500
” winding, to renew, 430
Squares, solid and hollow, 500
” to make, 422, 449, 500
Staff gauge, 275, 277
” to straighten, 505
Stake, riveting, 198
Staking tool, 293
Star cutters, 348, 357
” wheel, to true, 417
” ” sink, to make, 410
Steel, 61, 110
” characteristics of good, 63
” drawn, 70
” drill blade for, 242
” influence of impurities on, 88
” maximum elasticity of, 82
” precautions in hardening, 79
” preparation of, 72
” to anneal, 72
” ” braze, 119
” ” clean rough, 75
” ” determine qualities of, experimentally, 66
” ” distinguish from iron, 58
” ” polish, 153
” ” restore, 59
” ” snail, 145
” ” smooth, 143
” ” temper, 81
” ” turn hard, 185
” ” whiten, 84
” wheels, cutters for, 347
Stem wind pinion, to drift, 503
” ” wheels, to make, 441
Stepping device, 227
Sterro, 99, 110
Stone, pallet, to cement, 159
Stones for polishing, Cadot’s, 136
” precious, 161
” to make pallet, 172
Stool, 190
Stopping barrel holes, 412
” pivot-holes, 456
Stopwork, proportions of Geneva, 416
” to examine English, 389
” ” examine Geneva, 374
Straight groove, to make, 312
Straightening rods, etc, 504
Stud index, hairspring, 280
Studs, to remove, 291
Subdivision of angles, 44
” ” circle, 52
” ” lines, 43
Sulphuric acid, 127
Surfaces, smoothing of metallic, 139
Surfacing nickel movements, 147
Synchrometer, Guilmet’s, 398
T
Tailstock, 247
Tap, to increase diameter of, 323
Tapping holes, various methods of, 323
Taps for screw-making, 317
” left-handed screw, 320
Teeth, forms of, 365
” of escape wheels, to test, 290
” ” lever escape wheel, to polish, 153
” ” to cut, 330
” precautions in cutting, 341, 346
” steel, to polish, 427
” to renew in wheel, 439
” ” round up, 363
” ” true, 440
Temper, as indicated by blueing, 87
Temperatures, determined by melting alloys, 82
” determination of furnace, 82
” of furnace, approximate, 73
” of temper colors, 82
Tempering steel, 82
Tightening cannon pinions, 293, 449
” hands, 294
” set hands arbor, 294
Time, 54
” standard, 55
” to ascertain true, 54
Timing in positions, 399
” watches and clocks, 394
Tin, 97, 110
” solders, 114, 115
” use of, in brass, 90
Tinning surfaces, 119
Tool, form of, for turning, 238
” for balance spring collet, 286, 474
” ” closing barrel holes, etc., 293
” ” drifting, 296
” ” flat polishing, 301
” ” measuring verge pallets, 466
” ” polishing cylinder lips, 468
” ” ” pinion leaves, 445
” ” ” pivots, 454
” ” resetting jewels, 299
” ” riveting pinions, 293
” ” snailing, 146
” ” spotting, 141
” ” tightening cannon pinions, 293
” ” ” hands, 293
” ” ” set hands arbor, 293
Tools, ordinary small, 260
” need of good assortment, 187
” screw head, 329
” for hand-turning, 238
” ” making jewels, 165
” ” rounding up teeth, 359
” ” sinking screw heads, 260
” ” watchmakers, 189
” to set in handles, 193
” ” sharpen turning, 237
” ” test accuracy of, 366
” ” ” escape wheels, 290
Tool set, 237
Tongs, sliding, 196
Topaz, 164
Tourmaline plates, 167
Tracing, 30
” from dial, 495
Train, play of pivots of, 378
Trains of watches, usual, 394
Transferring, 30
Traverse spindle grinder, 258
Triangles, 26
Tripoli, 135
Trueing a barrel, 412
” ” ” arbor, 429
” ” star-wheel, 417
” ” wheel, 440
Truth of tools, to test, 366
Turning sphere, tool for, 241
” by hand, 238
” tools, forms of, 238
” ” to grind, 237
” velocity in, 235
” with either hand, 186
” ” slide-rest, 233
Turpentine, use of, in drilling, 480
” Venice, as flux for soldering, 117
Tweezers, 196
” for removing studs, 292
U
Universal face-plate, 256
” head, 256,303
Unlocking pallets, to make, 172
Uprighting a barrel, 413
” of center wheel, 378
” tool, to test accuracy of, 367
V
Velocity in turning, 235
Verge pallets, to measure, 466
” ” ” open or close, 467
” to straighten, 505
Vernier, 37
” caliper, 278
” gauge, 278
Vibrations of balance or pendulum, 460
” to count, 394
W
Watch-glass, to reduce, 499
” hand holder, 287
” ” to blue, 86
” ” ” tighten, 293
” plate, to make, 407
” to de-magnetize, 403
” ” time rapidly, 394
Watches, to clean, 382
” ” put together, 385
” ” repair and examine, 371, 389
” usual trains of, 394
Watchmakers’ bench, 221
” receipts, 407
Water, annealing steel in, 73
” of Ayr stone, 135
Watered surfaces on nickel, 147
” surfaces, to produce, 139
Wavy surfaces, to produce, 139
Wax chucks, 157, 230
” to set objects in, 157
Weight of balance, 401
Wheel, cutters, 258
” ” or punch, 438
” ” tool for making, 354
” ” to make, 340
” cutting engine, 330
” ” ” to divide a rule on, 50
” ” ” to polish in, 427
” foot, 218
” mode of holding in cutting, 337
” teeth, to cut in lathe, 336
” tooth, to renew, 439
” to divide, 333
” ” make steel, 441
” ” mark crossings of, 298
” ” rough out, 435
” ” straighten, 504
” ” true, 440
Wheels, arbors for cutting, 337
” identical, 438
” observations on cutting, 346
” steel, cutters for, 347
” to ease depths of, 365
” ” polish brass, 149
” ” repair, 439
Whetstones, 190
White smoothing, 143
Whiting, 136
Wind furnace, 201
Winding square, to make, 422
” ” ” renew, 430
Wire-drawing plate, 298
” gauges, 272
Work-bench, arrangement of, 189
Y
Yellow copper or brass, 90
Z
Zinc, 89
THE WATCHMAKERS’ HAND BOOK.
PART I.
ARITHMETIC, GEOMETRY, DRAWING, ETC.
ARITHMETIC.
=1.= We often hear the theory advanced that in this country, at the
present day, it is not necessary to have a knowledge of arithmetic,
geometry, drawing, etc., because our interchangeable system of
manufacturing watches, makes all knowledge in these lines superfluous,
and that without any knowledge of arithmetic or geometry a man may
become a thorough master of watchmaking. This is a mistake that too
many of our young men make. The fact that the leading watch factories
of the United States have adopted the interchangeable system, of course
lessens the number of parts which the repairer will have to make and
fit, but it by no means alters the situation as regards the repairing
of foreign-made watches, nor even the changing of American watches from
key to stem-winders. Without a thorough knowledge of arithmetic and,
at least, an insight into the principles of geometry, no young man can
hope to become a first-class watchmaker in the true sense of the word.
Without these accomplishments he will be deprived of the pleasure of
reading understandingly the best literature of the day, the works of
those who are best fitted to impart knowledge to the members of the
trade.
With a knowledge of geometry he will be able to comprehend the works
of the best authors, to ascertain the dimensions of solid bodies, and
be in a position to apply the rules that form the basis of linear
drawing. Every watchmaker, worthy of the name, should be able to make
and understand the drawing of any machine, or of any horological
instrument. Many inventors, and even ordinary workmen, would avoid a
large amount of hard work, often useless, and occupying much time, if,
instead of at once putting an idea into practice with brass and steel,
they were able as a preliminary, to make for themselves a correct
design drawn to scale.
=2.= It is taken for granted that the reader is familiar with the rules
of arithmetic at least, and we will touch upon some points in algebra
and geometry that it will be well to mention. Should the reader have
no knowledge of arithmetic, algebra and geometry, we would advise
him to take up these studies during his leisure hours, using some of
the standard text books for that purpose.[1] Besides possessing a
knowledge of prime numbers, numbers which have no divisors but unity
and themselves, the watchmaker should be able to determine the greatest
common measure of several numbers, a rule which is of great importance
in calculating a train of wheels that is complicated.
We shall confine our attention to the methods of extracting square
roots and proportions, the rules for which may have been forgotten,
owing to their being less frequently employed than the more common
rules of arithmetic; they are of frequent use in horology.
SOME SIGNS EMPLOYED IN CALCULATIONS.
=3.= The sign of addition is an erect cross, +, called _plus_, and when
placed between two quantities it indicates that the second is to be
added to the first. Thus, 5 + 3 equals 8.
The sign of subtraction is a short horizontal line, -, called _minus_,
and when placed between two quantities it indicates that the second is
to be subtracted from the first. Thus, 8 - 3 equals 5.
The double sign, ±, is sometimes written before a quantity to indicate
that in certain cases it is to be added and in others it is to be
subtracted. Thus 5 ± 3 is read 5 _plus or minus_ 3.
The sign of multiplication, ×, when placed between two quantities
indicates that the first is to be multiplied by the second. Thus, 3 × 5
equals 15.
The sign of division is a short horizontal line with a point above and
one below, ÷, and when placed between two numbers or quantities it
indicates that the first is to be divided by the second. Thus, 6 ÷ 2
equals 3.
The sign of equality is two short, horizontal, parallel lines, =,
representing the words equal to. Thus, 6 ÷ 2 = 3.
Inequality is denoted by the angle >, the opening always being toward
the larger number or quantity; thus, in 12 + 7 > 14, the sign >,
indicates that the sum of 12 and 7 is greater than 14, and the whole
expression is read, 12 plus 7 is greater than 14. The expression 9 < 4
+ 7 is read, 9 is less than 4 plus 7.
A parenthesis, (), denotes that the several numbers or quantities
included within it are to be considered together, and subjected to the
same operation. Thus, (10 + 4) × 3 indicates that both 10 and 4, or
their sum, are to be multiplied by 3.
A horizontal vinculum, ------, placed over the numbers or quantities,
is frequently used instead of the parenthesis. Thus, @2 + 4 + 6@ × 7 is
equivalent to (2 + 4 + 6) × 7.
Division is more usually indicated by a line between the two figures,
the dividend being written above and the divisor below the line. Thus,
¹⁶⁄₈ indicates division, the same as 16 ÷ 8.
Algebra is that branch of mathematics in which the operations are
indicated by signs or symbols, and the quantities are represented by
letters.
The sign of ratio consists of two points like the colon, :, placed
between the quantities compared. Thus, the ratio of _a_ to _b_ is
written _a_ : _b_.
The sign of proportion consists of a combination of the signs of ratio.
Thus,: :: :. The first two and last two dots are read _is to_, while
the four in the middle are read _as_. Thus, if _a_, _b_, _c_, and _d_,
are four quantities which are proportional to each other, we say _a_ is
to _b_ as _c_ is to _d_, and this is expressed by writing them thus:
_a_ : _b_ :: _c_ : _d_.
POWERS AND ROOTS.
=4.= The power of a number is the product formed by successive
multiplication of the same number by itself. Thus,
2 × 2 = 4, the second power or square of 2.
2 × 2 × 2 = 8, the third power or cube of 2.
2 × 2 × 2 × 2 = 16, the fourth power of 2, etc.
An exponent is a number written above a quantity, at the right-hand, to
indicate how many times the quantity is to be taken as a factor, as
6^3 = 6 × 6 × 6.
The root of a quantity is a factor which, multiplied by itself a
certain number of times, will produce the given quantity. Thus, in the
above examples 2 is the square root of 4 and the cube root of 8.
The radical sign, √, indicates that the root of the quantity placed
under it is to be taken, and the index of the root is expressed by a
little figure placed outside of the bend. If a square root the index
figure is usually omitted.
√4 = 2 or ²√4 = 2 and ³√8 = 2.
=5. Extracting the square root of whole numbers.= [2]
I. Point the given number off into periods of two figures each,
counting from the units place to the left. For example, we wish to find
the square root of 399424, we point it off thus: 39,94,24.
II. Find the greatest perfect square in the left-hand period, and write
its root for the first figure in the required root; subtract the square
of this figure from the first period, and to the remainder bring down
the next period for a dividend. Thus:
39,94,24(6
36
--
394
III. Double the root already found, and write the result on the left
for a divisor; find how many times this divisor is contained in the
dividend, exclusive of the right-hand figure, and place the result in
the root and at the right of the divisor. Thus:
39,94,24(63
36
--
123 394
IV. Multiply the divisor thus completed by the last figure of the root;
subtract the product from the dividend, and to the remainder bring down
the next period for a new dividend. Thus:
39,94,24(63
36
--
123 394
369
---
2524
V. Double the right-hand figure of the last complete divisor for a new
divisor, and continue the operation as before. Thus:
39,94,24(632
36
--
123 394
369
---
1262 2524
2524
PROPORTION.
=6.= It is often convenient to express the relations of qualities in
the form of a proportion and from the proportion derive an equation.
Ratio is the quotient of one number divided by another. Thus the ratio
of 30 to 6 is ³⁰⁄₆.
=7.= Proportion is the equality of ratios: Thus if ³⁰⁄₆ = 5 and ⁴⁰⁄₈ =
5 then we may state that ³⁰⁄₆ = ⁴⁰⁄₈ or the proportionality is usually
expressed (=3=) thus:
30 : 6 :: 40 : 8
and this constitutes what is called a geometrical proportion, and 30
and 8 are called the extremes and 6 and 40 the means.
=8.= The product of the extremes is always equal to the product of the
means. Thus: 30 × 8 = 6 × 40 = 240. Hence it follows that if we only
know three terms we can always determine the fourth, or unknown term,
which is usually represented by the letter _x_. Thus in the proportion
12 : 3 :: 16 : _x_
we find the product of the means, or 3 × 16 = 48; this product divided
by 12, the known extreme, gives us the value of _x_, or the unknown
extreme, as equalling 4.
=9.= If we know the two extremes and only one of the means the same
rule is applied. Thus in the proportion
20 : 5 :: _x_ : 25,
we have: 20 × 25 = 500. ⁵⁰⁰⁄₅ = 100, the value of _x_.
ELEMENTS OF PRACTICAL GEOMETRY.
=10.= The object of geometry is to measure the extent of bodies. A body
has three dimensions, _length_, _breadth_ and _thickness_, and one of
these latter is sometimes termed _weight_ or _depth_.
Either dimension taken by itself is measured by a straight line.
When the extent of a body is expressed by combining any two dimensions,
it is termed _area_ or _surface_, and when three are employed we obtain
the solid measure or _volume_.
_Plane_ geometry only takes cognizance of figures situated in one plane
or surface, and therefore only possessing two dimensions; _solid_
geometry, however, regards bodies as having all three dimensions.
Two lines are parallel when their distance apart is the same at all
points. The same is also applicable to parallel planes.
Two lines or planes meeting each other will form an _angle_. The point
at which they meet or intersect is termed the _apex_ or _summit_ of the
angle.
A straight line is _perpendicular_ or _at right angles_ to another
straight line, or to a plane, when all the angles which it makes with
that line or plane are equal.
A _circumference_ of a circle is a curved line _l c d f_ (fig. 1,)
such that all its points are equally distant from an internal point,
_o_, termed the _center_. The _circle_ is the space enclosed by the
circumference.
It will be noticed that in geometry these two words are distinguished,
although they are frequently referred to as identical. Thus, the rim of
a wheel or balance is generally termed a circle.
Two circles (_l c d f_ and _b r a_, fig. 1,) described from the same
center are said to be _concentric_. When their centers do not coincide
they are called _excentric_ with regard to one another.
Any portion of a circumference, such as _f n d_, is termed an _arc_ of
the circumference, or, more commonly an _arc of a circle_.
A _chord_ is a straight line, _f d_, which unites the two extremities
of an arc. When the chord passes through the center of a circle it is
termed a _diameter_.
The _radius_ of a circle or circumference is a straight line drawn from
the center to the circumference; and all the radii that can be thus
drawn are equal. A diameter is, then, always double the radius, and,
conversely, the radius, is always half the diameter.
A _tangent_ is a straight line that only touches a circumference at one
point, as _g l_ (fig. 1); whereas a _secant_ cuts the circle, as _i j_.
A circumference is assumed to be divided into 360 equal parts, termed
_degrees_. The degree is subdivided into sixty equal parts, or
_minutes_, and the minute into 60 _seconds_. These are respectively
symbolized by the marks ° ′ ″ placed at the right-hand top corner of
the figure.
Such an expression as 18° 30′ 15.5″ would, then, be read 18 _degrees_,
30 _minutes_, and 15.5 _seconds_.
=11.= =Ratio of the circumference to the diameter.= The diameter of
a circle is to the circumference as 7: 22; or, employing decimal
fractions, as 1: 3.14159 (a number which, in algebra, is always
represented by the Greek letter π.)
[Illustration: _Fig. 1._]
Knowing a diameter (D), the circumference, _x_, can be ascertained from
the proportion:—
1 : 3.14159 :: D : _x_.
Knowing a circumference (C), the diameter, _x_, can be determined from
the proportion:—
3.14159 : 1 :: C : _x_.
The latter proportion will also give the value of the radius, which is
half a diameter.
=12.= The _superficial area of a circle_ is equal to the circumference
multiplied by half the radius, or to the square of the radius
multiplied by 3.14159.
A _sector_ is the circle enclosed between an arc and two radii bounding
it, as _b_ O _r k_ (fig. 1.)
The area or surface of a sector can be ascertained by multiplying the
length of the arc by half the radius.
A _segment_ of a circle is the portion intercepted between an arc and
its chord, as _f d n_ (fig. 1.)
The surface of a segment, as _b k r s_, can be obtained by subtracting
from the area of the sector O _b k r_, the area of the triangle, _b r_
O (=15=).
=13.= _Ring._ To determine the surface of a flat ring, the area of the
inner circle must be subtracted from that of the outer circle; in other
words, take the difference between the areas of the two circles that
fix the inner and outer diameters of the ring.
The area of a flat ring can also be calculated by adding together the
internal and external diameters; then multiply the number so obtained
by their difference and by the decimal fraction 0.7854 (that is,
3.1415/4). The product will be the required area.
=14.= _Angles and their measurement._ When two lines meet one another,
they form an angle, as we have already seen. If we take the apex as the
center of a circle, the number of degrees intercepted between the two
straight lines gives a measure of this angle.
The angle measured by a quarter of a circumference, or 90°, is termed a
_right angle_.
An _obtuse_ angle is greater than a right angle, and an angle that is
less is termed an _acute_ angle.
=15.= =Triangles, squares, etc., and their measurement.= The triangle
or plane area enclosed within three straight lines joined two and two
together (A, B, C, fig. 2,) is said to be _rectangular_ when one of its
angles is a right angle; it is _equilateral_ when the three sides are
equal, under which circumstances the three angles are also equal; and
_isosceles_ when only two sides are of equal length.
The sum of the three angles of a triangle is always equal to two
right angles. If only two of the angles are known, it is thus easy to
determine the third.
_Similar_ triangles are characterized by the fact that their homologous
sides (that is, the sides opposite to equal angles) are proportional.
_Peculiarity of the right-angled triangle._ The square described on the
longest side, termed the _hypothenuse_ (B, fig. 2,) is equal to the
sum of the squares described on the two other sides. Hence, it follows
that, if the lengths of the two shorter sides are known, that of the
hypothenuse can be ascertained by extracting the square root of the
number formed by adding together the squares formed on these two sides
(=5=).
[Illustration: _Fig. 2._]
If the hypothenuse is known and one of the shorter sides, the third
can be determined by extracting the square root of the number formed
by subtracting the square of the known side from the square of the
hypothenuse.
The _surface of a triangle_ is determined by multiplying one of the
sides by half the perpendicular height of the angle opposite to this
side.
=16.= The _surface of a square_ or of an oblong or _rectangle_ (_a b
c d_, fig. 3) is equal to the product of the base multiplied by the
height.
The sum of the squares described on the four sides is equal to twice
the square described on a diagonal. This diagonal divides the rectangle
into two equal rectangular triangles.
=17.= The _surface of a parallelogram or lozenge_, a plane figure with
four sides, opposite pairs of which are parallel (_c f g d_ and _c i
j d_, fig. 3,) is equal to the product of one side multiplied by the
perpendicular height of the figure.
[Illustration: _Fig. 3._]
The sum of the squares described on the four sides of a parallelogram
is equal to the sum of the squares described on the two diagonals.
=18.= =Measures of various solid bodies.= The volume of a cube of
parallelopiped (that is, a body bounded by six four-sided figures,
every opposite two of which are parallel) is obtained by multiplying
the surface of the base by the height.
The _volume_ of a straight cylinder is the product of the surface of
the circle which forms its base into the height of the cylinder.
The _area_ of the curved surface of a cylinder is obtained by
multiplying the circumference of the circle forming its base by the
height.
The _volume_ of a tube or cylindrical ring of rectangular section, such
as the arbor-nut of a barrel, or the rim of a circular balance, etc.,
is equal to the product of the plane surface of its base (=13=) into
its height.
The _volume_ of a _right cone_ or of a _regular pyramid_ is the product
of the base into a third of the height.
The _surface_ of a _sphere_ may be determined by multiplying the square
of the diameter by 3.1416 (=11=).
The _volume_ of a sphere is equal to this surface multiplied by a third
of the radius.
GEOMETRICAL DRAWING.
=19.= An elementary knowledge of the art of drawing, an ability to
represent the outlines of objects by simple lines, is of the first
importance to the watchmaker.
Such a design is obtained by projecting on to one plane all the visible
points of the object represented.
Projection on a vertical plane gives an _elevation_; the object is
looked at from one side.
Projection on to a horizontal plane produces a _plan_; the object is
observed from above, thus giving a bird’s-eye view.
The projection of a point on a vertical or horizontal plane is the foot
of the perpendicular, from the given point on to the plane. Assume the
line _n m_ (fig. 4), to be fixed in space; its horizontal projection
will give _c d_, and its vertical projection, _r s_.
[Illustration: _Fig. 4._]
_Miscellaneous details._ When one portion of the object to be
represented is found to pass behind other pieces so that it cannot be
seen, the continuation is frequently indicated by dotted lines.
Surfaces that are situated in planes one behind the other are shaded,
the more deeply according as they are farther back. This shading
is produced by a number of parallel lines which may be vertical or
horizontal.
Parts that are in relief are indicated by projected shadows, or by
increasing the thickness of a line that would cast a shadow.
In order to distinguish the several shadings or to emphasize the lines
by which they are separated, it is a very usual, though not invariable
practice to assume the light to be coming from the left-hand upper
corner.
When drawing a square in relief, such as _a b c d_ (fig. 3), the lines
_c d b d_, will be made darkest; but if it is a recess, the lines _a
b_, _a c_ should be brought into prominence by means of dark lines.
[Illustration: _Fig. 5._]
These several directions will be found useful when a hole, any cavity,
a pin, a round object etc., has to be depicted, as in fig. 5. As a
general rule, the thick lines should indicate the position at which a
shadow would form, the light being assumed to fall on the drawing in
the manner indicated above.
A _section_ shows a body as it would appear if cut in two, and one
portion removed in order to expose the interior, as in fig. 6. A
section is indicated by a series of parallel lines drawn close together
and at an inclination of about 45° to the vertical.
[Illustration: _Fig. 6._]
In order to leave more room for important details, or to show objects
that are situated behind, a piece is often broken off by an irregular
line, as shown in that drawing.
Lines formed by a series of detached points sometimes serve as a means
of associating several figures representing the same object looked as
in different directions.
=20.= =Tracing and transfering.= These two operations are resorted to
when it is required to obtain one or more copies of a picture or design
already drawn.
Tracing consists in laying a piece of tissue or other translucent paper
over the drawing and copying it by following over the lines that are
visible with a pencil. Or ordinary paper can be used for the purpose,
providing it is not too thick, if the picture be placed against the
pane of a window or, what is more convenient, on a sheet of glass used
as a desk and illuminated from below. When either sheet of paper is too
thick to allow sufficient light to pass, one or other of the methods of
transfering indicated below must be resorted to.
=21.= This operation consists in reproducing a tracing on a separate
sheet of paper or on metal that is to be engraved. Either of the
following methods may be adopted:
1. The picture to be transferred is fixed to a table or drawing board
if tracing paper is to be used, or to a sheet of glass if only ordinary
paper is available. The lines are then traced with a black lead pencil
that must not be too hard. When this is finished it is laid, face
downwards, on a sheet of white paper, taking care that both sheets are
so fixed that they shall not slip. Apply pressure to the upper surface
by tapping with a small pad made on purpose and, at the same time,
gently rubbing. Experience will very soon show how hard the pad should
be. Now remove the tracing, still taking care to avoid any slipping,
and a faint reproduction of the design will be found on the lower sheet
of paper. It is only necessary to follow over the lines with India ink.
The figures will be reversed but a transfer with it in the original
direction may be obtained by inverting the picture and laying it on
glass so as to make a reverse tracing.
2. Lay the picture on a desk or drawing board and trace it with ink
on a very transparent sheet of paper. When the ink is dry, invert the
tracing and blacken the back with a No. 2 pencil. Now lay the tracing,
with the ink side uppermost, on a sheet of clean paper, taking care to
avoid slipping, and go over the several lines with an agate or metal
style, avoiding excessive pressure on account of the risk of tearing
the paper. On removing the upper sheet an impression will be found not
reversed. Go over all the lines with India ink and clean the paper with
India-rubber or stale bread.
_Observations._ The choice of paper and pencil is not a matter of
indifference. All kinds of paper do not receive an impression equally
well, neither do all pencils transfer with equal facility. The Faber
pencil No. 3, will generally be found best suited to such work.
In preparing drawings which you desire to preserve, as drawings of
escapements, etc., a good quality of light weight bristol board will
be found more desirable than the best drawing papers. White wedding
bristol, about two-ply in thickness, answers admirably, and India ink
lines drawn upon it will not spread as they often do on drawing papers.
The prepared liquid India inks now on the market are superior to any
you can prepare by grinding the sticks.
=22.= =To transfer an engraved design.= This method is available when
it is desired to obtain an impression, for example, of the engraved
surface of a watch case.
Procure some of the inks used by copper-plate engravers, or, in its
absence, ordinary stencil ink may be used. Taking a small quantity on
the end of the finger, tap it on the surface of a glass plate, in order
that the ink may be distributed, leaving only a small quantity evenly
spread over the finger: tap with the finger thus prepared over the
watch case long enough to make sure that all the surface in relief has
received some ink; take a piece of writing paper and, after slightly
moistening it, spread it over this surface. Lay above this a piece of
paper folded in four and pass over it in all directions any round body,
such as a small tool handle, and with some pressure; then raise the
papers without allowing them to slide.
If the operation has been carefully performed a very clear impression
will thus be obtained of the engraved surface. The relief will be black
and the hollows white, but, of course, the figure is reversed like
that in a looking-glass. If required in the right direction it must be
traced through to the other side of the paper.
DRAWING INSTRUMENTS.
=23.= It is needless here to describe the rule, set-square, =T=-square,
bow-compass, etc., as every one knows them.
_To verify the accuracy of a rule._ On a perfectly flat smooth surface
carefully draw, with the rule in question, a fine straight line. Then
turn the rule over, hinging it as it were on the line just drawn; if
quite straight the edge of the rule will exactly coincide with the
line, in this new position, throughout its entire length. Each edge
should be thus examined.
_To verify the accuracy of a set-square._ Having fixed an accurate
rule on a smooth surface, place one edge of the set-square against it,
and draw a line along the edge perpendicular to the rule; then, having
turned the set-square, hinging it on the line just drawn, bring it
against the rule and along the line. If the square is true the edge and
line will coincide throughout their length.
=24.= =The Protractor.= Fig. 7 represents a common form of this
instrument. It is made of horn, or, if of metal, the inner portion is
cut away, leaving only a base and a semicircular arc, which is divided
into 180 equal parts or degrees; a complete circle would therefore
consist of 360 such degree. The point indicating the center of the arc,
should be very small in order to facilitate the exact setting of it at
the apex of an angle.
[Illustration: _Fig. 7._]
When an angle has to be drawn with accuracy, the protractor is
unsuitable; it will be better to adopt one of the methods described at
paragraph =37=, or trigonometrical methods.
=25.= =Drawing scales.= When an object is represented by a drawing, if
the dimensions are the same as those of the object itself, or, rather,
as they would project on to a horizontal or vertical plane, the drawing
is said to be full size; but the object is generally represented either
on an increased or diminished scale, which is defined, the proportions
between all the parts being still, however, maintained the same.
With a view to avoid the many calculations that such a change would
involve, it is usual to employ drawing scales. The following notes will
sufficiently explain their construction and use.
Let it be required to reproduce a large drawing on a small scale, in
such a proportion that the dimensions are reduced in the ratio of 10 to
1.
[Illustration: _Fig. 8._]
Take a straight line of indefinite length, _a b_, fig. 8, and mark out
on it spaces equal to _a_ 1, which represents any measurement taken on
the original object; at _c_, the 10th division, draw a perpendicular,
and on it measure _c g_ equal to _a_ 1, or one-tenth of _a c_ and join
_a g_.
Through the points indicating the divisions into tenths draw lines
parallel to _c g_, and you will thus have a series of triangles, _d
a_ 1, _d′ a_ 2, _d″ a_ 3, etc., similar to the triangle _g a c_. In
virtue of a well-known property of such triangles (=15=), _d_ 1 will be
one-tenth of _a_ 1; _d′_ 2 one-tenth of _a_ 2; and so on.
Thus, if a measurement taken on the object, or on a large drawing, is
equal to _a x_, it will only be needful to turn the compass on the
point _x_ as a center, and to observe accurately the perpendicular
height, _x z_, to ascertain the corresponding measurement on the
reduced scale.
Such a scale can be employed to measure meters and decimeters, or feet
and inches (but in this latter case, it would have been necessary to
mark off 12 instead of 10 divisions from _a_). Since _a_ 1 might be
made to represent one metre; _a_ 2, two meters, etc., in virtue of
the principle of the triangle already referred to, _d_ 1 will be the
tenth of _a_ 1, and will therefore represent a decimeter; _d′_ 2 will
represent 2 decimeters, etc. The length required to represent, say 5.3
will be ascertained by taking the distance _a_ 5, to which the distance
_d″_ 3 is added. Similarly 6 feet 2 inches would be given by _a_ 6, to
which _d′_ 2 is added on a 12-division scale.
=26.= The following description of one of these decimal scales, which
is engraved on metal or ivory, and often included in cases of drawing
instruments, will suffice to enable any one to construct a scale on
this principle, that goes to a still further degree of accuracy,
measuring, for example, meters, decimeters and millimeters, or yards,
feet and inches.
[Illustration: _Fig. 9._]
Let A B, fig. 9, be a flat rectangular rule, divided throughout its
length by parallel equidistant lines into ten strips. At right angles
to these are the lines _o o′_, _a a′_, etc., separated from one another
by a distance of one centimeter (doubled in the drawing in order to
make the details more clear.) The first centimeter is subdivided along
the two edges, A _o_, _n′ o_, into 10 equal parts or millimeters, and
the division, _o_, on the upper edge is joined by an oblique line with
the 1 on the lower edge, and the others by parallel oblique lines as
shown in the figure. Thus _c i_ will be one-tenth of a millimeter, _s
j_ two-tenths, and so on.
If the compass is opened so as to reach from _x_ to _z_, it will
be seen that it covers a space of 16 millimeters and 2-10ths of a
millimeter, for there are one large division (or 10 mm.), 6 smaller
divisions (or millimeters) plus a fraction of a millimeter equal to _s
j_ or 2-10ths of a millimeter.
=27.= =Sector.= When it is required to reduce the scale of a drawing,
subject to the condition that the dimensions shall be all diminished in
the ratio of two given lines, we may state the problem thus:
The longer of the two given lines is to the shorter, as any given
dimensions of the old drawing is to _x_. The value of _x_ thus
determined will be the corresponding dimension of the new figure.
Such a rule of three proposition would involve a considerable amount of
work, and the required result can be arrived at with greater facility
by the geometrical methods which forms the basis of the scale just
described, or, better still, by using the sector shown in fig. 10. It
consists of two brass or ivory legs hinged about a center _m_ which is
at the apex of the angle _n m c_ formed by two straight lines similarly
divided into equal parts.
[Illustration: _Fig. 10._]
It is employed as follows: Let us assume that a drawing has to be
reduced in the ratio of the line A to the line B; set off the length
A along _m n_, and suppose its extremity to be at _s_, where division
number 5 occurs. Open a compass to a distance equal to B, and placing
one point on _s_, open the two legs of the scale until the second point
coincides exactly with the corresponding division _t_, that is, with
the 5 on the other leg, _m c_. Maintaining the scale open to this
amount, it is only needful, after measuring a distance on the original
drawing or object, to set it off along _m n_, and to measure the
distance between its extremity and the corresponding point on the other
leg; this distance will be the dimension on the reduced scale.
=28.= =Proportional compass.= This consists of two equal stems
terminating with points, fig. 11. They are cut through for a portion of
their length, and provided with a slide forming a hinge, that can be
clamped by a screw _a_ in any position. Graduations on the two slots
and a mark on the slide indicate in what position of the slide _a_,
the length _a b_ (equal to _a g_) is equal to ½, ⅛, ¼, etc., of _a d_;
and thus show what is the ratio of _g b_ to _c d_, a ratio which is
independent of the extent to which the arms are opened.
[Illustration: _Fig. 11._]
=29.= =The vernier.= The vernier consists of a small graduated slide
which is adapted to a graduated rule or circular arc with a view to
ascertain the value of small fractional parts of the divisions marked
on the rule or arc.
Let A B, in fig. 12, be a rule divided into millimeters (the
proportions are enlarged in the drawing so as to avoid confusion among
the lines), and let it be required to determine a length to within the
tenth of a millimeter.
As the measurement is required to the tenth, take ten less one or nine
of the divisions of the scale; they will extend from O to IX, and this
represents the acting length of the vernier.
Subdivide the vernier into ten equal parts; it is manifest that each
graduation of the vernier differs from the original subdivisions of
the rule by 1-10th of a graduation of the latter. In other words, unity
on the vernier is equal to 9-10ths of unity on the rule.
[Illustration: _Fig. 12._]
When the rule and vernier are placed as shown in fig. 12, so that the o
on both scales coincide, the successive divisions on the rule (marked
with Roman numerals for distinction) will be progressively more and
more in advance of the corresponding divisions on the vernier in the
following proportion:—
The marks I and 1 are 1-10th apart; the marks II and 2, 2-10ths; III
and 3, 3-10ths; and so on, the mark X being 10-10ths, or one complete
division in advance of 10, this division being a unit on the scale.
Thus if the vernier is caused to slide along the edge of the rule, when
1 coincides with I the vernier has advanced 1-10th; when 2 coincides
with II, it has advanced 2-10ths; and so on.
Let it be required to determine the distance P _d_, fig. 13. The
division 6 on the vernier coincides with a division of the scale; hence
it follows that the extremity _d_ of the vernier is at a distance of
6-10ths millimeters from III, the next division of the scale to the
left. The distance between P and _d_ is thus 3.6 millimeters.
[Illustration: _Fig. 13._]
With a vernier showing tenths, if two consecutive divisions of the
vernier fall between two divisions on the rule, and there does not
appear to be a tendency towards one side more than towards another,
even when observed with a strong glass, it is possible to take an
approximate reading to the twentieth.
[Illustration: _Fig. 14._]
In measuring circular arcs a curved vernier is used in place of a
straight one, and its graduations are made to correspond with those on
the circle as shown in fig. 14.
=30.= =Micrometer screw.= By employing a micrometer screw it is
possible to measure infinitesimal amounts, but the screw must be
perfectly accurate, and must work without appreciable backlash or loss
of time.
[Illustration: _Fig. 15._]
Assume V, fig. 15, to be such a screw, having a pitch of 1 millimeter.
It will advance by this amount with each complete rotation.
To the head of the screw is attached a disc of such a size that its
rim can be divided into a number of equal parts, say a hundred. These
graduations may be marks on the edge or notches cut in it when an index
is required to stop in them; but the index is less frequently met with
than a simple divided straight-edge almost in contact with the disc.
The divisions round the disc are numbered in ascending order as the
points _c_ and _a_ separate, so that zero comes under the index or rule
when these points are in contact. Readings of the numbers will thus
afford a measure of the displacement of the point of the screw.
When the disc is rotated the point a will move towards or from _c_
by 1-100th of a millimeter for each division passing under the
straight-edge, and one millimeter for each complete rotation. It is
thus possible to obtain the dimensions of an object when it enters
without play between the two jaws to within an error of about 1-100th
of a millimeter if the instrument is accurately made.
If, instead of passing the object between the two jaws, it is gripped
by them, the measurement will be less exact, as no account is taken of
the pressure exerted and of the elasticity. (=44.=)
GEOMETRICAL DRAWINGS.
=31.= =Sketches.= It is advisable from an early age to accustom oneself
to make rapid freehand sketches of objects as they present themselves
to the eye. Such a sketch will help in the preparation of a more exact
drawing, which involves a knowledge of the several geometrical methods
given below.
A drawing may be transferred, reduced or enlarged as follows:
Draw across the original picture a number of equidistant vertical and
horizontal lines, forming perfect squares, and number the two sets of
lines in succession. Then draw a similar series of lines on a clean
sheet of paper, setting the lines at an equal, less or greater distance
apart, and copy in succession the parts of the figure that are enclosed
within the several squares.
As it is not always possible to draw lines across a figure, they may
be replaced by a frame carrying fine threads or wires stretched in the
two directions. The frame is laid over the original drawing, which can
then be copied, as above explained, on a sheet of paper divided into
squares (fig. 16).
[Illustration: _Fig. 16._]
The frame may, moreover, afford assistance in the drawing of solid
objects. Having placed it above or in front of the object and
in contact with it, copy on to the sectional paper the contents
of each corresponding square, taking care to look at the object
perpendicularly. With a little practice, and by placing the eye in
the correct position and always at the same distance from the frame
(a distance which may be regulated by a glass), a sketch in fair
proportion may easily be obtained.
[Illustration: _Fig. 17._]
=32.= =To erect a perpendicular on a straight line.= Either the compass
or a set-square can be employed; the use of the latter instrument is so
simple that no further reference need be made to it. Assume _a_, fig.
17, to be the point in the line _n m_ at which a perpendicular is to be
drawn. On either side of _a_ measure off equal distances _a n_, _a m_;
from _n_ and _m_, with a radius about equal to the distance _n m_, draw
two circular arcs cutting one another. If their point of intersection
_b_ be joined to _a_, the line _a b_ will be the required perpendicular.
[Illustration: _Fig. 18._]
=33.= =To erect a perpendicular at the extremity of a line.= From the
extremity _c_, fig. 18, mark off four equal parts towards _s_. From
_s_, with a radius equal to five such parts, describe a circular arc,
and from _c_, with a radius of three such parts, describe another
arc cutting the first at _d_. The line joining _c_ and _d_ will be
perpendicular to _s c_.
For the square of 5 is 25, and this is equal to the square of 4 or
16 plus the square of 3 or 9. Thus the triangle _s c d_ must be
right-angled (=15=).
[Illustration: _Fig. 19._]
Or the following method may be adopted: With any center _i_ and radius
_i g_ (fig. 19), as large as possible, describe a circumference passing
through _g_. From the point _p_, where the circle cuts the line, draw
the diameter _p i h_. If the point _h_ be joined to _g_, it is the
required perpendicular; for, by a property of the semicircle, the angle
_h g p_ is a right angle.
[Illustration: _Fig. 20._]
=34.= =To let fall a perpendicular on a straight line.= In order to
let fall a perpendicular from the point _a_ on to the line _b c_ (fig.
20), describe from _a_ as a center, a circular arc sufficiently large,
cutting the straight line in two points, _b_ and _c_. From these two
points, with the same opening of the compass, draw on the under side of
the line two arcs that intersect. The point of intersection _o_ joined
to _a_ gives the required perpendicular.
[Illustration: _Fig. 21._]
=35.= =To draw parallel straight lines.= Having fixed a good
straight-edge over the drawing, as many parallel lines as are required
may be drawn with the aid of a set-square which is caused to slide
along the rule. They will be vertical, horizontal or inclined,
according to the position of the rule, which must be set exactly
perpendicular to the direction in which the parallel lines are to be
drawn (fig. 21).
[Illustration: _Fig. 22._]
_To draw, from a given point, a line parallel to a given line._ Let _d_
be the given point, and _a b_ the given line (fig. 22). From _d_ draw
the circular arc _a c_, and from _a_ where it cuts _a b_, with the same
radius describe the arc _d b_. From _a_ set off on _a c_, a distance
equal to _d b_. The line joining _d_ and _c_ is the required parallel.
[Illustration: _Fig. 23._]
=36.= =To subdivide a line into equal parts.= Let it be required to
divide the line _p v_ (fig. 23), into five equal parts. Draw a line _p
q_ inclined at any angle, and mark off on this line five equal parts of
any length; join _q_, the extremity of the five lengths, and _v_, and
through the points _a_, _b_, _c_, _d_, draw lines parallel to _q v_. In
virtue of a property of similar triangles these lines will divide _p v_
into equal parts. It is advisable that the lines _p v_ and _p q_ should
not differ very considerably in length, as, otherwise the inclination
of the parallel lines to _p q_ will render it difficult to observe the
exact point of intersection.
[Illustration: _Fig. 24._]
_To divide a line into proportional parts._ The proposition can be
solved in a similar manner. Let it be required to divide a line _t r_
(fig. 24), into two sections that are to one another in the proportion
of 5 to 3. On _t s_ mark off a series of equal parts given by the
addition of these numbers together, that is 8; and join the last point
_s_ to _r_. Then draw through _c_, the fifth division, a line parallel
to _s r_. This line _c d_ will cut _t r_ into two parts, which are to
one another in the proportion of 5 to 3.
By an analogous construction a fourth proportional can be graphically
obtained, as already indicated in articles =25=-=27=.
=37.= =To construct an angle equal to a given angle.= The angle may be
measured by means of the protractor (=24=), which then enables us to
draw a similar angle; but greater accuracy is obtainable by using the
compass.
[Illustration: _Fig. 25._]
Let it be required to construct at _m_ on the line _m p_ (fig. 25), an
angle equal to _b a d_. With as large a radius as possible, draw from
the points _a_ and _m_ the arcs _b d_ and _n p_. Measure the distance
_d b_ and mark it off with the compass from _p_ on the arc _p n_. A
line drawn through _m_ to the intersection of the two arcs will give
the required angle equal to _b a d_.
=38.= =To subdivide an angle into 2, 4, or 8 equal parts.= In addition
to the use of the protractor, the following graphic method is often
given in works on geometry.
[Illustration: _Fig. 26._]
An angle _e f g_ being given (fig. 26), from its apex _f_ as a center
describe the arc _e g_, and from its two points of intersection with
the sides, with a radius greater than half their distance apart, draw
two short arcs cutting each other at _s_. A line drawn from _f_ through
the intersection _s_ will divide the angle into two equal parts.
If four divisions are needed, repeat the process on the two angles _s f
e_, _s f g_, and so on for a further sub-division.
The line that divides the angle into two equal parts will also bisect
or divide into two equal parts the chord and the arc _e g_.
[Illustration: _Fig. 27._]
=39.= =To find the center of a circle or of a circular arc.= Take on
the circumference, or on the arc, three points _b c r_ (fig. 27).
Join _b_ to _c_ and _c_ to _r_. At the middle point of each of these
lines[3] erect a perpendicular. The point of intersection of these
perpendiculars is the required center.
A similar method should be resorted to when it is desired to describe a
circle passing through three given points.
[Illustration: _Fig. 28._]
=40.= =To connect up or associate lines.= In order to join up a
straight line, such as _i j_ (fig. 28), with the curve _l p_, erect a
perpendicular at _j_, and through the middle point of a chord, _l p_,
draw a second perpendicular cutting the first in _k_. This point will
be the center from which the curve uniting the two lines should be
struck.
[Illustration: _Fig. 29._]
To unite a curve _a b_ (fig. 29), with another curve, _c x_ or _c
z_, at the point _c_, first find _o_, the center of the curve _a b_,
draw the line _a o_, continuing it beyond the center; join _a_ and
_c_, and erect a perpendicular at the middle point of this chord. The
intersection of this perpendicular with _a o_, produced if necessary,
should be taken as the center for a curve uniting _b a_ with _c_.
[Illustration: _Fig. 30._]
To join up two lines inclined to each other or parallel lines of
unequal length, such as _a r_, _b s_, fig. 30, draw midway between the
two another line, _z d_; join the two extremities _r_ and _s_, and from
these points let fall perpendiculars _r i_ and _s c_; then from _d_
draw a line perpendicular to _s r_. The point _o_ thus obtained will be
the center of the arc _r d_, and _c_ will be the center for _d s_.
=41.= =To describe an ellipse.= Let _a b_ (fig. 31), be the major axis
of the ellipse; divide it into three equal parts, and from the two
points, _c_ and _i_, at which it is divided, with a radius equal to _i
c_, draw (in pencil) two circles, intersecting in the points _x_ and
_z_. Through these points draw the lines _x i g_, _x c h_, _z i f_, _z
c d_.
With the center _z_ describe the arc _d f_, and from _x_ draw _h g_;
the ellipse will be completed by the two arcs, _f b g_, _d a h_, of the
primitive circles.
[Illustration: _Fig. 31._]
If it be required to describe an ellipse that shall have a shorter
minor axis, divide the major axis into four equal parts, thus obtaining
three points of sub-division. With each point as a center and with a
radius equal to one of the spaces describe circles. Those to the right
and left will determine the extremities of the ellipse, and the central
circle will intersect the minor axis in two points which must be taken
as centers for describing the top and bottom portions of the figure.
[Illustration: _Fig. 32._]
When the length of the long and short axes are given, proceed as
follows (fig. 32): From the center _a_, where they intersect at right
angles, mark off the distances _a n_, _a o_, equal to the difference in
the length of two semi-axes. Join _n o_, and add one half of _n o_ to
_a o_ measured in the direction of _a v_, thus obtaining the point _k_;
with the radius _a k_ describe a circle. On this circumference will lie
the four centers; _k_ for the arc _r u s_, _m_ for the arc _p v q_, _t_
and _i_ for the short arcs _q j s_, _p e r_.
The figures obtained by the methods here given closely resemble the
ellipse, but are not of the strict mathematical form. It is well
to acquire some facility in drawing ellipses, for the projection
of a circle on a plane, when the two are neither parallel nor
perpendicular, is an ellipse, and one often has occasion to describe it.
=42.= The following may be added as a mode of describing an ellipse:
The major axis and the two foci (points in this axis) being known, fix
two pins in these foci. Then tie a piece of string into a loop and
place it over the pins; stretch it with a pencil, the point of which
is on the paper, and on moving this around in a circular direction,
the string being maintained stretched, an ellipse will be described.
When the string is so stretched that it lies along the major axis, the
length should be such that the pencil is exactly at its end.
[Illustration: _Fig. 33._]
=43.= =To draw a spiral curve.= Draw four lines forming a small square
(fig. 33). The point _o_ is taken as the center of the first arc, _i
j_; _s_ is the center of _j k_; _u_ of _k l_; _i_ of _l n_. Then,
to continue the curve, _o_ is again taken as the center for _n p_,
and so on. This method produces a volute in which the coils are at a
considerable distance apart, such as has no special applicability to
horology.
[Illustration: _Fig. 34._]
As the balance-spring of a watch is partially concealed by other
pieces, it is generally sufficient to represent the parts that show
themselves by concentric circular arcs, or arcs described from two
centers. If a more accurate representation be required, the following
method may be resorted to: when working on a small scale it involves
the use of the eyeglass, for the figure (fig. 34,) here given is
exaggerated in order to avoid confusion in the lines, numbers, letters,
etc.
A small circle having been described, it is divided into an even
number of equal parts, say four; a less number than this should never
be adopted. From the same center describe another circle as small as
possible, which will be cut by the two diameters drawn between opposite
points of division numbered 1, 2, 3, 4.
Assuming _a_ to represent the starting-point of the curve, from the
center 1 with radius 1 _a_ draw the arc _a b_; from 2 with radius 2 _b_
draw the arc _b c_; from 3 with 3 _c_ draw _c d_; from 4 with 4 _d_
draw _d s_; then recommencing with 1 and the radius 1 _s_ draw _s f_,
and so on.
The less the radius of the small circle and the greater its number of
divisions, the closer will the successive coils be together. To secure
accuracy when working on a small scale, it is advisable that the center
and the several points be in a thin brass or horn plate, which is
maintained in position by steady pins.
THE MICROMETRICAL DIVIDING TABLE.
=44.= This instrument is no more than a simple application of the screw
to dividing straight lines, but it will suffice to enable the reader to
understand the principles on which the more complicated instruments are
based.
[Illustration: _Fig. 35._]
A plate, P, fig. 35, supports a bracket _a_, in which a screw, similar
to the one described in paragraph =30=, is engaged by means of a
collet; it rotates, being supported between this bracket and the small
bearing _b_, that receives the pivot at the end of the screw.
The screw is fitted carefully into a nut _n_, which is rigidly attached
to the small plate _h_; this carries a fine marker, movable on an axis,
and terminating with a chisel edge or a fine diamond point, according
as the instrument is to be used for engraving metal or glass; or it
may be provided with a fine pencil if the object is merely to make
subdivisions on a drawing.
This being understood, it will be evident that, if a rule or rod of
any form be fixed by screws or otherwise between _f_ and _g_, it can
be graduated by means of the marker, the screw being made to advance;
the millimeter screw can be used for dividing into millimeters and
fractions direct, or, with a little calculation, into fractions of an
inch. Each complete rotation of the head means a displacement of the
marker by a millimeter; a half turn will be half a millimeter, etc.
OTHER METHODS OF DIVIDING INTO EQUAL PARTS.
[Illustration: _Fig. 36._]
=45.= =First method.= Having fixed a sheet of drawing paper on a smooth
board, draw the line M N, fig. 36, longer than the rule which is
required to be divided. Then, with a compass or graduated scale, mark
off a series of equidistant points, commencing at N, equal in number
to the required series on the rule, and let M be the last division.
With the center N and radius N M describe the circular arc _p v_, and
with M as a center and the same radius, describe a second arc _r s_,
intersecting the first at O. Join O with M and N. Assume _a c_ to be
the rule that is to be divided into equal parts; slide it on the paper
parallel to M N until the extremities, _a_ and _c_, coincide with the
lines O M, O N, and are equidistant from O. This position can be easily
found by the aid of a compass with one of its centers at O. Now fix
the rule in position with sealing-wax, or by some other means, and,
with a firm upright pin, center the brass rule R at O, so that it can
rotate round this center on the pin as a pivot. It now only remains to
trace a series of lines O _k_, O _b_, O _d_, etc., with the rule, to
the division points of the line M N. The line _a c_ is thus divided
into as many equal parts as the line M N. The graduations will be all
the more exact according as the divisions of the line M N are longer.
=46.= =Second method.= By the side of the chuck of a wheel-cutting
engine, arrange a horizontal slide _y f_ fig. 37, that can travel
easily in a direction perpendicular to _a_ T. A watch fusee-chain, or
a very flexible spring, is fixed by one end to the chuck, and by the
other to the slide at _d_. The chain or spring is kept stretched by a
weight which tends to draw the slide from _f_ towards _d_.
[Illustration: _Fig. 37._]
The rule to be graduated, _a_, is now fixed on the slide, and an
initial division is marked on it with a pointed rotating cutter in the
position usually occupied by the wheel cutter, or else by striking a
small pointed or flat-edged chisel arranged for the purpose, in such a
manner as not to be liable to derangement.
Rotate the table through a definite distance; the rule _a_ will advance
through the same distance; mark the second division; then having moved
the division-plate through a distance equal to its first displacement,
mark the third graduation, and so on. Suppose, for example, that it be
required to make 30 divisions on the rule between _f_ and _d_; select
on the plate the circle corresponding to twice or thrice this amount,
so that the radius of the chuck may not be relatively too short, and
that the chain or spring may not act at a disadvantage; take the number
60 for example:
The two marks at _d_ and _g_ on the spring indicate the length that
corresponds to the straight line to be divided.
The chuck is placed in the lathe and reduced in diameter until the half
circumference is exactly equal to the distance between these two marks
on the spring, which thus fall on a diameter, _i g_, of the chuck.
The spring having been fixed by its two extremities, the slide with the
rule attached is placed in position, so that the mark _g_ is on the
line _a_ T; it will be evident from the figure that each displacement
of the division-plate through one-sixtieth of its circumference will
cause _a_ to advance through one-thirtieth of the space between _f_ and
_d_.
_Remarks._—Knowing the relation of a diameter to the circumference (as
1 : 3.1416), we can determine the diameter of the chuck at once by
calculation.
Its form should be a true cylinder, and it is well to place guides that
will prevent the spring or chain from assuming a helical position.
The side that carries the rule should be strictly perpendicular to _a_
T; and the portion of the spring that is not coiled on the chuck should
always be parallel to this slide.
The chuck and spring must be quite clean and smooth, and the latter
should be very pliable. A greater weight will be needed to keep
the spring stretched than will suffice for a chain, and it must be
increased as the strength of springs is greater.
The slide, _y f_, may simply travel over a horizontal surface between
pins planted in two parallel lines. But it would be preferable to adopt
some other method, for instance, to make this piece (F, fig. 37),
travel with a little friction along a perfectly true cylindrical rod.
=47.= =Third method.= This is merely an application of the arrangement
mentioned in paragraph =44=. The lathe can be employed for marking
off a series of equidistant points in a straight line. Knowing the
pitch of the slide-rest screw, determine the distance apart in, say,
millimetres, of the required divisions, and fix the rule perfectly flat
on the face-plate, which must be rendered immovable by any convenient
means. Then mark the first point with the drill-stock. Advance the
screw by the amount previously determined upon and mark the second
point. After withdrawing the drill, again advance by the same amount
and mark the third point, etc. Always be careful, before making the
first mark, that the screw has already traveled some distance in the
direction it will continue to move, so as to avoid backlash, or loss of
time.
TO SUBDIVIDE A CIRCLE.
=48.= =To divide the circumference into equal parts.= After having
drawn the circle, A, fig. 38, draw two diameters, _d a_, _b c_, at
right angles to each other, dividing the circle into four equal parts.
Join the points, _c a_, and divide the line, _c a_, accurately into
nine equal parts.
Draw a series of circles concentric with the first, at distances apart
equal to one of the divisions of _c a_, and to the number of one, two,
three, etc., according as it is required to subdivide the circle, say
for a pinion, into seven, eight, nine, etc., equal parts.
[Illustration: _Fig. 38._]
With a fine-pointed compass, measure off the radius of the initial
circle A. Placing one point of the compass at _c_, the other point
will give the position of the next leaf, and so on, all around the
circumference. If the innermost circle A be selected for sub-division,
six divisions will be obtained, and there will be one more division for
each larger circle.
The operation will be facilitated by selecting the first circle, so
that the line _a c_ contains exactly nine divisions equal to those of
some scale that is accessible. Such a circle can be easily found, by
first drawing the two diameters, laying the scale in the direction _c
a_, and determining by trial the radius for which the first and ninth
divisions correspond to _a_ and _c_ respectively.
=49.= =To divide a surface into rings of equal or proportional
superficial area.= The following solution is due to M. Brocot:
Let _a d_ be the radius of a circle (fig 39), that is required to
be subdivided into four rings of equal area by concentric circles.
Taking _a d_ as a diameter, draw the semicircumference, _a b d_;
accurately divide _a d_ into four equal parts, and at each point so
obtained, erect a perpendicular. Through the intersections of these
perpendiculars with the semicircle, draw a series of concentric
circles; they will trace out rings, 1, 2, 3, 4, that have equal
superficial areas.
If it be required to divide the surface in a given proportion, divide
the line _a d_, according to that proportion.
[Illustration: _Fig. 39._]
The right-hand side of fig. 39 gives a special application of this
method to the division into two equal areas of the interior of a barrel
exclusive of the space occupied by the arbor-nut. If the mainspring
accurately covers _i c_ when wound up, and _i j_ when unwound, it will
give the greatest possible number of turns.
TIME.
=50.= Solar time is taken from the revolutions of the earth, and the
watchmaker can easily get the exact solar time of any point at which
he may happen to be by a little calculation from known standards.
These standards are: 1. The zenith. 2. The longitude of the point of
observation. 3. The difference between noon at the point of observation
and noon of a known meridian either east or west of the point of
observation. The zenith is that point in the heavens where the rays
of the sun are in a plane exactly perpendicular to the surface of the
earth at the point of observation, and when the rays of sunlight are
in this plane it is noon at that point. The circumference of the earth
is divided into 360 degrees or meridians of longitude, so that as the
earth revolves once every twenty-four hours, each of these meridians
will pass the zenith, or fixed point, in that time. In twenty-four
hours there are 24 × 60 = 1,440 minutes, so that the interval between
the passage of one meridian and the next will be 1,440 ÷ 360 = 4
minutes. A degree of longitude is divided like an hour, into minutes
and seconds, so that
1 degree of longitude equals 4 minutes of time.
1 minute ” ” ” 4 seconds ” ”
1 second ” ” ” ¹⁄₁₅ or .066 seconds of time.
=51.= Thus it happens that, at a town one degree east of a given
point the sun will be visible four minutes sooner, and if to the
west, four minutes later than at that point. The “local,” or solar
time, therefore, will be four minutes earlier at the first town, and
four minutes later at the second town, than it is at the point of
observation.
=52.= It will be readily seen that, having any two of the three factors
given above, the other can be readily found. Thus having the time of
a given meridian and the local noon or meridian time, the longitude
can be readily found; or, having the longitude (which can be readily
obtained from a surveyor) and the time of a given meridian, “noon,”
can be calculated, etc. The first method is followed in calculating
distances at sea; the chronometer keeping Greenwich time, and the local
noon giving the longitude.
When great accuracy is necessary, however, a fixed star is used as a
means of observing the exact time when a revolution of the earth is
completed, as the revolution of the sun in its orbit causes a slight
variation during the year. For further information on this point the
reader is referred to works on astronomy.
To obviate the constantly varying time in running east or west, the
railroads use the time of a given meridian over each fifteen degrees
of longitude, and as each degree of longitude equals four minutes of
time, it follows that only the hour is changed in changing from one
standard to another. In Europe the zero of longitude, or the time of
the meridian of Greenwich is used. In the United States the time of
the 75th degree, which passes through Philadelphia, is used from the
67th to the 80th degree, which comprises the territory from Princeton,
Maine, to a line drawn north and south, passing through Erie and
Pittsburg, Pa., and is called Eastern time. The time of the 90th
meridian is used from the 80th to the 102d meridian, and is called
Central time. The time of the 105th meridian is used from the 102d to
the 114th meridian, and is called Mountain time. The time of the 120th
meridian is used from the 114th meridian to the coast (which ends at
about the 124th meridian) and is called Pacific time. The time of the
various standards is telegraphed through their various territories at
noon each day, and furnishes an accurate standard of comparison to all
watchmakers.
=53.= In very many cities the actual or solar noon has been discarded
and the railway standard adopted, thus making but one standard and
removing the source of confusion and annoyance to many people. In
others, however, the two standards are still used, and it becomes
necessary for the watchmaker to be able to calculate both standards,
in case of accident or irregularity in his regulator. Hence he should
calculate his longitude within one second by means of the difference
between railroad and local noon, and have the nearest surveyor correct
his reckoning; then, by means of the accurate longitude and the
railroad time, correct the solar time; then by means of the solar
noon and the longitude calculate the railroad time. When all these
calculations check each other perfectly, he possesses all the time data
he needs for that place, and can correct his standard or regulator
if at any time it should become irregular. The calculations are very
simple, and can be easily performed from the data given above.
FOOTNOTES:
[1] Loomis’ Treatise on Arithmetic.
Loomis’ Treatise on Algebra.
Loomis’ Elements of Geometry.
Robinson’s Algebra and Geometry.
[2] Adapted from Robinson’s Algebra.
[3] Determined in the manner explained for erecting a perpendicular in
par. 32 except that intersecting arcs are described on both sides of
the line (_n m_, fig. 17); the perpendicular will be a line joining
these points of intersection.
PART II.
MATERIALS EMPLOYED IN HOROLOGY.
IRON.
=54.= Iron is an elementary body, that is to say it cannot be
decomposed. It is the most tenacious of the metals, having a breaking
strain of about 75 kilo. per sq. mm. (or 106,000 pounds per sq. inch)
of section. Two pieces can be perfectly welded together when raised to
a white heat.
In the smaller horological appliances, the metal is not employed except
after conversion into steel. In common clocks it is used from motives
of economy, for forming pins, screws, etc. In turret clocks, however,
considerable use is made of it, many of the parts after they are formed
being cemented, that is to say, having their surface rendered hard in a
manner subsequently indicated (=65=).
Such a mode of manufacture is particularly applicable to pieces that
are subject to a constant succession of impacts; their hardened,
steelified surface resists wear, while the iron core affords security
against rupture.
It is important to carefully distinguish the cases in which iron is
preferable from those in which its substitution for steel serves merely
to augment the profits of the manufacturer.
The fracture of a good piece of iron is characterized by long twisted
fibres of a brilliant white color.
If heated frequently or carelessly, the quality of the metal is
impaired—it ceases to be fibrous and looses its tenacity: in this
condition it is said to be _burnt_.
It is better to work with a charcoal or gas fire, as coal acts
more rapidly in rendering the metal brittle. Cold hammering, or
“hammer-hardening,” also makes it brittle and diminishes its tenacity,
but this is again restored by a suitable annealing.
Iron dissolves slowly in dilute nitric acid; if not diluted, this acid
rapidly oxidizes it. Dilute sulphuric acid dissolves the metal easily,
but if concentrated, it has no action in the cold, whereas, on heating
to ebullition, the iron is dissolved with evolution of sulphurous acid
gas. It is also dissolved by hydrochloric acid, or aqua regia.
Iron is less magnetic than steel, especially hardened steel, which,
owing to its great coercive force, is magnetized with greater
difficulty, but retains its magnetism for a longer period. Indeed,
_soft iron_, if properly prepared, can be magnetized and demagnetized
instantaneously.
Some workmen can distinguish iron from steel by the musical note
emitted on striking. A more certain method, however, consists in using
dilute nitric, or sulphuric acid. If the surface remains unaltered, or
nearly so, when touched with a drop of either acid, the metal is iron,
but, in the case of steel, a black mark will be left, owing to the
liberation of carbon.
=55.= =To Remove Rust.= The usual mode is to rub the object with a
piece of oiled rag, or emery paper. It appears that more rapid and more
satisfactory results are secured by using very pure petroleum, and
wiping with a hempen or woolen rag.
=56.= =To Prevent Rust.= Dip iron or steel articles in a mixture of
equal parts of carbolic acid and olive oil, rubbing the surface with
a rag. Others rub the metal with a mercurial ointment, leaving a thin
layer over the entire surface. It is stated that, if iron be dipped
in a solution of carbonate of potash or soda in water, the surface
will be protected against rust for a long time, and objects can be
protected for any period by burying in quicklime. Rubbing the surface
with plumbago has a similar effect, and Barff has pointed out that, by
exposing iron to the action of steam, heated above the boiling point of
water, a coating of magnetic oxide of iron is formed, which is equally
serviceable.
=57.= =To restore iron and steel that has been burnt, or badly forged.=
When iron is burnt, or carelessly forged, it becomes crystalline and
brittle; in order to restore it to its original condition, a fresh and
very careful forging is generally needed. This can be avoided by having
recourse to the following method, suggested by Caron: it consists in
treating the metal somewhat after the manner adopted in hardening steel.
He experimented with a bar of good iron, which was easily bent when
cold, without breaking or showing any cracks. It was then burnt and
became brittle when cold, the fractured surface showing brilliant
shining facets.
Prepare a boiling saturated solution of sea-salt, heat the piece of
iron to a bright redness, and plunge it into the bath until it is of
the same temperature (about 110° C. or 230° F.) After undergoing this
operation, it is found that the metal can be easily doubled in the
cold, exactly as it did before being burnt.
Perret states that steel which has been deteriorated by frequent
hardening can be restored as follows: Heat it short of dull redness and
quench in melted tallow, repeating the operation, if necessary, when
the steel may be again hardened in the ordinary manner, and will be
nearly, if not quite, restored to its original condition.
CAST IRON.
=58.= This is only used in the manufacture of tools and large clocks;
the employment of cast iron wheels in the striking train of such clocks
has materially reduced their price.
Like steel, it is a compound body, consisting mainly of iron and
carbon. Cast iron, however, differs from steel in the quantity of
carbon present, for, whereas its proportion in cast iron varies from 2
per cent. upwards, there is never, in steel, an amount exceeding 1.5
per cent., and even .5 per cent. renders an iron hard, converting it
into “mild” steel.
Cheapness is not the only argument in favor of the use of cast iron. In
virtue of its molecular structure, this material offers a considerable
resistance to a crushing strain, so that the teeth of wheels, made
of carefully selected cast iron, will work for a long time without
sensible wear; moreover, the founder’s art has made such important
advances that there is no difficulty in casting, to a constant pattern,
a wheel, together with the pinion that it carries, and any other
projections, etc., that may be required; this economizes labor to a
very great extent.
The use of cast iron in the construction of certain classes of wheels,
and parts of tools, presents advantages which we cannot afford to
ignore; but it must be carefully observed that this material is not
suitable in cases where great accuracy in the acting parts is required,
as it cannot, like brass and steel, be conveniently worked by the
turning tool or file. In recent years, however, this difficulty
has been overcome by the introduction of what are termed “malleable
castings,” produced as follows:
=59.= =Malleable Castings.= The object is first made of ordinary cast
iron, and the invention consists in rendering this malleable by the
removal of the carbon that has served the very important purpose of
rendering the metal fusible. In large cast iron pots, the castings are
laid with alternating layers of powdered red hæmatite, and the whole is
kept at a temperature of about 900° C. (1,650° F.), or cherry-red heat,
for 72 hours. On cooling, the castings are found to consist of nearly
pure iron, and to be perfectly malleable, and, therefore, workable.
STEEL.
=60.= The treatment of steel involves some of the most prolonged and
delicate operations in the entire range of horology. If the metal is
badly selected and prepared, the working of it will be laborious,
difficult and unsatisfactory; the resulting object will be distorted
in the hardening, and will not harden uniformly; in short, it will
occasion much toil and loss of time, with very little success.
Let the young watchmaker accustom himself from the first to study the
steel that he uses, so that he may be thoroughly cognizant of both its
advantages and defects; he will, in the practice of his art, be amply
repaid for the brief time spent in making such an examination.
=61.= Steel is not an elementary body; it is usually regarded as a
carbide of iron, that is to say a combination of carbon and iron.
Analysis, however, proves other substances to be usually present in
almost infinitesimal quantities; their remarkable influence on the
physical properties of the metal has not yet been fully investigated,
but much attention is being devoted to them at the present day.
The varieties of steel are very great. What are known as _puddled_
and _natural_ steel are obtained by acting directly on cast iron.
_Cementation_ is a very old method of converting bars of malleable or
pure iron into steel by enclosing them in charcoal and heating the
whole for several days, until the carbon has worked itself into the
center of the bars in such quantity as to covert the iron into steel.
The steel obtained by the above method is very heterogeneous; in other
words, the composition is not uniform throughout a given block or
bar. One part is highly carbonized, whereas another part, especially
towards the center, will not be sufficiently so. The _grain_, although
very fine in one part, will be more coarse in another; hard particles
of pure cast iron, termed “pins,” are to be met with that resist
the action of the graver or the file and give rise to cracks in the
hardening, hammering, etc., and portions or sometimes even entire
layers that have taken up no carbon whatever. The differences in the
density, hardness, malleability, etc., that can be shown to exist at
different points in the same bar arise from this cause.
Such faults can in part be corrected by _shearing_, an operation which
consists in binding together a number of bars in a bundle, raising
them to a red heat and beating them with sledge or steam hammers so as
to weld them into one. The bar thus obtained is again heated, folded
several times on itself, again hammered, rolled, etc., when it is
termed _shear steel_. If these operations are performed carefully and
without a too great heat, the quality of the steel is much improved;
it is more homogeneous and can be worked with greater facility.
=62.= The discovery of the earliest method of producing _cast_ steel,
thoroughly homogeneous, was made by a watchmaker, B. Huntsman, of York,
and metal produced by his method is very highly prized at the present
day. Many other methods have been since introduced, amongst which may
be mention the Bessemer and the Siemens-Martin processes, and steel
is now produced from iron of very varying quality, so that the mark
_cast steel_ is now far from being a guarantee of quality. The fusion
of shear or cement steel will only secure a marked superiority in its
quality under two principal conditions: (1) The metal must be carefully
selected, since certain qualities do not intermingle thoroughly. (2)
Very great care and skill must be devoted to all the operations, the
successive heatings, forging, rolling, etc.
In short, in the case of steel it is exceptionally true that we must
never accept the metal merely on its own recommendation. Whatever
maker’s mark is selected, the results obtained will never be
satisfactory unless the degree of hardness, the elasticity, cohesive
force, etc., are such as will suit the metal to the special purpose to
which it is to be applied as well as to the working it will have to
undergo. _Experiment can alone make us fully cognizant of the qualities
of a steel._
GENERAL OBSERVATIONS.
=63.= All steels, if of good quality to begin with, will deteriorate
if subjected too often or too long (according to the character of the
metal) to the action of either the fire or the hammer. They will become
brittle and incapable of hardening, in the end even reverting to the
condition of iron.
The quality of steel becomes worse as the number of flaws, blackish
filaments, more or less carbonaceous veins, and occasional particles of
pure iron in its substance are greater; as its surface is _cindery_,
that is to say spotted with minute black marks which become more
prominent after polishing, etc.; as its fracture presents an uneven
grain, etc.
Such a metal is found to vary considerably as regards hardness,
elasticity, etc.; not being uniformly affected in the hardening, it
becomes difficult to work with the file and almost impossible to form
into a perfect cylinder in the lathe.
Other conditions being equal, these faults are characteristic of
natural steel rather than of the two other varieties. At the same time,
if well sheared, it becomes very elastic, and has the great advantages
of not being deteriorated under the hammer and of being less ready than
the other varieties to be converted into iron.
Rolling, wire-drawing and hammering occasion a molecular
re-arrangement; it is necessary, therefore, to anneal the metal from
time to time, as otherwise it becomes brittle or cracks.
There is a certain temperature, corresponding to each variety of steel,
which cannot be exceeded without the metal being injuriously affected;
this temperature must, then, be previously determined.
The grain of a piece of steel that has been superheated or _burnt_
is characterized by brilliant diamond-like particles; the mass loses
its beautiful color, and resembles iron more or less according to the
degree of heat applied.
Some few workmen are enabled, by long experience and a very delicate
touch, to judge approximately of the quality of a steel from its
weight, feel, and resonance. Metal that is of a good quality,
homogeneous, and very dense, they term _full_.
SPECIAL OBSERVATIONS.
=64.= =Natural Steel.= In the case of natural steels of low quality,
the fracture is usually characterized by uneven grains, a somewhat
fibrous nature and a bluish tint. The grain becomes finer and more
even and the surface presents more and more the appearance of a
piece of coke, as the quality of metal improves. In addition to
these distinctive features a natural steel of high quality can be
distinguished by the fact of its being more thoroughly hardened and
less liable to break when hard.
In hardening it must be raised to a higher temperature than cement
steel; in other words, steel of a low quality must be heated somewhat
above bright redness, while the better qualities should be heated to an
orange-red, or nearly so (=77=).
=65.= =Cement Steel.= The cement steel ordinarily met with has a
lamellar fracture, the lamellæ varying in form and color from the
center towards the circumference. The grain is usually finer and more
uniform than that of natural steel, there is seldom any appearance of
fibres, veins, or flaws. The color of the fracture is greyish, tending
towards blue in the ordinary qualities.
The better qualities are marked by a closer grain, a more uniform,
dull, greyish-white color, exhibiting neither streaks or black spots
after hardening, and by the further fact that hardening can be effected
at a lower temperature. If of the very best quality, it should not
require heating beyond a clear cherry-red; often even a still less
degree of heat will suffice.
=66.= =Cast Steel.= Cast steel is the most homogeneous, full, and
beautiful of the three classes. Several varieties exist. The fracture
of cast steel, as compared with others, is smooth, compact, and of
a white-grey color, resembling coke. The grain is fine and very
even. The metal must be hardened at a temperature much lower than
can be safely applied to other classes of steel, since it is rapidly
deteriorated by heat.
Cast steel is more fusible than ordinary steel, and will fracture with
ease under the hammer when heated to a blue tint, so that great care is
essential in hammering it.
The metal should never be heated beyond a dull or cherry-red heat, lest
it be _burnt_.
The tenacity will be increased by forging at a low temperature or even
by cold hammering.
The fineness in grain, together with its high density, afford an
indication that the metal can be rendered very uniformly hard; that
very fine cutting edges and the most minute rods can be made of it;
and that, after hardening, it can be highly and uniformly polished;
in other words, that it does not exhibit spots or streaks differing
in color from the mass, as is always the case with natural and cement
steels. For most horological purposes (such as making pinions, staffs,
pivots, etc.) cast steel is preferable. It is the only kind that can
with certainty be highly polished, turned perfectly round, and that
does not get distorted in the smoothing. Moreover, when wear does occur
it exhibits less irregularity.
Highly-carbonized shear steel exhibits a fine, close grain that would
make it easily mistaken for cast steel. They can be best distinguished
by the application of dilute sulphuric acid. The side of the bar when
acted on by this means exhibits lines that indicate the junctions of
the several layers constituting shear steel.
DETERMINATION OF THE QUALITIES OF STEEL.
=67.= It is unnecessary to observe that as we are writing mainly for
the use of practical watch and clockmakers, we shall make no reference
to those elaborate systems of testing that form a remarkable feature
of the engineering of the present day, but shall confine ourselves to
the tests which workmen can apply for themselves.
When the grain is fine, close and homogeneous, the fracture in even
curved lines and the surface of a uniform grey aspect, the metal is
considered to be of good quality. It is, nevertheless, unsafe to rely
too much on such indications, for a steel that has been hammered
until cold will exhibit a fine close grain, whereas the grain of the
same metal will be coarse and open if it was still red hot when the
hammering or rolling was concluded. The grain of hardened steel,
moreover, depends on the degree of heat to which it has been subjected.
When of equal quality, even if from the same maker, the grain will be
finer in bars of small dimensions than in those that are larger.
Cast steel even, especially in large pieces, is not always perfectly
homogeneous, as can be easily perceived on applying the file, or
still better, in the lathe; an object can with difficulty be turned
perfectly round, and loses its shape in the smoothing. _As a general
rule it is impossible to form a reliable opinion on a specimen of steel
until after it has been worked, filed, turned, and tested according
to the particular use to which it is to be applied; for a steel that
is excellent for making, say, a spring or a cutter, may be quite
unsuitable and give most unsatisfactory results if used for making
staffs or fine pivots, or the converse may be equally true._
As a preliminary test, break a piece of the metal; after having
examined the fracture, form a cutting edge, harden to what seems to be
a convenient degree, then sharpen and employ for cutting small pieces
of iron. If the edge is in no way damaged by the iron, this may be
taken as a good indication that the metal possesses body and tenacity,
and that it can be hardened as much as is required for such purposes.
The following are methods of obtaining more complete information as to
the homogeneity, the character of grain, the degree of hardness a given
sample can attain, as well as its malleability, body, elasticity, etc.
=68.= =Homogeneity.= Place drops of dilute sulphuric acid equidistant
along the surface of a bar. If the metal is homogeneous all the drops
will impart the same color.
Cold hammer or hammer-harden, and then fire-harden part of the bar.
Break off the extremity in order to study the fracture; if the result
of this examination is satisfactory, polish the hardened end carefully,
and with the aid of a glass again examine into the homogeneity of the
metal. The polish will be the better and more uniform according as the
steel is more homogeneous.
=69.= =Grain, hardness and temperature of hardening.= All varieties
of steel do not harden to the same degree, and each requires to be
heated to its own particular temperature for hardening; moreover, the
character of the metal, its color, and the size of its grains vary
according to the degree of heat to which it is subjected. It would be
difficult to draw any exact conclusions as to the character of grain
and the hardness without the following practical method, which we owe
to Reaumur:
At a temperature not exceeding a dull redness, forge a piece of the
steel to be tested into the form of a razor-blade, that is to say,
leaving it thick on one edge and thin on the other, in the direction of
its length. Then heat the blade, holding it by one end, and when the
other end has reached a bright red heat, plunge the whole into water.
Part of the steel will then be hard hardened. Along the entire length
of the thinner edge carefully break off the metal with a hammer or
otherwise, and examine the character of grain at different points of
the exposed thicker edge thus left.
As the form, color, etc., of the grain depend on the degree of heat to
which each portion was subjected, it follows that we shall observe four
types of grains: (1) Large, white, sparkling grains; (2) Grains that
are medium sized and intermixed, some being white and sparkling, others
white and dull; (3) Fine dull grains; and (4) Grains that are medium
sized, but dull and ill-defined.
According as the third class of grains is observed to be more numerous
than the second class, so is the fineness of the steel greater, and
conversely.
This method of testing possesses, moreover, the advantage that the
workman can experiment on his blade of steel with a view to determine
the temperature best suited for hardening.
Grain No. 1 corresponds to a white-red heat for hardening.
Grain No. 2 corresponds to an orange-red heat for hardening.
Grain No. 3 corresponds to some shade of cherry-red heat for hardening.
Grain No. 4 corresponds to a dull red heat for hardening.
As there is some difficulty in remembering the exact points at which
these several temperatures are reached we will complete this account of
the mode of testing by the following:
=70.= On a thick plate of metal, maintained at an orange-red heat,
place three fragments of the steel under examination, previously
marking them, so as to observe the order in which they are immersed
in water; and have three vessels of water standing near. As soon as
one of the pieces reaches a dull cherry-red heat, allow it to slide
into one of the vessels; heat the second to a medium cherry, and the
third to a bright cherry-red, introducing them in succession into
the water-vessels. If these pieces be examined as to the resistance
they offer to breaking, and the fracture of each be compared with the
fracture at different points of the razor-blade, the file being used
to test hardness, we shall have sufficient evidence as to the most
suitable temperature for the hardening of this particular variety of
steel.
=71.= =Body.= A steel that possesses _body_ is not brittle. This
quality may be tested in the following manner: Several bars of
different kinds of steel, of equal dimensions and hardened as uniformly
as possible, are bent until the breaking point is reached. If all
the conditions of the trial are identical, those bars that stand the
greatest angular deflection without breaking have the most body.
Steel that possesses body does not break as easily as that which
is wanting in body. Its fracture will be, as it were, bevelled off
like the mouth-piece of a whistle. If soft and fibrous, it will be
characterized by parts being torn asunder.
=72.= =Elasticity.= The elasticity may be tested in a similar manner.
It is proportional to the curvature or to the weight that a rod or
blade of the metal under examination can support without failing to
return to its initial position as soon as the weight or obstacle is
removed. A sample of steel that is distorted by a weight that another
specimen resists, is evidently inferior in elasticity.
=73.= =Malleability, tenacity, ductility.= A cold hammering, if
carefully managed, will suffice to indicate the limits between which
steel will support frequently repeated percussion, without breaking,
cracking or flying.
Forge a piece, introducing it a number of times into the fire in order
to ascertain whether it loses its distinctive characteristics rapidly,
and whether it can be successfully forged.
It is more difficult to forge, according as it is harder and more
“steely.”
The degree of malleability is indicated by the manner in which it
supports hammering and rolling, and by the smallness of the dimensions
to which it can be brought by such operations.
Passing the metal through a draw-plate with smooth holes, or tapping it
in a screw-plate will give useful indications as to degree of ductility
and tenacity.
A metal is said to be _malleable_ when it can be easily spread out
under the hammer or in the laminating rolls. It is called _ductile_
when it can be reduced to very thin wire by passing through the
draw-plate.
It would seem that these two properties, ductility and malleability,
should always exist together, to the same degree, in any given metal,
but such is not the case. Iron can be drawn into very fine wire, but
cannot be reduced to sheets of relatively equal thinness; tin and lead
give leaves of extreme thinness, but cannot be drawn out into very fine
wires; gold and silver are both very malleable and ductile, and they
rank highest as regards the possession of these properties.
Steel is more fusible and malleable than iron, but less ductile.
=74.= _Observations._ Formerly the makers of cylinder escapements
preferred forged steel, and their cylinders often cracked after the
hardening: modern makers employ drawn steel, and it is much preferable.
At the same time they do not appear to recognize the principal reason
for the difference in the two varieties of steel. It seems to us to be
as follows: forged steel is malleable; drawn steel, which has passed
well through the draw-plate, is ductile, and, therefore, tenacious. But
tenacity in a metal is nothing else than an exceptional resistance,
opposed by its particles to a fracture or separation; it follows, then
that drawn steel will crack with less facility than the other.
PREPARATIONS OF STEEL.
=75.= When a variety of steel has been selected that possesses the
requisite properties: that is to say, fibre and elasticity for springs;
body and tenacity for circular cutters, gravers, etc., it must be
prepared; in other words, it must be made so that it can be worked with
ease, for steel that is badly prepared will resist both the file, the
graver and the drill. It can never be turned perfectly round, and will
harden unevenly.
=76.= =To anneal steel.= The commonest, and at the same time best,
method consists in heating the metal to a dull, red heat, burying it in
hot ashes and allowing it to cool slowly.
Steel raised to a red heat in contact with air loses a portion of its
carbon, so that it is better to place the metal in a vessel of burnt
clay; this is introduced into a fire which must not be too bright at
first, and when the vessel has attained a red heat the fire is checked
and left until the whole is quite cold.
In order to soften steel by annealing with a view to work it, engineers
entirely cover the metal with dry powdered wood charcoal or dry iron
filings or turnings, in a cast iron box or pot, or in a crucible,
shutting up all the openings so as to protect it from the direct
action of the fire and from the air. The vessel is then put in a dull
fire, the heat being gradually raised until the whole has acquired
the requisite temperature, which is known by observing the color (see
the following table); this degree of heat is maintained for about
ten minutes and the fire quenched, after which it must be allowed to
gradually die out. Frequently the cooling is not complete for a day or
two, and even more when the crucible is of large dimensions.
The metal will become softer, according as the cooling is more slowly
effected. It is generally heated to 800° or 900° C. (1500° or 1600°
F.), a cherry-red heat. When the steel is associated with brass, as in
the case of a compensation balance, it is not safe to exceed 600° C.
(1000° F.)
=77.= It will be useful here to give the following table, compiled by
Pouillet, of the temperature, as indicated by the air-thermometer,
corresponding to various colors of a heated body:
Incipient red heat corresponds to 525° C. ( 980° F.)
Dull red ” ” ” 700° C. (1280° F.)
Incipient cherry-red ” ” 800° C. (1470° F.)
Cherry-red ” ” 900° C. (1650° F.)
Clear cherry-red ” ” 1000° C. (1830° F.)
Deep orange ” ” 1100° C. (2010° F.)
Clear orange ” ” 1200° C. (2190° F.)
White ” ” 1300° C. (2370° F.)
Bright white ” ” 1400° C. (2550° F.)
Dazzling white ” 1500-1600° C. (2730-2910° F.)
=78.= _Annealing or softening in water._ Instead of allowing a piece
of steel to cool slowly, it may be thrown into water when heated to
a temperature just below that at which it would harden. In this case
the metal will not harden, but, on the contrary, become very soft.
A single operation suffices for certain varieties of steel, but with
others it must be repeated.
The only difficulty consists in fixing upon the precise moment at which
the metal has the requisite tint (a purplish yellow or dull red), and
this is more especially felt when dealing with small pieces; experience
can alone guide the workman in this matter.
A skilful workman recommends the employment of water containing
one-fifth of its weight of gum arabic. He also recommends that the
metal be wiped over with an oiled rag, then held in the fire, and, as
soon as the oil is converted into a thick smoke, and is on the point of
igniting, to immerse in water.
=79.= =Hammering steel.= Watchmakers who are called upon to manipulate
exceedingly small pieces of steel, can somewhat increase the body and
homogeneity of the metal by a cold hammering. After annealing, the
object is hammered with light, uniform blows, again annealed, and the
same operation is repeated one or more times, according to the degree
of malleability already acquired by the metal. Steel thus prepared
has more body; the particles composing it are more closely pressed
together; it files and turns well, can be heated more evenly, and
is not distorted or only very slightly in hardening, providing the
requisite precautions are taken.
=80.= _The hammer and anvil._ It is important that in these operations
the surfaces of the hammer and anvil employed be perfectly smooth and
even polished. If they are rough or cracked, if they are uneven or have
a grained surface, a flaw will be produced in the body of the steel or
a crack on its surface.
=81.= =To clean rough steel.= The black coating known as “scale,” which
covers the surface of the metal after it has been in the fire, will
rapidly spoil gravers and files, and, in addition to this, it leaves
behind in them excessively hard particles that will become imbedded in
the steel itself after a clean surface has been exposed. It is then
essential, in order to ensure good and rapid workmanship, to previously
remove this crust from the surface.
This can be done in two ways: by using a rapidly-revolving grindstone,
which instantaneously removes the oxide, at the same time smoothing the
surface of the steel; or by leaving it for a sufficient length of time
in dilute acid, by which the superficial oxide is dissolved.
Sulphuric acid is usually preferred; in addition to the cleaning, it is
said to produce an effect somewhat similar to annealing. On withdrawal
from the acid, the steel must be thoroughly washed with water and wiped
dry with care.
=82.= =Ordinary mode of preparing steel.= When the metal has been
annealed by one of the methods indicated above, its preparation is
completed by “pickling” in acid, after which it is hammered cold
between an anvil and hammer (=79=, =80=). When the metal has been
worked, it is heated to a bluish tint, and after cooling slowly is
ready for the hardening.
=83.= _M. Covillot’s mode._ This author adopts a method whereby he
obtains steel that is very soft to work and perfectly free from hard
grains or “pins” of cast iron, which are so often to be met with in
steel, causing it to crack in consequence of their inability to spread
under the hammer.
Take some garlic, the younger the better, mix it with sufficient good
walnut-oil to cover the garlic and form into a paste; then place it in
an earthenware pot on the fire. When beginning to boil, heat the steel
to dull redness and plunge it into the boiling paste. Withdraw it with
a quantity of oil and garlic adhering; again heat to redness and plunge
into the paste. This operation may be repeated two or three times. Then
heat the steel, while inclosed in an iron tube or box placed on the
fire, and allow the whole to cool. Finally, the steel may be finished
by setting it to _cook_ (if we may use such an expression) for ten or
twelve hours in the composition of garlic and nut-oil.
The last operation may be performed by setting the boiling solution
over an oil-lamp, after depressing the wick in such a manner that the
paste may be kept just simmering.
M. Covillot employed the same mixture for hardening the objects; but
then, of course, it must be cold.
HARDENING.
=84.= It is well known that by the operation of hardening, which
consists in heating a piece of steel to a red heat and immediately
chilling it, the hardness is very materially increased.
Hardening increases the dimensions of the object. A steel collar
adjusted to fit a cylinder will slide on more easily after hardening.
Rolled steel is more liable to be distorted in the hardening than metal
which has been forged or hammer-hardened. As a general rule, when
steel—especially cast steel—has been carefully annealed, cold-hammered
and, after working, heated to a blue temper and slowly cooled, it will
not be distorted in the hardening, providing the heating is skillfully
conducted, and if, at the moment of introducing the object vertically
into the bath, the heat is evenly distributed throughout. Some
practical men affirm that the mere presence of an oily layer on the
surface of the water will check the tendency to distortion.
A workman frequently pretends that he has some exceptionally good
solution for hardening, of which a great mystery is often made; but it
is very generally admitted by those who are well-informed that these
so-called secrets are a delusion and in no sense superior to pure
water. There is a certain amount of truth on both sides, and the former
class are somewhat justified by experiments with the various solutions
enumerated below. We may, however, lay down the three following
conditions as essential to the successful conduct of the operation of
hardening: (1) _The steel must previously be carefully prepared and
worked_; metal that has been skillfully hammered cold or below a red
heat, for instance, will harden better than when not so treated; but
if hammered too much or carelessly, it will crack; (2) _The method of
heating_ should be such that the heat is evenly distributed throughout
the object; if, on immersion, its temperature is not uniform, the
degree of hardness will vary; (3) _The skill of the workman_ must
enable him to detect the exact degree of heat the variety of steel
can withstand, and this must on no account be exceeded, for in that
case the steel will lose tenacity, will be more or less _burnt_, &c.
In the case of irregular shaped articles, considerable skill is often
needed to ensure that the several parts of the mass shall be cooled at,
approximately, the same rate.
=85.= =Methods of hardening.= The baths used for hardening may be
classed under three heads: _Tough_, _Hard_, and _Glass-hard_. It must
be understood, however, that these classes may be made to merge more or
less into one another, by varying the degree of temper.
=85a.= The following receipts are drawn from
various sources, and the reader is recommended to select the one which
he finds on trial to be best adapted to his requirements, for, as Prof.
Akerman has pointed out, there are very many conditions exceedingly
difficult of calculation that influence hardening, and hence it follows
that a workman accustomed to hardening often considers that only one
method, which he has been in the habit of employing, can be used for a
certain purpose, while another equally skillful workman can only attain
the same result by a method essentially different.
I. _Tough._ Tallow; tepid water; oil; resin; sealing-wax; lead;
beeswax; a solution of 3 to 4 parts (by weight) of gum arabic in 100
parts of water; 1 part of soft soap in 100 parts of water; cold water
with a layer of oil over it, the thickness of which varies with the
degree of hardness required; 10 parts mutton suet, 5 parts resin, 2
parts sal-ammoniac, and 35 parts olive oil.
II. _Hard._ Cold water; water containing various salts, such as
sal-ammoniac and sea-salt; a solution of 5 parts sea-salt and 1 part
sal-ammoniac in 20 parts of water; 4 parts sulphuric acid, 50 parts
sea-salt, 10 parts alcohol, and 1,000 parts water (all by weight); 4
parts sulphuric acid, 1 part nitric acid, 1 part pyroligneous acid in
1,000 parts water (to be used very cold).
III. _Glass-hard._—Mercury; nitric acid; opium; any cyanide.
=86.= As a rule it is well to employ tallow for the hardening of small
objects in which hardness without brittleness is needed. Oil renders
the surface harder than the interior, and soapy water has the same
effect. Saline solutions generally give great hardness. Very minute
drills may be hardened by simply whisking them about in the air after
heating the blade to redness, and small objects may be hardened by
pressing between two cold surfaces, as those of the hammer and anvil.
If hardened in nitric acid, opium, or mercury, the hardness of steel is
so great that it will easily cut glass. But such steel is brittle and
all the more delicate according as the precise temperature necessary
(which is not very high) has been exceeded. For it must always be borne
in mind that steel which has been heated too highly has deteriorated in
quality and will remain brittle.
=87.= =Precautions to be observed in hardening.= In the case of
delicate pieces it is necessary to avoid the use of the blow-pipe, as
the current of air causes the surface to scale, and, as is well known,
the metal being unevenly heated will be distorted in the hardening, and
will not be uniformly hardened.
It is better to enclose the article between two pieces of ignited
charcoal, or in a metal tube, or to bring it in contact with a
sufficiently hot piece of metal, etc. An excellent plan is to heat
the article in a bath of hot lead, or of lead and tin in proportions
dependent on the temperature required. The heating is thus exceedingly
uniform, and, if operating in a dark room, the temperature can be
accurately judged.
When it is required to harden an object without discoloring the surface
or destroying the polish, it may be placed in a tube, and completely
surrounded with powdered wood charcoal, or, preferably, animal
charcoal. The whole after being heated is plunged in water without the
steel being in any way exposed to the air. The powder must be heaped up
as a precaution against access of air. On being taken from the water,
the steel is at once placed in alcohol, and if at all dull it will
generally be only necessary to rub the surface with a little rouge.
It is essential that the animal charcoal be previously heated in order
to expel moisture, as otherwise it would adhere to the surface and
produce marks and even irregularity in the hardness.
As a rule the object must be immersed in the cooling liquid vertically
in the direction of its greatest length, and if of unequal thickness,
the stout portion should touch the surface first, so that the metal
may cool more uniformly. In hardening large masses of steel, various
devices are resorted to in order to insure uniformity in the cooling,
but space prevents us from entering more fully into this interesting
question.
The vessel must be of such a depth that the object will not reach the
bottom until quite cold. It is liable to distortion if introduced
sideways, or if the vessel is too shallow.
The method described above for protecting the surface from the action
of the fire should be adopted when hardening delicate or complicated
articles; but in the case of drills, for instance, a simple coating of
one of the following preparations is sufficient.
When an object is hardened in a saline solution, it is well to cover
it with a paste composed of water, salt and flour (some use yeast and
salt for this purpose), or a thin clay. This precaution prevents any
blistering or oxidation of the surface. If it be desired to avoid
oxidation, and, at the same time, to restore to the steel the carbon
it has lost owing to the action of the fire, it must be rolled, while
still wet, in another paste, containing powdered horn or leather, or
some such calcined animal matter. Delicate parts can also be protected
by a layer of beeswax and olive oil made hot.
In hardening small drills, very good results are obtained by enclosing
the blade in a pellet formed of prussiate of potash, lard and Castile
soap, and cooling in beeswax, or the surface may be protected by a
layer of soft soap.
Steel as forged, that is with the thin scale on, is less liable to
break in hardening than if previously brightened, for the scale causes
it to cook, and, therefore, contract more slowly. At the same time it
should be borne in mind that when the surface is bright the hardness
will be somewhat greater.
It will be well to warn the beginner that, if an object is not entirely
immersed in the cooling liquid, it should never be held still, but
rapidly moved up and down, as otherwise there is a liability to crack
at that part which was level with the surface.
As a watchmaker only uses steels of the best quality, he should, in
hardening never exceed a cherry-red heat, and cherry-red comprises
three distinct tints (=77=); incipient cherry-red, cherry-red, and
clear cherry-red. The second of these should not be exceeded in
hardening cast steel, and the third should be taken as an extreme limit
in the case of shear steel.
Ice-cold water should never be employed, but the extreme chill should
be first taken off. Indeed, it is found that frosty weather interferes
materially with the operation of hardening.
Some workmen maintain that the hardening is done better if the water
has been long used for the purpose without renewal.
TEMPERING.
=88.= Hardened steel is extremely fragile, but its tenacity may be
restored by _tempering_, that is to say, by heating it to a degree
dependent on the amount by which its original softness has to be
restored. The color of the metallic surface will gradually change as
the temperature rises, each tint corresponding approximately to the
degree of heat given in the following table (Stodart):
1. Very pale straw yellow 220° C. (430° F.) }
2. A shade darker yellow 235° C. (450° F.) } Tools for metal.
3. Darker straw yellow 245° C. (470° F.) } Tools for wood and
4. Still darker straw yellow 255° C. (490° F.) } screws, taps, etc.
5. Brown yellow 260° C. (500° C. 500° F.) } Hatchets, chipping
6. Yellow, tinged slightly } chisels and other
with purple 270° C. (520° F.) } percussive tools,
7. Light purple 275° C. (530° F.) } saws, etc.
8. Dark purple 290° C. (550° F.) }
9. Dark blue 300° C. (570° F.) } Springs.
10. Paler blue 310° C. (590° F.) }
11. Still paler blue 320° C. (610° F.) } Too soft for the
12. Still paler blue, with tinge } above purposes.
of green 335° C. (630° F.) }
=89.= It will facilitate the precise determination of these points if
it be remembered that
An alloy of 1 part lead and 1 part tin (by weight)
melts at 196° C. (385° F.)
Metallic tin ” ” ” 230° C. (446° F.)
An alloy of 2 parts lead and 1 part tin ” 240° C. (465° F.)
Metallic bismuth ” ” ” 270° C. (520° F.)
An alloy of 5 parts lead and 1 part tin ” 290° c. (550° F.)
Metallic cadmium ” ” ” 310° C. (590° F.)
Metallic lead ” ” ” 320° C. (608° F.)
=90.= Before proceeding to temper an object, at least one of its faces
must be smoothed with pumice-stone, oilstone dust, or emery paper, and
the surface must be left perfectly clean, care being taken to avoid
contact with the fingers, as otherwise it will be difficult to ensure
the requisite tint being obtained.
Tempered to any shade between Nos. 1 and 6 the steel will, if
previously well hardened, be left too hard to be worked by a file or
graver; heated beyond No. 10, it can no longer be much bent without
distortion.
When the quality and the degree of hardness of steel differ, the temper
corresponding to a given tint will also vary. As a rule, hardened cast
steel, tempered to No. 8, will be found as soft as natural steel which
has been let down to No. 9, or even to No. 10.
A piece of steel can be let down to the same tint several times in
succession without altering its properties.
If a good and uniform color is desired, the steel must be highly
polished, as the oxidation of rough parts will render the tint
irregular. The rouge employed must not be too dry, and, if the
burnisher is used, care should be taken that it acts on the entire
surface. Metal of a bad quality, which will not take an even polish,
can rarely be nicely blued.
When the object is finely _smoothed_ with a uniform white surface, very
good results may be obtained; but in such cases the cleaning must be
carefully conducted, as the presence of minute greasy particles will
always render the color irregular, and may even entirely prevent its
appearance.
A uniform color can only be obtained by heating the object in such a
manner that its temperature is raised evenly throughout.
The tempering may be performed by placing an object on the _bluing
tray_, a thin metallic plate, often covered with a thick layer of
fine brass filings, which should be renewed for each operation; or on
a thick piece of metal previously heated to a sufficient degree; on
ignited charcoal covered with a layer of white ash; in a bath of molten
metal, the temperature of which corresponds to the requisite degree of
heat, or the object may be laid on the surface of such a bath, etc.
Some watchmakers when letting down a piece of steel immerse it in water
to check the action; but by so doing they produce an exactly contrary
effect. If a piece of steel be cooled suddenly in water as soon as it
assumes any given color it will be _softer_ than if left to cool in the
open air (=78=).
At one of the blue tints, steel possesses its _maximum elasticity_. The
exact shade varies with the different qualities of steel.
If a hardened and tempered spring has lost its initial elasticity, this
may be restored or even improved upon by gently hammer-hardening, and
after whitening with emery, again tempering to the proper blue tint.
=91.= A very convenient way of tempering a large number of small
articles at a time, heating them with absolute uniformity, is to place
them in a small vessel with sufficient tallow or cold oil to cover
them; the whole is then heated to the requisite degree, which may be
determined by a thermometer or by observing the smoke. When smoke
is first seen to rise, the temper corresponds to No. 2 in the table
(article =88=). Smoke more abundant and darker corresponds to No. 5.
Black smoke still thicker, No. 7. Oil or tallow takes fire with lighted
paper presented to it, No. 9. After this the oil takes fire of itself
and continues to burn. If the whole of the oil is allowed to burn away,
the lowest temper in the table is reached.
It is often convenient to simply smear an article with oil or tallow,
and hold it over a flame or piece of hot iron. The temper can then be
judged in the manner just explained.
With a view to combine the two operations of hardening and tempering,
M. Caron suggested that the temperature of the water used for hardening
be heated to a pre-determined degree. Thus the requisite temper may
be given to gun-lock springs by heating the water in which they are
hardened to 55° C. (130° F.).
TO WHITEN AND BLUE STEEL.
=92.= Some makers of watch-hands and balance-springs, when they are not
satisfied with the color assumed by an object in tempering, immerse it
in an acid bath, which whitens it, after which the bluing operation is
repeated.
We have seen watchmakers whiten small pieces of steel with a piece of
pith moistened with dilute sulphuric acid, but the method cannot be
recommended.
Others fix fine steel work, a watch-hand for example, with wax on a
plate, and whiten it by means of pith and polishing rouge, or a small
stiff brush charged with the same material. It is then detached, by
heating, and cleaned in hot alcohol.
These methods, if judiciously employed, are of great service, but it is
important to remember always to thoroughly wash after the use of acid,
and then to allow the object to remain for a few minutes in alcohol.
Sulphuric acid does not whiten well. It often leaves dark shades on the
surface. Hydrochloric acid gives better results.
=93.= =To blue steel uniformly.= In order to secure a uniform color in
tempering or bluing, it is essential that the smoothing and polishing
should have been very evenly done. The surface must be perfectly clean;
for otherwise parts that are greasy, or on which the rouge has remained
too long, or has been too dry, will not exhibit the same tint as the
rest. The heat must be uniformly distributed. This is why, when bluing
screws in a perforated bluing pan, it is customary to lightly strike
the handle, for the vibration and the perpetual change in the contacts
ensures their receiving the heat more evenly. A similar purpose is
served by placing the pieces in brass filings. Steel must not be
tempered while only in contact with bodies that are bad conductors of
heat, stone, either in powder or block, for example; because, as we
have already observed, the distribution of heat would occur unevenly
throughout the metal.
Watchmakers secure a uniform tint more easily by using an iron or
copper polisher than one of any other metal.
=94.= _To blue small pieces of steel evenly._ If the foregoing
precautions are carefully observed, the following methods will give
satisfactory results:
First blue the object without any special regard to uniformity of
color. If it proves to be imperfect, take a piece of dead wood that
does not crumble too easily, or of clean pith, and whiten the surface
with rouge without letting it be too dry. Small pieces thus prepared,
if cleaned and blued with care, will assume a very uniform tint.
A clever mechanic assures us that he easily obtains a similar result by
rubbing the surface, after it has been well smoothed, with the end of a
stick that has been partly burnt in the fire.
=95.= _To blue a clock hand or a spring._ To blue a piece of steel
that is of some length, a clock hand for example; clockmakers place it
either on ignited charcoal, with a hole in the center for the socket,
and whitened over its surface, as this indicates a degree of heat that
is approximately uniform, or on a curved bluing tray perforated with
holes large enough to admit the socket. The center will become violet
or blue sooner than the rest, and as soon as it assumes the requisite
tint, the hand must be removed, holding it with tweezers by the socket,
or by the aid of a larged-sized arbor passed through it; the lower side
of the hand is then placed on the edge of the charcoal or bluing tray,
and removed by gradually sliding it off towards the point, more or less
slowly according to the progress made with the coloring; with a little
practice, the workman will soon be enabled to secure a uniform blue
throughout the length, and even, if necessary, to retouch parts that
have not assumed a sufficiently deep tint.
Instead of a bluing tray, a small mass of iron, with a slightly rounded
surface and heated to a suitable temperature, can be employed; but the
color must not form too rapidly, and this is liable to occur if the
temperature of the mass is excessive. Nor should this temperature be
unevenly distributed.
A spring after being whitened can be blued in the same way. Having
fixed one end, it is stretched by a weight attached to the other end,
and the hot iron is then passed along it at such a speed that a uniform
color is secured. Of course the hot iron might be fixed and the spring
passed over it. A lamp may be used, but its employment involves more
attention and dexterity.
=96.= =Bluing as an indication of temper.= This subject has already
been very fully considered in article =88= to =90=. When the color
assumed by a piece of steel does not require to be preserved, and it is
only necessary to temper the object at a certain temperature, the means
best adapted to expedite the operation will naturally be sought. Thus,
in factories, large numbers are tempered at once in a bath of tallow,
oil, etc. The workman, in judging temper by color (=88=), must have
enough experience to enable him to determine, for a given sample of
steel, what are the successive colors as well as the temperature of the
bath, etc. His success is certain; but it depends on the experience,
and, therefore, on the sense of sight of the operator, and, we should
again add, on the knowledge he possesses of the qualities of the steel
he is using.
CASE-HARDENING.
=97.= This process is often resorted to when a hard surface is required
on objects of wrought iron, for example the face of an anvil. It is
the exact converse of the method already described in article =59=
for obtaining malleable castings, and consists in heating the object
to a red heat in contact with charcoal, or some substance containing
carbon; this enters into the surface iron, converting it into steel.
Or after heating to a bright redness the object may be sprinkled over
with prussiate of potash, returned to the fire, and after a few minutes
cooled by immersion in water. When a greater thickness of steel is
needed, or when dealing with large articles, they must be enclosed in
wrought-iron boxes, and bedded in such substances as fragments of horn,
bones, leather cuttings, etc; the box is then luted up and the whole
maintained at a red heat for twelve hours, after which the fire is
allowed to die out. Articles may sometimes be case-hardened by coating
with a paste of arsenious acid, powdered leather, horn, or other
nitrogenous body and hydrochloric acid, and then heating them to bright
redness in a muffle or other suitable furnace.
INFLUENCE OF FOREIGN METALS AND METALLOIDS ON THE QUALITIES OF IRON AND
STEEL.
=98.= It would be impossible to give a full account of this subject in
the space at our disposal, and the reader must be referred to works
on the metallurgy of iron and steel for details in regard to the
remarkable influence of minute traces of phosphorus, tungsten, silicon,
manganese, arsenic, etc., on the mechanical and chemical properties of
those metals.
COPPER.
=99.= Copper is an elementary body of a reddish-brown color, which must
not be confounded with brass, occasionally termed yellow copper. In
tenacity it comes next below iron, breaking with a strain of 34 kilo.
per sq. mm. of section (or 48,000 lbs. per sq. inch).
In horology, the only use made of the pure metal is for the
construction of compensation pendulums on the gridiron principle, and
as wire in electric clocks. It is also employed, when rolled into thin
sheets, for a base to receive the enamel of watch dials, in consequence
of its expansion being about the same as that of the enamel, which does
not therefore crack in the cooling.
The copper of commerce is seldom pure, and this gives rise to many of
the imperfections met with in ordinary brass.
ZINC.
=100.= This is an elementary metallic body of a bluish white color. It
is used in the form of rods, for compensation pendulums.
It must be obtained of great purity, whether it is employed by itself
or to alloy with another metal. The presence of foreign bodies in zinc,
even in very small quantities, has a marked influence on the physical
properties of an alloy into which it enters.
The purer the metal the more easily will it roll, and this fact can be
taken advantage of as a test of quality.
Although very brittle at 0° C. (32° F.) and 200°C. (400° F.), it has
a maximum malleability at about 100° C. (212° F.), the boiling point
of water; it should, then, be heated to this degree before bending,
rolling, hammering, etc.
It may be annealed in boiling water, or by heating to such a
temperature that water hisses when allowed to drop on to it.
It melts at 420° C. (790° F.) and volatilizes if raised to a red heat.
A sudden cooling, or the presence of arsenic or antimony, will render
zinc brittle. It must not be melted in cast iron vessels, as the
quality of zinc is deteriorated by the small quantity of iron it takes
up under such circumstances.
This metal possesses a great affinity for oxygen, and therefore
oxidizes very readily when fused.
It is usual, before pouring zinc that is intended for rolling, to
throw some pieces of the solid metal into the molten mass, the object
being to somewhat reduce the temperature, and thus prevent a too rapid
cooling, as, in that case, zinc is very brittle.
BRASS.
=101.= Pure copper is difficult to work with the graver or file, but
such is not the case when this metal is alloyed with zinc; we then
obtain brass, or, as it is sometimes termed, yellow copper.
Alloys containing copper, zinc, and tin are termed bronzes.
If a small quantity of lead, about 1 per cent. of its weight, be added
to brass, it renders the metal less fibrous, imparting to it a certain
degree of brittleness so that it is more easily worked with the graver,
file, drill, or the saw.
When the brass is required to be hammered, a portion of the lead is
replaced by tin; by this means the metal becomes more malleable, or, in
terms of the workshop, soft.
The color, tenacity, ductility, malleability, etc., vary with the
percentage composition of the alloy. It is, then, of the utmost
importance that a watchmaker be able to test and select the brass
before employing it in his work; metal that is excellent for
wire-drawing, for example, would be utterly useless for making an
escape wheel, since it would become distorted in the cutting in
consequence of its ductility. It belongs, in fact, to the class of
metals that will extend under the hammer without hardening (very soft
brasses).
The following is given as an analysis of brass very frequently employed
in horology: copper, 66 per cent., zinc, 33 per cent.; and lead, 1
per cent. But it must not be forgotten that this is only to be taken
as a mean. Both the proportions and the qualities vary with different
makers, doubtless also according to the degree of purity of the metals
employed in their manufacture.
=102.= =To select brass.= By following the directions given below
any watchmaker should be able to select the brass best suited to his
special requirements.
When the copper is in excess, zinc being proportionately reduced, the
brass is usually soft and of a beautiful golden color. On the other
hand, as the proportion of zinc is increased, the brass becomes more
and more brittle, and at the same time, more fusible; the color changes
to a light yellow, ultimately becoming greyish-white, and brass of this
nature is said to be “hard.”
Very soft brass chokes the file, and spreads without hardening under
the hammer; very hard brass, on the other hand, is fragile, liable to
crack when hammered cold, and breaks in passing through the draw-plate.
Metal of a good yellow shade, intermediate between the golden and the
pale yellow color, passes well through the draw-plate, spreads out
slowly under the hammer, but without cracking, until of about half the
initial thickness, and then resists the further action of the hammer,
which rebounds from it; such brass is usually found to be of good
quality for watchwork.
A sheet of brass is rarely homogeneous. If, after pouring, the metal
has been allowed to cool slowly, the interior will be crystalline, and
there will be an uneven fracture. This will cause the tenacity, etc.,
to vary throughout the mass. Similar differences are occasionally to be
observed between the two faces of the same plate, due to the phenomenon
of _liquation_; that is to say, to a tendency that characterizes
certain metals when melted together to separate from one another when
the cooling is not affected under proper conditions.
If the two surfaces of a plate be scraped clean at several points, and
drops, as nearly equal as possible, of very pure watch oil, be placed
on these clean surfaces, it may be taken as a rough indication that
the metals are uniformly distributed if the successive shades of color
of the oil as time goes on are the same at all the points experimented
upon.
Some watchmakers heat the brass to a red heat (which must never be
exceeded), and plunge it into nitric acid (equal parts acid and water).
By this means the entire surface is cleaned, and the above examination
is facilitated.
HAMMER HARDENING OF BRASS.
=103.= =Plates.= The selection of the metal will depend on the purpose
for which it is intended, and the thickness must be such that, when
hammered till of sufficient hardness, it will approximately equal one
dimension of the required object; for it is advisable to remove as
little of the surface metal as possible, a plate always hardening much
more at the surface than in the interior.
There is considerable difficulty in indicating clearly in a book the
exact mode of conducting the operation of hammer-hardening, and the
assistance of a competent master is essential, at any rate for the
first few trials. It must suffice to point out that the anvil, with
a slightly convex surface, and the hammer, of sufficient weight, must
be in very good condition and, if possible, polished on their faces;
the head of the latter should be rather convex, and the pene or chisel
end somewhat broad and gently rounded off in all directions, for it
will be needed as a means of bending the metal upwards; the curvature
being such that there is not a danger of starting a crack, etc., by its
means. We have already spoken of these two tools (=79=, =80=); it is
only necessary to add that a thick straw pad should be placed under the
anvil or block.
When one is compelled to use brass that is too thick, so that there is
much work to be done with the hammer to reduce the thickness to what is
required, it is a good plan to commence by elongating the metal in one
direction, striking with the pene of the hammer a series of parallel
blows in the direction of the required elongation; when the thickness
is two or three times that ultimately needed, the surface is smoothed
with the hammer-head and annealed; then it is brought to the right
thickness by another hammering in the manner explained below, but it
should be again pointed out that, when possible, metal of a suitable
thickness ought to be taken in the first instance, since too much
hammering has a detrimental effect.
Before hammer-hardening a plate, it must be dressed, an operation which
consists in rounding off the edges very carefully in order to prevent
their cracking, and in rounding the bottom and sides of internal angles
which, without such a precaution would occasion a rupture. After this
is completed, proceed to the hardening, using a rather heavy hammer,
and giving sharp blows along lines parallel to the sides of the plate;
commence from one of the corners in the case of a square plate; and
with a round plate let the blows be in circles. In the latter case,
work from the circumference towards the center, at the same time
gradually increasing the force of the blows, since the metal opposes a
greater resistance towards the center. If the work is done evenly and
without hurrying, the surface will remain fairly flat, a fact which
should be verified from time to time by the aid of a metal rule.
Round plates are sometimes hardened by commencing to hammer in the
center and working towards the circumference along two radii in
opposite directions; that is along a diameter. This first diameter
is then crossed by another at right angles; the intervals are filled
in with other diameters that must not touch until the entire surface
is covered, always taking care to work from the center towards the
circumference.
When the metal is thin only the hammer-head is used, but beyond a
certain thickness the pene of the hammer must be employed until about
half the required thickness is reached; the surface is planished and
the hardening finished with the face.
Blows that are irregular, too hard or roughly given, will cause the
metal to crack. Hurried working will disturb the molecular grouping
of the alloy; it will at the same time be heated and therefore
softened, thus losing all the good qualities that are anticipated from
hammer-hardening, namely increased body and elasticity. It was in order
to avoid this heating that the old watchmakers used to hammer the brass
in cold water, an excellent precaution which is too much neglected at
the present day.
Brass that is badly hammered, the blows being violent or irregular,
will spring out of shape on being cut and occasionally crack when
gilding.
If during the process of hammering, a crack is observed to be
commencing at the edge, it must be removed with a rat-tail file, all
sharp angles being rounded off; and when cracks immediately reappear
on continuing the operation, it is an indication that the metal cannot
support any further hammering cold.
If brass is compact or well forged it may be relied upon to preserve
the oil at pivots, etc., better, as oil is decomposed more rapidly in
presence of a finely divided metal.
=104.= =Brass rods.= Rods having a square section must only be hammered
on two opposite faces.
A rod of square section can be hammered on all four faces but it must
be first filed perfectly square; the hammering must not be pushed too
far, and the four angles must be maintained right angles. If some are
made obtuse and others acute, a flaw will be produced in the direction
of a diagonal.
The three following methods are employed in the case of round rods:
The first consists in hammering over the entire surface, the rod being
at the same time rotated on the anvil by hand; but this operation must
not be much prolonged, as the metal is liable to crack lengthwise.
The second method consists in reducing the diameter of an annealed
brass rod to about one-half or two-thirds its initial amount by causing
it to pass in succession through a number of holes of the draw-plate.
When the third method, which is due to Brocot, is adopted, one
extremity of the brass rod is gripped in the bench vise and the other
end in a hand vise, which is then caused to rotate round the rod as
an axis. If the torsion be continued until the metal is on the point
of breaking, it will be found to be very effectually hardened. This
method is resorted to with advantage for hardening pin-wire and the
metal for making pillars.
TO ANNEAL BRASS.
=105.= When it is necessary to considerably reduce the dimensions of a
piece of brass, either with the hammer, rolls or draw-plate, it must be
annealed from time to time.
The metal should not be heated to redness; it is supposed, rightly or
wrongly, that such a proceedings especially if repeated, separates
a portion of the zinc, or at least changes the mode in which it
is associated with the copper. Brass should be heated slowly and
uniformly, in a moderate fire, until the temperature is such that drops
of water thrown onto the surface are rapidly converted into vapour, or
paper turns yellow and begins to smoke. It is then withdrawn from the
fire and allowed to cool.
Brass is brittle when hot, so that it can only be worked cold.
When brass is annealed, just as when steel is tempered, the metal
should not be allowed to rest on a bad conductor of heat, such as wood
or stone, because there will be a tendency to uneven distribution of
the heat throughout the metal.
CAST BRASS.
=106.= This is usually brittle, owing to the fact that the copper
employed in its manufacture consists, as a rule, of all sorts of
scrap, from good or bad metal; moreover, from motives of economy,
the proportion of zinc is generally increased and, in pouring, the
precautions essential to avoid the effects of liquation (=102=), etc.,
are frequently neglected. Such an alloy must never be used for small
objects, it must be entirely excluded from a watch, and in a clock only
such pivots as are called upon to perform an insignificant amount of
work should be allowed to run in it.
In order to avoid injuring the file, or embedding in the metal any
particles of the hard coating of oxide that always covers rough
castings, it is usual to dip the object in dilute nitric or sulphuric
acid (=155=), by which the oxide is dissolved.
TIN.
=107.= This is an elementary body, almost as white as silver and having
a breaking strain of only 8 kilo. per sq. mm. of section (or 11,300
lbs. per sq. inch.)
Watchmakers use it in making solder. It is also sometimes used in the
form of plates or rods for polishing with rouge, and it is said to be
much more efficient when very pure.
If a strip of pure tin is bent, a crackling noise, termed the “crying”
of tin, is heard. After frequent bending, the metal loses this property.
The degree of purity may be judged:
(1) By the loudness of the “cry,” which is found to be greater as the
tin is purer;
(2) By the relative lightness of two balls of equal size, one of which
is formed of very pure tin and used as a standard;
(3) By pouring the metal, when just melted, in a mould 1 or 2
centimetres (about ¾ inch) in diameter. If tin is pure, when cast
into plates or ingots, the surface will be perfectly smooth, without
exhibiting any sign of crystallization at the moment of solidification,
whereas the presence of small quantities of foreign metals causes it to
be covered with a network of needle-formed crystals, which are the more
numerous according as the metal is less pure.
The Banca tin is almost chemically pure; English tin is also very pure;
but others contain a small percentage of copper, lead, iron, or arsenic.
BRONZE.
=108.= Bronze is an alloy, in very variable proportions, of copper
and tin, to which may be added, according to circumstances, a small
percentage of lead or zinc, or even iron, when it is desired to
increase the hardness or tenacity.
As a rule, this alloy is tough and hard to work; it is especially used
for parts of large machines that are subjected to considerable pressure.
The fusion and casting of bronze require special precautions, for the
proportion between the metals is liable to vary through oxidation of
the tin, which then goes to form a dross, and the composition may
vary throughout the mass. It sometimes results from this that the
bronze bearings for the pivots in large clocks are not even as good as
ordinary brass, and wear away more rapidly than the pivots.
Bronze is also used by watchmakers for making plates or small rods
for polishers, and for the bells of clocks. Bell-metal contains about
78 per cent. of copper and 22 per cent. of tin; it has a beautiful
fracture, and is very fusible and sonorous. The addition of any other
metal is rather prejudicial than otherwise; this explains why so many
clock bells are wanting in sonorousness.
An impediment to the use of bronze is its want of malleability; but
Dronier has recently pointed out that such alloys may be rendered
perfectly ductile and malleable by adding from ½ to 2 per cent. of
mercury. These alloys are said to be less oxidizable than ordinary
bronzes, and at the same time more hard, elastic, resisting and
sonorous.
STERRO.
=109.= This is an alloy containing 56 per cent copper, 41 zinc, 2 tin
and 1 iron. It resembles a reddish-colored brass, and has been much
used in Vienna, where it is considered superior to brass from the point
of view of ductility, tenacity and malleability.
An experienced horologist, M. Grossmann, made satisfactory lever
escape-wheels of it, and he considers it to be superior to the best
brass in regard to both density and elasticity. At the same time he
points out that it clogs the cutter, and the color is inferior to that
of good hard brass.
LEAD.
=110.= A metal with a brilliant bluish grey lustre, which rapidly
becomes dull when exposed to the air. It is very malleable and ductile.
It breaks with a strain of 2.9 kilo. per sq. mm. section (4,000 lbs.
per sq. inch), but possesses extreme flexibility.
Lead is not used in horology, except as a constituent of solders; in
these, however, it plays a very important part. It is occasionally
used in the pure state as a lap for applying polishing materials, but
more frequently alloyed with tin, by which hardness is imparted to the
metal, the alloy being known as “pewter.”
NICKEL.
=111.= An elementary metallic body of a greyish-white color, resembling
that of platinum. With care it can be forged when hot and formed into
plates; its structure in that case is fibrous. Its hardness is the same
as that of iron, and nickel will take a high polish. Next to iron, it
is the most powerfully magnetic of all metals.
It can be caused to alloy with many other metals—notably iron, cobalt,
copper, zinc, tin, and antimony. According to Stodart and Faraday,
an alloy of 33 parts iron and 1 part nickel is as malleable as the
former metal, but less liable to rust. Fleitmann has recently shown
that by the addition of about 1-10th per cent of magnesium, nickel is
rendered perfectly malleable and ductile, capable of being drawn into
wires or rolled into sheets, and Garnier finds that 3-10ths per cent of
phosphorus has a similar effect.
Nickel is useful as a coating for objects that are not subjected to
friction, for preserving them from the action of the air. It takes a
beautiful polish, and is not tarnished by being touched.
GERMAN SILVER.
=112.= Although the proportion of copper in this alloy is considerably
greater than that of nickel, watchmakers frequently apply the latter
name to it, doubtless on account of the beautiful polish of which the
metal is capable and the comparative inoxidizability which it derives
from the presence of nickel.
German silver is an alloy of copper, nickel and zinc, with the
occasional admixture of a small proportion of iron or tin. When used in
the construction of objects that require soldering, 2 per cent. of lead
is added.
The alloy usually employed in horology is very malleable; it has a mean
composition: copper, 60 per cent; nickel, 20 per cent; and zinc, 20 per
cent. That containing 58 per cent copper, 14 nickel, 25 zinc, and 3
iron, is said to be highly elastic.
The following useful details with regard to the employment of German
silver for watchwork are due to M. C. E. Jacot.
Watch movements have been made of this alloy for the past thirty years;
it was long thought that the taste would die out, but, on the other
hand, the demand for “nickel” movements increases each year.
The alloy is better prepared at the present day; it has a beautiful
grayish-white colour, it is more malleable, and better to work than
formerly, but still not so easy as brass. The latter alloy is less
detrimental to the file, and can be turned and drilled more rapidly.
German silver is only used for the plates, cocks and bars. The barrels
and wheels are of brass, and surfaces exposed to friction, such as the
center pivot-hole (all other holes being jewelled) are bushed with
the same metal, for it is observed that in presence of nickel oil is
rapidly blackened and the pivots wear sooner than when working in good
brass.
The color remains unaltered for a long time if the surface has been
carefully smoothed in the first instance; and if cleansed with soap and
water, its original freshness can be to a great extent restored. Some
watchmakers prefer to employ chemical preparations for cleaning the
metal.
The following is recommended as very effective for this purpose: Mix 50
parts alcohol, 1 part sulphuric, and one part nitric acid. Allow the
pieces to remain in this liquid for 10 or 15 seconds, wash with cold
water, and subsequently with alcohol, dry with a soft rag or in boxwood
saw dust.
GOLD.
=113.= An elementary body, the most beautiful and the most valuable of
all the ordinary metals. In the unalloyed state it has a pure yellow
color, and when reduced to extremely thin leaves, appears green by
transmitted light. It is the most malleable and ductile of all the
metals, but its tenacity is low.
Gold resembles platinum, silver, iron, etc., in being capable of
welding, that is to say, two pieces of the metal can be united without
previous fusion. Indeed, by the application of great pressure it can be
made to weld when cold.
It is insoluble except in aqua regia (a mixture of 1 part nitric acid
and 4 parts hydrochloric acid), alkaline persulphides and selenic acid.
Chlorine, phosphorus, and a few other substances can be made to combine
with it by the acid of heat.
It is as a preservative, that is applied in layers termed “gilding,”
that gold is principally used in watchwork, and some details will be
found on this subject under “Gilding,” (articles =142=-=153=). Owing to
its softness the metal is not used in a pure state, but usually alloyed
with copper. The principal alloys in use in this country are:
22 parts (carats) gold, 2 parts (carats) copper, for coin and wedding
rings.
18 parts gold, 6 parts copper, for high-class jewelry and watch-cases.
15 parts gold, 9 parts copper, for ordinary jewelry.
12 parts gold, 12 parts copper; and 9 parts gold, 15 parts copper, for
common jewelry.
The alloys used for soldering gold will be described under “Solders”
(=126=).
Alloys of gold with silver and copper have been employed for making
watch wheels; they wear well, and will take a beautiful polish, which
is maintained for a longer time than in the case of brass wheels.
Chronometer balance-springs and the suspension-springs for astronomical
clocks have also been made of gold-copper or gold-silver alloys rolled
and hardened (=591=.) If carefully prepared, they maintain their
elasticity unimpaired for a long period, and there is no liability to
rust.
The dilatation for a given change of temperature is, however, greater
than that of steel, so that a greater compensating effect becomes
necessary, but this inconvenience is partially compensated for by its
inoxidizability and the fact that it is not liable to become magnetic.
SILVER.
=114.= This metal in an unalloyed state is too soft for use in
horology; its principal use is for cases, and as a constituent of
solders.
Houriet made watch wheels of an alloy containing 2 parts silver to 1
part 18-carat gold, and he affirmed that this alloy became polished at
the acting surfaces of the teeth. Jurgensen states that chronometer
escape-wheels made of this alloy, carefully hammered, do not require
oil at the points of their teeth.
Dumesnil proposed an alloy of 2 parts copper, 1 part silver, and 1 part
zinc, all perfectly pure. Lecocq made chronometer balances in which the
brass was replaced by pure silver deposited on the surface of the steel
by electrolysis, thus avoiding the use of a fire. The compensation is
said to have been very efficient.
ALUMINIUM AND ALUMINIUM BRONZE.
=115.= Aluminium is an extremely light elementary body, having a
density of only 2.56; with equal bulks, therefore, it will weigh only
about as quarter as much as silver. As its capacity for heat is very
great, this metal is observed to heat or cool more slowly than other
metals.
Pure, or in a slightly alloyed state, it has not been used in horology,
except for pendulum rods and large hands in regulator clocks; in short,
it can be employed where lightness is the principal quality in view.
It is extremely ductile. The presence of 1-100th part of bismuth,
however, renders the metal somewhat brittle, and it develops cracks
under the hammer. Traces of iron also decrease its malleability.
An alloy of 5 parts silver and 95 aluminium can be as easily worked as
the pure metal, but is harder and takes a better polish.
We would add a curious observation of M. Redier: After passing a piece
of aluminium several times through the draw-plate, he observed that the
elongation had only occurred at the surface; for on cutting the wire at
different points, he noticed that, throughout a portion of the length,
the metal was hollow, a very fine capillary tube being thus formed.
=116.= _Aluminium Bronze_ is an alloy of aluminium with copper. A
alloy of 5 parts of the former to 95 of the latter has a beautiful
golden color, but if the proportion is changed to 10 and 90 parts
respectively, we obtain the most serviceable and the most easily worked
alloy.
This bronze can be forged at a cherry-red heat, and even near its
melting point; and its thickness can be reduced to a very small amount
under the hammer. It is easily filed and turned, but does not possess
any special advantage over brass, which is less detrimental to the
file; the density is 7.7, very little below that of brass, 8.4.
It appears from a considerable number of experiments that it might
be used with advantage for the bearings of axes that rotate with
high velocities. It resists wear better than any other metal. In the
experiments made by Foucault to demonstrate the rotation of the earth
by means of the pendulum, he found that an aluminum bronze wire lasted
for the longest period. Its tenacity is equal to that of iron. It has
been shown that slide-bars of locomotives made of this bronze resist
wear twice as long as those formed of the ordinary bronze. There would
then be an advantage in using it for the bearings of foot-lathes, etc.
Grossman asserts that lever escape-wheels of this metal have proved
satisfactory, and he makes the following observation on the subject. If
aluminium bronze be reduced to three-fourths of its original thickness
by hammering, it will begin to crack. This can be prevented by heating
to a red heat and plunging into water; it can then be again reduced by
one-fourth of its thickness, and again annealed, and so on. He reduced
the thickness from 2.5 millimeter to 0.2 millimeter, and the metal
resisted for a long period repeated flexures backwards and forwards;
and he observes that no other metal, after being so much compressed,
would possess the same marvellous degree of tenacity.
In order to obtain aluminium bronze of the best quality, the copper
should be absolutely pure, and, in the manufacture, the alloy must be
melted and forged two or three times in succession, as by this means
the strength and tenacity are increased, and the metal can be more
easily worked.
The beautiful golden color possessed by certain of these bronzes when
polished, has caused them to be used for cheap watch-cases, but they
always tarnish at those parts that are not subject to daily wear.
MERCURY.
=117.= This is the only metal liquid at the ordinary temperature; it
solidifies at -40° C. (-40° F.). It possesses a high metallic lustre,
resembling silver, but with a slightly bluish tint, and does not
oxidize at ordinary temperatures.
Mercury alloys with many other metals, forming amalgams, and as small
a quantity as 1-40th per cent of lead suffices to entirely alter its
character. The presence of such traces can be easily detected by the
liquid wetting glass or china, and therefore forming a tail when a
vessel containing it is tilted.
The commercial metal is rarely pure, but the greater portion of the
lead, tin, bismuth or copper, by which it is contaminated, can be
removed by distillation. The most convenient method consists, however,
in agitating the metal with either dilute nitric acid, a solution of
mercurous nitrate, strong sulphuric acid, a solution of corrosive
sublimate or of perchloride of iron, and subsequent washing with
distilled water. When mercury is only contaminated with mechanical
impurities, they can be very effectually removed by agitating with
powdered loaf sugar.
This metal has many uses in the arts, for the construction of
thermometers, barometers; for plating, etc.; in horology it is used
for compensation pendulums, and has also been occasionally used for
compensation balances.
PLATINUM.
=118.= This elementary body is almost as white as silver, takes a
brilliant polish, and is highly ductile and malleable. It is the
heaviest of the ordinary metals, the least expansive when heated, and
has a breaking strain of 40 kilo. per sq. mm. section (56,500 lbs. per
sq. inch.).
Platinum is infusible, except at the high temperatures attainable with
the oxy-hydrogen blow-pipe. At a white heat, however, it softens,
and can be forged and welded. It is unacted upon by the air at any
temperature, and is insoluble in acids, except aqua regia (=155=),
although acted on by certain alkalies.
This metal is used in the construction of scientific instruments, and
for objects that are exposed to the air, as, for example, sun dials.
Alloyed with irridium, (a rare metal of the same group) it possesses an
excellent and unalterable surface for fine engraving, as the scales of
astronomical instruments, etc. This alloy has also been adopted for the
construction of international standards of length and weight.
Platinum is much employed for chemical apparatus, in consequence of its
being unacted on by acids, and its non-liability to melt in ordinary
furnaces. Both the pure metal and its alloys with silver have been
employed in the form of wire for bushing the pivot-holes of watches,
and in sheets for cutting out cocks and wheels, but the results
obtained were not as good as with good brass. As a rule, such wheels
are found to occasion a rapid wear of pinion leaves.
Attempts have also been made to construct balance-springs of this
metal, but we are informed that they were not found to possess any
sufficient advantages.
It is advisable to heat platinum in a spirit lamp or Bunsen burner; the
naked flame is objectionable, because, being charged with a certain
amount of carbon, it deteriorates the metal.
PALLADIUM.
=119.= This metal resembles silver rather than platinum, and is almost
as infusible as the latter metal. It has a density of 12.5. When heated
in contact with air it becomes blue, owing to the formation of an
oxide. It possesses the remarkable power of absorbing (or _occluding_)
about 900 times its own volume of hydrogen, if attached to the negative
pole of a battery in acidulated water; its bulk is increased slightly
by this charge, and, on expelling the gas by the aid of heat, the
metal shrinks to less than its initial dimensions. Palladium is useful
for the graduated scales of scientific instruments, since it is not
discolored by sulphurous acid. It forms alloys with most of the metals
and some of these can be hardened like steel. If 100 parts of steel be
alloyed with 1 part of this metal, the resulting alloy is said to be
excellent for making scientific instruments, and an alloy of 24 parts
palladium, 44 silver, 72 gold, and 92 copper has been recommended for
use in horology.
M. Paillard, of Geneva, has introduced balance-springs made of an
alloy, whose composition is not given, possessing the following
advantages: they are non-magnetic, their tenacity is considerable, are
not tarnished by the air, sulphurous acid, or sea water; nor are they
distorted by heating, and, on cooling, they recover their original
elasticity, which is equal to that of steel hardened and tempered to a
blue color. The co-efficient of expansion of this alloy is rather less
than that of steel.
CHARACTERISTIC PROPERTIES OF ALLOYS.
=120.= _Density._ This is sometimes rather greater and sometimes less
than that deduced from the densities of the constituent metals,[4] but
no exact law has been discovered in regard to this question.
_Hardness, Ductility, Tenacity._ Alloys are usually harder, more
brittle, and less ductile and tenacious than the most ductile and
tenacious constituent metal.
_Elasticity._ The co-efficient of elasticity of an alloy generally
approximates closely to the mean of the co-efficients of its
constituent metals.
_Expansion._ The co-efficient of linear expansion of an alloy, that is
to say, the number representing the proportional part of its length
by which it increases for each degree rise of temperature, may be
approximately estimated as follows: multiply the linear co-efficient of
each constituent metal by the percentage of it present in the alloy,
and divide by its density. Add together the several numbers thus
obtained. Multiply this sum by the density of the alloy (which must be
experimentally determined) and divide by 100. The resulting figure is
the required linear co-efficient (=122=).
_Fusibility._ Alloys are always more fusible than the least fusible of
their component metals, and often more so than any one of them.
_Oxidation._ As a rule, the air acts with less energy on alloys than
on their constituent metals. There are, however, cases in which the
converse is the case.
_Action of acids._ This is generally similar to the action on the
predominating metal.
_Observations._ Alloys formed of metals that differ materially in
density are rarely homogeneous, especially if they have been allowed
to cool slowly. It is, then, essential that they be thoroughly stirred
and cooled rapidly. It is for this reason that alloys are frequently
poured out on to a flagstone to cool, or that they are compressed after
pouring, whereby the formation of crystals is prevented.
=121.= =Metals and alloys.= The following table gives the more
important physical properties of the metals and alloys generally met
with, and will be found useful for reference. The precise meaning of
each number may be gathered from the notes in paragraph =122=.
+-------------------+------------+----------+-----------------------+
| | Specific | Degree | Linear Expansion |
| METALS. | Gravity. | of | per |
| | (Water=1) | Hardness | 1° Fahr. 1° Cent. |
+-------------------+------------+----------+-----------+-----------+
|Aluminium (115) | 2.56 | -- | 0.0000123 | 0.0000222 |
| ” Bronze (116)| 7.7 | -- | -- | -- |
|Brass, Drawn (101) | 8.54 | -- | 0.0000107 | 0.0000193 |
| ” Cast (106) | 8.10 | -- | 0.0000104 | 0.0000187 |
|Bronze (108) | 8.40 | -- | 0.0000100 | 0.0000180 |
|Copper (99) | 8.94 | 2.5-3 | 0.0000102 | 0.0000183 |
|German Silver (112)| -- | -- | -- | -- |
|Gold (113) | 19.26 | 2.5-3 | 0.0000077 | 0.0000138 |
|Iron, Wrought (54) | 7.84 | 4.5 | 0.0000066 | 0.0000119 |
| ” Cast (58) | 6.9 to 7.5 | -- | 0.0000062 | 0.0000112 |
|Lead (110) | 11.33 | 1.5 | 0.0000167 | 0.0000301 |
|Mercury (117) | 15.60 | -- | 0.000101 | 0.000182 |
|Nickel (111) | 8.82 | 5 | [cubical | [cubical |
|Palladium (119) | 11.80 | 4.5-5 | -- | -- |
|Platinum (118) | 21.50 | 4-4.5 | 0.000005 | 0.000009 |
|Silver (114) | 10.57 | 2.5-3 | 0.0000111 | 0.0000190 |
|Steel (60) | 7.72 | 6-7(hard)| 0.0000057 | 0.0000103 |
|Sterro (109) | -- | -- | -- | -- |
|Tin (107) | 7.30 | 2.5-3 | 0.0000152 | 0.0000273 |
|Zinc (100) | 7.13 | 2 | 0.0000122 | 0.0000220 |
+-------------------+------------+----------+-----------+-----------+
+-------------------+---------------+---------+---------------------+
| | Specific Heat | Melting | Conductivity |
| METALS. | per Degree | Point. | for |
| | Cent. | | Heat. Electricity. |
+-------------------+---------------+---------+--------+------------+
|Aluminium (115) | 0.2143 | 1500° F.| -- | 56.1 |
| ” Bronze (116)| -- | [about| -- | -- |
|Brass, Drawn (101) | } 0.0939 | { -- | -- | -- |
| ” Cast (106) | } | { 1870° | -- | -- |
|Bronze (108) | -- | 1692° | -- | -- |
|Copper (99) | 0.0951 | 2000° | 73.5 | 99.8 |
|German Silver (112)| -- | -- | -- | 7.67 |
|Gold (113) | 0.0324 | 2610°
Read full text (200,001 characters)
Fields
| author | Claudius Saunier |
|---|---|
| language | English |
| chars | 862616 |
| source_url | https://www.gutenberg.org/ebooks/76850 |
Cite this record
MLA
"The watchmakers' hand book." Project Gutenberg, n.d., https://gutenberg.go-v.org/record/76850.
Chicago
"The watchmakers' hand book." Project Gutenberg. n.d.. https://gutenberg.go-v.org/record/76850.
APA
Project Gutenberg. (n.d.). The watchmakers' hand book. https://gutenberg.go-v.org/record/76850