Non-technical chats on iron and steel, and their application to modern industry
The Project Gutenberg eBook of Non-technical chats on iron and steel, and their application to modern industry This eBook is for the use of anyone anywhere in the United States and most other parts of the world at no cost and with almost no restrictions whatsoever. You may copy it, give it away or re-use it under the terms of the Project Gutenberg License included with this eBook or online at www.gutenberg.org. If you are not located in the United States, you will have to check the laws of the country where you are located before using this eBook. Title: Non-technical chats on iron and steel, and their application to modern industry Author: La Verne W. Spring Release date: March 3, 2024 [eBook #73090] Language: English Original publication: New York: Frederick A. Stokes, 1917 Other information and formats: www.gutenberg.org/ebooks/73090 Credits: Richard Tonsing, deaurider, and the Online Distributed Proofreading Team at https://www.pgdp.net (This book was produced from images made available by The Internet Archive.) *** START OF THE PROJECT GUTENBERG EBOOK NON-TECHNICAL CHATS ON IRON AND STEEL, AND THEIR APPLICATION TO MODERN INDUSTRY ***
The Project Gutenberg eBook of Non-technical chats on iron and steel, and their application to modern industry
This eBook is for the use of anyone anywhere in the United States and
most other parts of the world at no cost and with almost no restrictions
whatsoever. You may copy it, give it away or re-use it under the terms
of the Project Gutenberg License included with this eBook or online
at www.gutenberg.org. If you are not located in the United States,
you will have to check the laws of the country where you are located
before using this eBook.
Title: Non-technical chats on iron and steel, and their application to modern industry
Author: La Verne W. Spring
Release date: March 3, 2024 [eBook #73090]
Language: English
Original publication: New York: Frederick A. Stokes, 1917
Other information and formats: www.gutenberg.org/ebooks/73090
Credits: Richard Tonsing, deaurider, and the Online Distributed Proofreading Team at https://www.pgdp.net (This book was produced from images made available by The Internet Archive.)
*** START OF THE PROJECT GUTENBERG EBOOK NON-TECHNICAL CHATS ON IRON AND STEEL, AND THEIR APPLICATION TO MODERN INDUSTRY ***
NON-TECHNICAL CHATS ON IRON AND STEEL
AND THEIR APPLICATION TO MODERN INDUSTRY
BY
LA VERNE W. SPRING, A.B.
CHIEF CHEMIST AND METALLURGIST, CRANE CO., CHICAGO
_WITH TWO HUNDRED AND NINETY-FOUR ILLUSTRATIONS AND DIAGRAMS_
[Illustration: [Logo]]
NEW YORK
FREDERICK A. STOKES COMPANY
PUBLISHERS
_Copyright, 1917, by_
FREDERICK A. STOKES COMPANY
_All rights reserved, including that of translation
into foreign languages_
TO
MY FELLOW WORKERS
IN THE VAST IRON AND STEEL INDUSTRY
THIS BOOK IS
AFFECTIONATELY DEDICATED
FOREWORD
It has long been a desire of the author to put into non-technical form
the interesting data here given. During several years spent in the
service of one of the great steel companies of this country, first in
the laboratories and afterward in the rolling mills, he acquired a love
for the industry that is now of fairly long standing. Spending as much
of his spare time then and since in visiting various parts of that
mammoth plant and as many others as he was able, he has always felt that
this extremely interesting subject could not fail to prove fascinating
even to those who had previously known little of the manufacture of
steel and steel products. Later work with gray and malleable cast irons
and with cast steel enlarged the outlook and further urged his sharing
these interesting things with others not so fortunately situated.
Such an inspiration, if it may so be called, is the reason for the
appearance of these articles. Practically as here reprinted, the first
thirteen of them were published during 1915 and 1916 in serial form in
the “Valve World,” the house organ of Crane Company of Chicago, with
which the writer for some time has been connected. The enthusiasm with
which they were received has been very gratifying, while the scores of
letters bearing favorable comment testify to the correctness of the
judgment that the metallurgy of our most useful metal, iron, is of very
general interest.
It may be remarked by some that certain of the statements made in the
book are not strictly accurate in that few details have been stated or
exceptions made. This is true, but it seemed necessary if main facts
were to be made to stand forth with the boldness required to accomplish
the purpose which the author had in mind. The chapters are in no way
intended to be an encyclopedia of the subject. The idea throughout has
been to present only the main points and to show the derivation of the
products from the raw materials and their relationships to each other.
In other words the book is intended only as a sort of outline.
References are given which will aid in the selection of works to be
consulted by any who are sufficiently interested to go farther.
Without the encouragement and coöperation of Crane Company and the kind
assistance of friends, some within and some without the iron and steel
industry, this little book would not have been possible. Special mention
must be made of the aid given by Messrs. I. M. Bregowsky, J. A.
Matthews, C. D. Carpenter, and others whose reading of and suggestions
concerning parts of the manuscript were of much help. Thanks are due
also to many individuals and firms for their very hearty coöperation in
furnishing information and the photographs which appear in the pages of
the book.
L. W. S.
_Illustrations are from the following sources:_
A. M. Byers Co., Pittsburg.—National Tube Co., Pittsburg.—U. S. Steel
Corporation, New York.—Tennessee Coal, Iron & Railroad Co., Birmingham,
Ala.—Shenango Furnace Co., Pittsburg.—Pickands, Mather & Co.,
Pittsburg.—United States Geological Survey.—Wellman-Seaver-Morgan Co.,
Cleveland, O.—Lackawanna Steel Co., Buffalo.—Cleveland-Cliffs Iron Co.,
Ishpeming, Mich.—J. H. Hillman & Sons Co., Pittsburg.—Harbison-Walker
Refractories Co., Pittsburg.—By-Products Coke Corporation, Chicago.—H.
Koppers Co., Pittsburg.—Federal Furnace Co., Chicago.—Crucible Steel
Company of America, Pittsburg.—Crane Co., Chicago.—Interstate Iron &
Steel Co., Chicago.—LaBelle Iron Works, Steubenville, O.—Morgan
Construction Company, Worcester, Mass.—J. A. Matthews. Syracuse, N.
Y.—McLain’s System, Milwaukee, Wis.—Allis-Chalmers Co., Milwaukee,
Wis.—J. H. Williams & Co., New York.—Griffin Wheel Co., Chicago.—U. S.
Molding Machine Co., Cleveland.—Bradley Manufacturing Co., Bradley, Ill.
(Sears, Roebuck & Co., Chicago).—Snyder Electric Furnace Co.,
Chicago.—Commonwealth Steel Co., St. Louis.—John A. Crowley & Co.,
Detroit.—Illinois Steel Co., Chicago.—Pickands, Brown & Co.,
Chicago.—“Sketches of Creation,” by Alexander Winchell. Harper & Bros.,
New York.—“Descriptive Metallurgy of Iron,” by S. Groves.—“Materials of
Engineering,” by R. H. Thurston. John Wiley & Sons, New York.—“Chambers’
Encyclopedia.” J. B. Lippincott, Philadelphia.—“Cast Iron in the Light
of Recent Research,” by W. H. Hatfield. Charles Griffin & Co., Ltd.,
London.—“Handbook of Chemical Technology,” Wagner-Crookes. D. Appleton &
Co., New York.—“The Ore Deposits of the United States and Canada,” by J.
F. Kemp. McGraw-Hill Book Co., New York.—“The Valve World.” Crane Co.,
Chicago.—“The Romance of Steel,” by H. Casson. A. S. Barnes & Co., New
York.—“The Metallurgy of Steel,” by Harbord & Hall. Chas. Griffin & Co.,
Ltd., London.—“Metallurgy of Steel,” by H. M. Howe. McGraw-Hill Book
Co., New York.—Tomlinson’s “Encyclopedia of Useful Arts” (1854). G.
Virtue & Co., New York.—“Liquid Steel,” by E. G. Carnegie. Longmans,
Green & Co., New York.—“Iron and Steel in All Ages,” by James Swank.
American Iron & Steel Association, Philadelphia.—“The A.B.C. of Iron and
Steel.” Penton Publishing Co., Cleveland, O.—“The Iron Age.” David
Williams, New York.—“The Iron Trade Review.” Penton Publishing Co.,
Cleveland, O.—“High Speed Steel,” by O. Becker. McGraw-Hill Book Co.,
New York.
[Illustration: CONTENTS]
CHAPTER PAGE
I THE EARLY HISTORY OF IRON 1
II THE RAW MATERIALS 17
III RAW MATERIALS (_Continued_) 37
IV THE BLAST FURNACE 52
V A GENERAL GLIMPSE AHEAD 69
VI WROUGHT IRON 91
VII CEMENTATION AND CRUCIBLE STEELS 106
VIII BESSEMER STEEL 123
IX THE OPEN-HEARTH PROCESS 142
X CAST IRON 160
XI CAST IRON (_Continued_) 178
XII MALLEABLE CAST IRON 195
XIII CAST STEEL 214
XIV THE ALLOY STEELS 233
XV THE HIGH-SPEED STEELS 240
XVI THE MECHANICAL TREATMENT OF STEEL 245
XVII THE ROLLING PROCESS 259
XVIII THE ROLLING OF RODS 277
XIX WIRE AND WIRE DRAWING 284
XX THE MANUFACTURE OF PIPE AND TUBES 292
XXI THE MANUFACTURE OF SEAMLESS STEEL TUBES 302
XXII TRANSFORMATIONS AND STRUCTURES OF THE STEELS 310
XXIII THE EQUILIBRIUM DIAGRAM OF THE IRON-CARBON ALLOYS 335
REFERENCES 350
INDEX 355
NON-TECHNICAL CHATS ON IRON AND STEEL
CHAPTER I
THE EARLY HISTORY OF IRON
[Illustration:
PREHISTORIC MAN
]
When in imagination we see the iron maker of early days sitting
cross-legged on his platform between two crude bellows formed from goat
skins with slits for air intakes and nozzles of bamboo, working them
alternately to deliver their pitifully small streams of air into the
hole in the side of a bank of clay which served as a furnace, we wonder
at his patience; and after long hours of such effort his reward was only
a few pounds of iron!
Contrast with this, if you please, the modern blast furnace with its
towering height of 100 feet, its four huge heating stoves, the big
blowing engines which each minute deliver to the furnace 50,000 cubic
feet of blast, and the whole array of dust arresters, gas washers, and
automatic ore and coke handling machinery which are essentials of this
king of modern metallurgical devices. How insignificant seems the output
of the ancient furnace when compared with the daily yield of 500 tons
from this giant of to-day!
How has this come about?
[Illustration:
THE FIRST RAZOR
]
Looking back over the centuries we see a period many thousands of years
ago when primitive man lived in caves or other rude habitations and was
entirely without the implements which we now consider indispensable. The
weapons with which he defended his wife and babes from the wild beasts
and from his warlike neighbors were clubs, wooden spears with perhaps a
bone or shell tip, and hatchets of chipped stone tied with thongs of
hide into a split stick. He managed by ingenious snares and his crude
weapons to provide game and fish for the support of his family.
He did not shave often, for his wife was not as particular in regard to
his appearance as are modern women, but when such a thing happened, a
piece of shell was his razor. The good wife had no steel needles with
which to sew together skins for their crude clothing. If she darned her
husband’s socks it is not recorded, nor did she use steel crochet hooks
in making the “doilies” for their parlor table.
When grain began to supplement the wild game, fruit, and berry diet, it
was broken between flat stones or ground in stone mortars. Fires were
kindled after long and laborious twirling or rubbing together of two dry
pieces of wood. With his stone hatchets and by liberal burning away of
parts by fire he formed his canoes from trunks of fallen trees.
This was the “Stone Age,” and iron and steel were unknown and not to be
heard of for many thousands of years.
In various parts of the world copper always has occurred “native”; i.e.,
in the metallic form and not in combination with other elements as an
earth or ore. As the centuries rolled on, man eventually learned that
this soft red metal could be pounded into thin-edged implements and that
it made more useful tools than those of stone, which his ancestors had
taught him to form. Some of these metal implements were hard and had
fairly good cutting edges, made so by accidental or intentional presence
of tin, and little did he dream that the twentieth century upon finding
his buried bronze implements would think his crude alloy so wonderful
and talk reverently of a “lost art of tempering copper.”
[Illustration:
IMPLEMENTS OF THE STONE AGE
]
Gold, too, became known to him because it also occurs “native.” Its
melting point was low enough that he could fashion it into ornaments,
idols, and other articles for religious purposes. But during the
hundreds of centuries of the “Stone Age” and during much of this—the
“Bronze Age”—copper, bronze, and gold were the only metals used. Though
the smiths became very dextrous in casting and modeling these metals,
they yet knew not iron or steel.
[Illustration:
IMPLEMENTS OF THE BRONZE AGE
]
Round about them during these many centuries, as multi-colored earths or
rocks, were the ores of various metals. They little dreamed that when
rightly treated certain of the heavy red, yellow, or black earths which
lay right at their doors could give up that most useful metal, iron. No
one even had knowledge of such a substance, for, unlike copper and gold,
iron never occurs “free,” having too great a tendency to chemically
combine with other elements, for example, oxygen of the air, with which,
in moist climates, it so readily forms “iron rust.” Besides, its melting
point is high and so much heat and carbon are needed for its “reduction”
from the ore that, during the thousands of years that had gone before,
it had never been produced.
[Illustration:
PRIMITIVE FURNACE FOR SMELTING IRON
]
But one day by accident and under fortunate coincidence of rich ore,
high heat, and plenty of carbon in the form of charcoal from the wood, a
lump of metallic iron was formed underneath a pile of logs which had got
afire and burned fiercely because of a high wind. When pounded between
two stones this new heavy metal, too, was malleable and could be formed
into a spearhead superior to anything yet known. Every one was
interested and an observant one soon “doped out” that certain earths
could be made to yield this new metal, iron.
The art of extracting it spread slowly, each artisan learning from his
neighbor, and, as rich ores were plentiful in many districts, iron
became more and more generally produced. Not only in one country was
this so but evidence shows that in many others—in Egypt, Chaldea,
Borneo, India, China, etc.,—roughly similar processes and crude furnaces
came to be used.
Tubal-Cain, supposedly about 4000 years B.C., is mentioned in the Bible
as an “artificer in iron and brass,” and a wedge of wrought iron was
buried in the great pyramid of Cheops probably as early as 3500 B.C.
This wedge was recently found and is now the property of the British
Museum. The Chinese made use of iron many centuries before the Christian
era, but the Assyrians are supposed to have been the first to use the
metal on a really extensive scale.
[Illustration:
THE PILLAR AT DELHI, INDIA
]
The much discussed pillar at Delhi, India, which is still standing in a
remarkable state of preservation, is twenty-two feet high. It is made up
of several wrought iron sections cleverly welded together. As the
natives regard it with religious awe, metallurgists have been unable to
make thorough investigation and chemical analysis. While the date of its
erection is somewhat in doubt, it is supposed to have been about the 4th
or 5th century A.D.
But from our modern viewpoint those early iron furnaces were queer
things. The first were little more than piles of ore and wood or
charcoal on the tops of hills where a brisk wind would make a hot fire.
Later, with the invention of the crudest of bellows, the smelting was
done in small holes in the side of banks of clay, charcoal made from the
forest trees being used as fuel. Indeed, some of these types of furnaces
still exist and are so operated to-day in neglected districts in Western
India and elsewhere, producing their little five to 100 pound balls of
iron after several hours of tedious work.
When the Romans invaded Britain (now England), they found the Britons
making iron in crude furnaces called bloomaries; and not a great deal of
improvement, except in size, was made up to Queen Elizabeth’s time, when
strict laws had to be enacted to prevent destruction of the forests
which were being denuded for production of charcoal, coke, which we know
so well, not yet having been produced for fuel.
[Illustration:
MILADY’S NEEDLE
]
[Illustration:
THE CATALAN FORGE
]
But the real forerunner of our modern blast furnace was the Catalan
forge, developed in and named from Catalonia, north Spain, where it
originated. The Catalan, however, and all of such crude early furnaces,
including those thus far described, produced a variable kind of what we
now know as “wrought iron,” and our modern “cast” iron did not appear
until about 1350 when, with larger furnaces, an excess of charcoal, with
greater heat and other favorable conditions, the Germans found that the
pasty, difficultly melting metal could be made to absorb carbon enough
to make it easily fusible. _This_ was the secret.
To state the matter in a simple way, iron ore, which is essentially a
natural “iron rust,” is the metal, iron, held in the strong chemical
grip of the gas, oxygen, which normally forms one-fifth of the air we
breathe. As you note, the combination forms a substance entirely unlike
either the iron or the oxygen, but both of these can be regenerated from
it (the ore) by chemical methods. Under influence of high heat (this is
one of the chemical methods, by the way), this stranglehold can be
broken by carbon, of which lampblack, graphite, charcoal, and coke, are
our most familiar examples. The result, in the small, crude, and
inefficient furnaces of long ago was a disappointingly small ball of
crude iron, pasty and scarcely meltable, even at highest heats, but soft
and malleable when cold. As mentioned, it was a variety of what is now
commonly called “wrought iron.”
[Illustration:
A CATALAN FORGE WITH ITALIAN TROMPE, OR WATER BLOWER
]
The ancients got this far.
But this was not “cast iron.” When, however, much more charcoal was
present in the highly heated furnace than was necessary simply to
combine with the oxygen of the ore, the liberated iron greedily absorbed
enough of the extra carbon to change its own nature. The metal then
became very fluid, whereas before it had been pasty and stiff even at
much higher temperatures, or, indeed, at white heat. This liquid iron
could be “cast,” that is, poured into molds and in that way made into
various useful shapes. It therefore became known as “cast iron” because
of this property.
So the brittle metal (cast iron) in our kitchen ranges, for instance, is
only the early malleable form of the metal _surcharged with_ or having a
large amount of carbon (3½ per cent to 5 per cent) in its make-up, and
it is this supercarbon content which confers the fluid quality while hot
and the extreme brittleness when cold. True, there are other important
constituents in our modern cast iron, but for our present purpose they
need not be dealt with.
It has been stated that the ancients got only as far as balls of wrought
iron. They really got further as their very fine sword steels show—the
“Wootz” of India, the “Damascus” of Syria, and later the “Toledo” of
Spain. These they produced by heating rich ore in very small, closed
crucibles with just enough carbon (pieces of wood or green leaves) to
make what we now call “carbon tool steel.” As carbon steel is simply
iron which has absorbed _not over_ 2 per cent of carbon (cast iron
described above has a supersaturation with its 3½ per cent to 5 per cent
of carbon and therefore is entirely different) they were able to make it
in small quantities. When hardened by cooling quickly in water, a
forged-out blade of this product would cleave without dulling its edge a
piece of iron, it is said, or cut cleanly a tuft of silk floss tossed
into the air. These steels attained well deserved renown.
While no one can desire to cast the slightest disparagement on the
product of that period, much of which was excellent, astonishingly so
considering the period, a moment’s consideration will convince one that
modern products not only do not suffer in comparison but in reality are
immensely superior. The ancients had little or no knowledge of the
reason for the proper qualities of their tools and they made the metal
from variable materials in a crude way in such small quantities that
little uniformity was possible. While some of the product was
undoubtedly excellent, much must have been less desirable.
Modern discoveries and inventions, with the great mechanical progress of
the last three centuries and the scarcely half-century-old application
of chemical control, have given during recent years products of great
uniformity and marvelous quality. What can compare with thirty thousand
pound lots of steel turned out from one Bessemer converter each
seventeen minutes during the 24 hours in the day, that is, a total of
1300 tons or 2,600,000 pounds, in which not only the main controlling
element, carbon, but also four lesser ones, silicon, manganese, sulphur,
and phosphorus, are held within extremely narrow limits; or the modern
blast furnace which produces a million pounds each 24 hours, run with
the same certainty of control? Modern high-speed steels which are every
day being made have such high quality that tools formed from them will
stand up for hours working red-hot under a lathe speed of two or three
hundred linear feet per minute taking a deep cut and “plowing out” chips
faster than a laborer can carry them away.
[Illustration:
THE GERMAN STUCKOFEN
]
Modern war armament which has recently been so well advertised is
sufficient answer as to whether modern metallurgy is in advance of that
of centuries ago.
The only necessity for such comparisons is that it seems to be a failing
of many to think that our forefathers were more wise and better in other
ways than we. It was but a few years ago that the fallacious
announcement was made that during archeological excavations in Egypt
there had been found a fully equipped telephone system. The inference
intended to be conveyed, of course, was that Bell’s invention of the
telephone had been antedated many hundreds of years.
[Illustration:
A GERMAN BLAST FURNACE OF FIFTY YEARS AGO
]
The forerunner of the modern steels was crucible steel, first made by
Huntsman about the middle of the eighteenth century. Previous to his
time steel had been made by the “cementation” process by which method
hammered-out bars of wrought iron were given a hard steel crust by
heating to a red heat in charcoal or bone dust. Huntsman’s product began
to come so uniform and of such quality that his competitors were quite
outdistanced. It is related that one of them took advantage of a very
severe storm to gain admittance to the forest forge of Huntsman, who, he
knew, could not refuse shelter at such a time. What he beheld was a very
simple thing—the melting in a clay pot of pieces of cementation steel.
Even to-day the crucible process is holding its own where quality is the
main consideration. It is the method by which practically all of the
tool, automobile, and other special steels of to-day are manufactured
and can hardly be given too high a rating. The newly devised electric
furnace process is the only possible competitor in sight. Of course for
quantity and for lower cost the Bessemer and the open-hearth processes
are the only available ones, but crucible steel has been the mighty
factor in the commercial development of the world—at least until the
latter half of the last century when the two other processes last
mentioned began to acquire honor of their own without, however,
detracting much from the importance of crucible steel as the steel of
“quality.”
[Illustration:
THE FIRST IRON CASTING MADE IN AMERICA
]
Though more interesting than any of the “six best sellers” much of the
subsequent history of iron will have to be passed over at this time. We
can now only mention those very great and revolutionary discoveries and
inventions which led to and absolutely are the basis of the quantity and
excellence of modern irons and steels; namely, the trial for a time of
coke made from pit coal by Dud Dudley of England and its failure which
was turned into a great success a century later (about 1713) by Abraham
Darby; Watt’s invention of the steam engine in 1770 which made possible
application of a strong continuous blast; invention of the process of
“puddling” of iron and of the rolling mill by Cort about 1784; the
introduction by Neilson about 1830 of the hot instead of the cold blast
which increased blast furnace production fourfold; the regenerative
system of furnace heating invented by Frederick and William Siemens; and
the invention of the Bessemer and Siemens-Martin or open-hearth
processes which provided methods for steel making on such an immense
scale that this invaluable material was made available for general
purposes.
It should be repeated that the inventions just mentioned have been of
the utmost importance to the iron industry, and through them only has it
acquired its consequence of to-day. Without them we would not have the
wonderful steel bridges, the skyscrapers, the gigantic steel ships, the
all-steel railway trains, etc., and the hundreds of iron products that
are to-day so plentiful and so constantly about us that we disregard
their presence. It is difficult thus to pass them by, but as most of
them will be referred to in later chapters we must do so.
Early iron making in America is of interest to us and must be briefly
stated.
The colonists were aware of some of the iron ore deposits about them and
sent samples to England where these yielded very fine iron. In 1619 a
company known as the “London Colony” was sent out from England to engage
in the manufacture of iron at Falling Creek, near Jamestown, Virginia,
but three years later all were massacred by Indians. It was many years
before attempt was again made to manufacture iron in Virginia.
About 1637 the General Court of Massachusetts granted to Abraham Shaw
one-half of the benefit of “any coles or yron stone w^{ch} shall bee
found in any comon ground w^{ch} is in the countryes disposing.”
Apparently little resulted from this high-sounding grant.
Real iron making in America began six years later with John Winthrop,
Jr., and his “Company of Undertakers for the Iron Works” which for many
years operated in several localities in the New England States. Heaps of
cinders left from their furnaces may still be seen and testify to their
very extensive operation. One of Winthrop’s men was Joseph Jenks, who
became known as the “Tubal-Cain” of New England. What is claimed to have
been the first casting made on the Western Continent was made by him. It
is a small pot, which was acquired and is said to be still owned by the
family of Thomas Hudson, a descendant of Hendryk Hudson.
Sand molding as used at present was introduced by an ingenious
Englishman, Jeremy Floris, and is vastly superior to the previously used
system of molding in clay. Hollowware began to be extensively produced
about this time.
As the country developed, iron works sprung up here and there and
various kinds of articles came to be regularly manufactured. Of the
early plants we can only mention the Stirling Iron Works, at Warwick,
New York, which made the great 186–ton chain with links weighing 140
pounds each, which spanned the Hudson River near West Point, and where
in 1816 was cast the first cannon made in America; the foundry of Sharp
& Curtenius, in New York, where was cast the first steam cylinder; and
the Trenton Rolling Mills, which first rolled iron as fireproof
structural material.
Before the Revolutionary War the colonies exported considerable bar and
pig iron to Europe, and as early as 1791 England began to foresee that
this country would eventually be a serious rival.
Pittsburg’s great advantage as an iron and steel center has been due to
its proximity to an extensive seam of bituminous coal and ore in
adjacent counties, and to its location so near the Great Lakes, which
provided cheap water transportation for the Lake Superior ores. The
first iron works there was that of Turnbull & Company, which was
established in 1790.
Though Reameur, a Frenchman, is the accredited discoverer of the process
of malleableizing cast iron, Seth Boyden, in a little shop in Newark,
New Jersey, made malleable iron castings a commercial success.
[Illustration:
TWO MODERN BLAST FURNACES, SHOWING SKIP-HOISTS, CAST HOUSES, STOVES,
AND ORE PILE
]
The utilization of the great beds of high grade coking coal of eastern
Pennsylvania, well known as the Connellsville district, and the
discovery and development of the Lake Superior ore deposits have made
the United States the leading producer of iron and steel of the world.
The development of the Birmingham, Alabama, district, also has been a
chapter of great importance but lack of space forbids description at
this time.
We can have only a very slight appreciation of the debt which
civilization owes to iron, for practically everything we see or with
which we daily come in contact contains or has resulted from application
of iron in some way or other. Our cooking utensils and implements (even
the enameled and tinned ones), the kitchen range, the water and drain
pipes, and the furnace and heating plants of our houses, are they not
largely of iron? Our main building materials—the steel frames of
skyscrapers and bridges, and are not even wood, brick, stone, and cement
either shaped, molded, or of necessity made by aid of iron machinery?
The conveyances by which we travel—wagons, automobiles, street cars,
steam railways and steamships—how would they be possible without iron or
steel? Consider the power plants of our factories, of gas and electric
lighting plants, the pumping machinery and distribution systems of water
works, mines, etc. Would the electric current which supplies so much of
our power and light be known to-day or even be possible but for the
magnetic properties of iron? And how many of the materials and articles
which we wear, use, and have about us constantly would be in any way
possible without the wealth of steel machinery and tools which are
available and absolutely necessary for their production?
The iron industry is often spoken of as the barometer of a people’s
civilization. If all iron and iron products and their influence upon the
world should be obliterated, it seems impossible that we could be even
started on the road to civilization.
No matter how we try, probably none of us ever realizes the immensity
and importance of the iron and steel industry with approximately 460
huge blast furnaces here, 5000 cast and malleable iron foundries, about
1000 Bessemer and open-hearth steel and some 3000 puddling furnaces, and
the many thousands of factories which each day are turning the products
of these into rails, plate, wire, pipe, and the infinitude of finished
articles which enter into and are mighty factors of our civilization.
Yet with these furnaces, forges and factories at our very doors, 99.9
per cent of us are entirely oblivious to their wonders and to their
presence except to be annoyed by their noise and smoke. Even the
blacksmiths and their service we scarcely note, though they are daily
fashioning for us a material which is vastly more important and more
wonderful than any of the “Seven Wonders of the World.”
CHAPTER II
THE RAW MATERIALS
A story has it that a minister once visited a friend who was a
zoölogist. Upon realizing for the first time how highly organized a
creature was the humble earth-worm with its three-layer skin covering,
alimentary canal, nephridia or excretory system, reproductory organs,
rude nervous system, and setæ for purposes of locomotion, he exclaimed:
“Wonderful! I had always supposed that worms were only skin and squash.”
With millions of tons of heavy reddish-brown earth from northern
Michigan and Minnesota going by our doors continuously during the
shipping season, the position of most of us is very similar to that of
the minister relative to the earth-worm. We know that something is going
on but we are not aware of its importance or the immensity of it.
Iron Ore
Almost every one knows that there are extensive copper deposits along
the Lake Superior shore of what is now northern Michigan. In the 17th
century word of these was several times taken to Europe where in old
publications was mentioned a huge ingot of copper from which the Indians
chopped pieces with their hatchets. At that early date maps of the
region were drawn which are wonderfully accurate, and, from time to time
over a period of a century and a half, adventurers attempted to gain
wealth in this favored region.
[Illustration:
MAP SHOWING DISTRIBUTION OF IRON ORES OF AMERICA
]
However, despite the definite knowledge of considerable mineral wealth
there and rumored claims of much more, Michigan at the time of her
admission to the Union in 1836 bitterly opposed having what is now the
northern peninsula included within her territory in lieu of a ten mile
wide strip of northern Indiana and Ohio, and it has been said that she
nearly went to war to resist it. Even after the discovery of the iron
ore deposits, no one realized the full importance of the minerals of
this region.
[Illustration:
SHOWING TYPICAL MESABA ORE BED WHICH, AFTER EARTH COVERING IS REMOVED,
BECOMES AN OPEN PIT MINE
]
During the many years of campaigning for Federal help in the building of
a canal at Sault Sainte Marie, the fisheries, valued at $1,000,000 a
year, were given as the leading reason why a canal should be built, and
it was no less a personage than Henry Clay, who, in opposing
appropriation for this purpose, referred to the project and the district
as “beyond the remotest settlement, if not in the moon.”
Now, within eighty years of that time, the annual tonnage of shipping
passing through the Sault Sainte Marie canal is as great as the combined
tonnage from the ports of New York, London, Liverpool, Antwerp, and
Hamburg, and, as against the $1,000,000 value of the fisheries, the
value at the mines of the ore alone shipped from this region amounts to
about $100,000,000 yearly.
[Illustration:
SHENANGO OPEN PIT MINE, CHISHOLM, MINN.
]
[Illustration:
INTERIOR OF A HARD OR LUMP ORE MINE
]
As the copper deposits are mostly along the shore of the lake and the
great iron ore beds occur seven or more miles inland, the latter were
not discovered until Sept. 19, 1844, when William A. Burt, a Deputy
United States Surveyor, noticed that the needle of a solar compass of
which he was the inventor became unreliable. In looking about to
discover the magnetic source which must be the cause of the variation,
members of his party discovered ore just beneath the sod near what is
now Negaunee, Michigan. Inventor-like, Burt’s only concern was to devise
some preventive for future interference by stray magnetic currents. He
simply noted in his book that there was here a deposit of iron ore and
neither he nor any of his party profited or apparently attempted to
profit from the discovery.
[Illustration:
SHOWING ORE BODY AND SHAFT METHOD OF MINING
]
The Indians seem to have had no previous knowledge of these ore
deposits.
The first shipments of ore naturally were samples taken from what
afterward came to be known as the Jackson mine and trials of them in
blacksmiths’ forges were made at Jackson, Michigan (from which town went
the first seriously-minded pioneer, Philo M. Everett), and at Cucush
Prairie. They were soon afterward tried in a blast furnace at Sharon,
Pa.
The first plan was to build forges and manufacture iron near the mines.
So there was established on Carp River a forge to which the ore was
hauled in winter when the ground was frozen. It turned out, however,
that while very good bar iron was manufactured here, it could not be
delivered in Pittsburg at a cost less than $200 a ton. As the market
rate for iron then was but $80 a ton the plan was not financially
successful.
[Illustration:
LIGHTING THE FUSES IN A SHAFT MINE
]
Attention was turned to the shipping of ore to furnaces better located
as regards coke supply and market. It was possible to make this a
profitable undertaking only through cheap ore handling and
transportation. So, to-day, the ore which is better adapted than the
other raw materials for handling by labor-saving devices and
transporting without deterioration, is taken to the coke and limestone,
and to the market for the product. While the weight of coke used is but
half that of the ore smelted, its greater bulk, loss by breakage when
handled in quantities, and deterioration upon exposure preclude its
manipulation in the way which would be necessary to get it to the ore.
[Illustration:
VIEW OF HULL-RUST MINE, NEAR HIBBING, MINN.
]
The marvelous development of this territory into the greatest ore
producer of the world, including the hauling of the first small shipment
on mule back, the building of the plank and then the “strap” railroad
with grades so steep that the small trucks often ran over and killed the
mules, the building of the steam railroad, the successive building and
enlarging of canal locks at Sault Sainte Marie connecting for use of
ever larger and larger ore boats the waters of Lake Superior and Lake
Michigan, and the growth of ore boat fleets to such size that during the
shipping season scarcely ever is one boat out of sight of another over
the entire 800 mile journey from Duluth to the furnaces along Lake
Michigan and Lake Erie, is within the memory of men still living.
Marquette was the shipping point during the earlier days and the history
of this and adjacent regions during the latter half of last century vies
in pioneering flavor with the tales of our early western frontiers, and
with the more recent Yukon mining camps.
[Illustration:
THE ROUTES BY WHICH LAKE SUPERIOR ORES GO TO THE FURNACES
]
The first two mines, the Jackson and the Marquette, have come to be
particularly well known historically. The development of these and other
ranges in northern Michigan and Minnesota, particularly the Menominee,
Gogebic, Vermillion, etc., and, since 1890, the Mesaba and Cuyuna, have
brought about revolutions in ore digging, handling and transportation,
which followed each other with extreme rapidity. The ore carrying boats,
for instance, may almost be said to have jumped from a length of three
hundred to six hundred feet, and the Sault Sainte Marie canal locks were
several times almost immediately outgrown, though rebuilt again and
again, each time so much larger than before that they were deemed
impossible to be outgrown.
[Illustration:
LOADING ORE AT AN OPEN PIT MINE
]
[Illustration:
SHOWING OTHER TYPICAL ORE BODIES, SHAFT MINED
]
Practically all of the ore beds, with the exception of the Mesaba, yield
hard or lump ores and most of them are shaft mines in which mining has
to be done underground and the ore blasted down. Blast furnaces had
never used any but lump ores when along came discovery of the immense
soft ore deposits lying just beneath the surface of the ground over a
region one-hundred miles long in what is known as the Mesaba district of
Minnesota. These soft ores were so accessible and so rich that they drew
the attention of the iron makers of the whole country. But, alas! While
perfectly good in every other respect, they were merely dry powder and
not adapted to blast furnace methods. There were great discussion,
excitement, and ridicule among or at those who invested in these soft
ore mines. Eventually, of course, blast furnace men worked out feasible
methods of converting soft or what are termed “Mesaba Range” ores into
iron in the blast furnace. Those brave spirits, who in the face of
ridicule dared to invest in and develop Mesaba properties, have long
been reaping their financial reward which still shows no sign of
diminishing, as “Mesaba Range” mines are “the” mines of to-day.
[Illustration:
A CLOSE VIEW OF THE HOOVER & MASON UNLOADERS
]
While it may be done, it has not been found desirable to make up the
entire “burden” or furnace charge of soft ores alone as long as lump or
hard ores are obtainable to mix with them, but often more than half is
soft ore.
[Illustration:
STARTING AN OPEN PIT MINE. THE EARTH COVERING IS BEING REMOVED
]
While ores from the shaft mines, called “Old Range” ores, are won by
going down into the earth sometimes as far as 3,000 feet, drilling holes
in the rock, blasting down the ore, and loading it into buggies which
are hoisted to the surface, “Mesaba Range” ores are made available by
simply “stripping” off the thin earth covering, then caving or loading
with steam shovels the soft ore into railway cars. Some of the
illustrations presented show the ore trains and shovels, and the manner
in which the open pits are worked in terraces.
One naturally wonders how it is possible to mine and carry these ores to
the shipping ports of Duluth, Superior, Two Harbors, Marquette, Ashland,
Escanaba, etc., put them aboard ore carrying boats, transport them by
steam power to Milwaukee, Chicago, Gary, Detroit, Cleveland, Pittsburg,
Buffalo, and the many other iron centers and convert them into iron and
steel at a profit. This, of course, is only possible because of the
inventive genius of man. For every operation ingenious machinery has
been constructed which has brought the cost of such operations to its
lowest terms.
[Illustration:
UNLOADING CARS OF COAL OR ORE IS A SIMPLE MATTER WITH THE MODERN CAR
DUMPER
]
[Illustration:
ORE CARS ARE UNLOADED BY GRAVITY AT DOCKS. THE CHUTES THEN CONVEY THE
ORE FROM THE ORE POCKETS INTO THE BOAT’S HOLD
]
By modern methods the cars carrying the ore from the mines are run up
trestle-work into positions above the ore bins high over the docks. The
mammoth ore carrying boats are merely steel shells with quarters for
crew and machinery at bow and stern, and hatches built with exact twelve
foot centers between. They are tied alongside the dock, long steel
chutes, also spaced twelve feet apart, are lowered along most of the
length of the boat and the ore slides into the vessel’s hold evenly all
along as it has to do, else the buoyancy of lighter parts of the boat
might break the frail shell. The entire load of 10,000 tons of ore is
ordinarily taken aboard in less than one hour. Pulling out immediately
the vessel traverses Lake Superior, the Sault Sainte Marie canal, Lake
Michigan or Lakes Huron and Erie as the case may be, and ties up at the
dock at destination. Years ago it would have been unloaded by men with
buckets or wheel-barrows, requiring some days at best. Now, however, the
hatches are uncovered and several ore unloaders with huge clam shell
buckets taking as high as fifteen tons of ore at a “bite” descend like
vultures upon it. Within four or five hours the boat is again empty with
no manual labor having been done upon the ore from the mine to the
furnace pile with the exception of a little heaping up of the ore in the
corners of the boat’s hold, which the ore unloaders could not reach.
[Illustration:
HOOVER & MASON UNLOADERS AT THE ILLINOIS STEEL CO., SOUTH CHICAGO,
ILL.
]
A young man named Alexander E. Brown could not bear, in the old days, to
see the ore so awkwardly unloaded, and in 1880 started the procession of
ore unloading devices. There are now several successful ore unloaders of
which the Brown hoist, the Hoover & Mason, and the Hulett are probably
the best known. With the Hulett unloader the operator has to be an
aviator, as his position is directly above the grab bucket. He descends
into the hold with the bucket, comes up with it and is with it in its
entire journey from the boat’s hold to the dump and back again. It must
be dizzy business.
[Illustration:
THE HULETT UNLOADER. NOTE THE OPERATOR’S HEAD IN WHITE SPOT JUST ABOVE
THE GRAB
]
Time is too precious to hold the boat at the dock long enough that each
bucketful, large as it is, can go directly to its final bin. It is
dropped just back of the unloading machine from which it is again picked
up by other buckets which carry it back toward the furnaces and deposit
it in cement ore troughs awaiting further journey to the ore house, from
which it goes to the furnaces. The empty ore boat immediately coals with
whole car loads of the fuel dumped into chutes leading to her bunkers by
the car dumper and proceeds on her way back to the mines for another
cargo of ore. The round trip, including loading and unloading, requires
but seven days.
[Illustration:
A GOOD VIEW OF THE HATCH SYSTEM OF MODERN ORE BOATS AND FOUR HULETT
UNLOADERS AT WORK
]
As in many other lines of commercial endeavor of to-day, speed and large
tonnage have been the aim and it would seem that in ore handling and
conveying devices the limit has about been reached. The big steam
shovels, gravity docks, ore tanks or boats, and unloading and coaling
devices, with the low cost of water transportation have made our modern
iron and steel preëminence possible. To show the importance to us of
this water transportation, we might mention that the rate for carrying
ore from Lake Superior ore ports to the Lake Erie furnaces has been as
low as $.0007 per ton per mile while the transportation cost by way of a
well operated railway at that particular time was more than $.005 per
ton per mile—more than seven times as much.
[Illustration:
THE REHANDLING BRIDGE WITH STOCK ORE PILE AND BLAST FURNACE AT REAR
]
Though for some years past more than three-quarters of all of the iron
ore used in the United States has come from seven or eight mines in the
northern peninsula of Michigan and the adjacent part of Minnesota, it
must not be understood that the Lake Superior mines are the only ore
deposits in this country. Figures show that such an inference is far
from the truth. It is true, however, that they have made the United
States what it is, the leading iron producer of the world. There are
still immense quantities to be mined on the Lake Superior ranges. Their
heavy production of cheaply handled high grade ore has, of course, held
back development of other districts, which also have great natural
resources. The Birmingham, Ala., region for instance, is a great ore and
iron producer, right now producing the third largest tonnage of any
district in the country. Some time in the not far off future, Alabama
with her great deposits of iron ore, coal, and other natural resources
is going to announce herself in no small voice. New York, Pennsylvania,
Tennessee, and Virginia rank next after Minnesota, Michigan, and Alabama
as ore producers, and several other states of the Union are not paupers
in resources of iron ore.
[Illustration:
HULETT GRAB BUCKETS IN THE HOLD OF AN ORE BOAT
]
We should not get so enthusiastic over our ore supply and iron
production as to think that other countries are devoid of such material.
Almost every civilized country has ore enough that it does pretty well.
With many the trouble is that the ore has objectionable constituents or
that supply of cheap fuel is not available. Germany has large deposits
of iron ore, but until the invention of the basic Bessemer process about
1870 she was handicapped because of the high phosphorus content of her
ore. The basic processes, both Bessemer and open-hearth, allow of the
removal of this phosphorus during the conversion into steel, and they
therefore brought Germany to the front as an iron producer.
The excellence of Sweden’s iron and steel has long been known the world
over. Sweden produces approximately one per cent of the world’s total
production of iron and steel, but her ore has been of such high grade
that iron made from it has maintained its position as a standard for use
in the manufacture of highest grade crucible steels. The very finest
steels for cutlery and tools, and even the softer grades of steel of
northwestern Europe, have been made from Swedish iron as a base.
Iron ore, of course, is classified by geologists and chemists into
varieties with such names as hematite, magnetite, siderite, etc., which
here little concern us.
To be worked at a profit, the iron content of the ore must be high with
the smallest possible amounts of undesirable impurities, particularly
phosphorus, sulphur, and silica. There are, however, certain impurities
which are not undesirable, for instance, lime, which will act as a flux
and neutralize the effect of some of the undesirable impurities. For
these reasons the prices for iron ore are based on the iron content and
modified by the relative amounts of undesirable and desirable
impurities. Phosphorus is almost a domineering factor and at present
approximately fifty cents a ton more is paid for Bessemer ore (that
containing less than .050 per cent phosphorus) than for non-Bessemer
ore. As might be expected the best ores have been the first used and the
grade is constantly falling. Instead of the 66 per cent iron ores of
some years ago those coming nowadays contain not much more than 59 per
cent of iron and the Bessemer ores described above are getting scarcer,
so that for some years practically all of the furnaces have been mixing
with them as much higher phosphorus ore as could be used without pushing
the phosphorus content of the mixture over the allowable limit.
We often hear people surmising what is to become of us when all of the
iron ore of this planet has been used. There is no harm in taking stock
of resources and in this case it does us much good. It happens that each
time the count is taken of iron ore available and that which under
future and better methods of working can be utilized, we find ourselves
immensely better off than the previous report had made out and we have
less cause to worry about the future. The last inventory was taken by
the extremely ambitious International Geological Congress held at
Stockholm, Sweden, in 1910. It shows that the world yet has enough rich
ore to make 10,192,000,000 tons of iron, and, a further supply of ore
for 53,136,000,000 tons of iron, which could be used if necessary.
So we will get along for a while yet.
CHAPTER III
THE OTHER RAW MATERIALS
[Illustration:
OLD CHARCOAL KILNS, NEAR NEGAUNEE, MICH.
]
Since the beginnings of iron manufacture, charcoal has been a favorite
fuel. Though during the past two centuries coke has grown to be the
standard, with anthracite and some few bituminous coals finding use in
certain favored localities, charcoal may be considered the fuel which
developed the iron industry, at least until recent years.
Charcoal
As most of us know, charcoal is completely charred wood, usually hard
wood, though sometimes resinous or other soft woods are used. Of
well-dried timber more than 50 per cent by weight is moisture. This and
certain other constituents are driven off by heat in the absence of air,
which process is usually called “destructive distillation.”
By primitive methods a considerable part of the wood was completely
burned and wasted during the production of charcoal. Stacked in piles or
long rows the cut wood was well covered with earth, except for a small
opening at the top through which the fire was lighted down a center
cavity left to the bottom of the pile. The air coming in through the
opening at the top was sufficient to keep the wood smoldering. After a
period, which had been shown by experience to give the best results, the
opening was closed and the fire smothered.
[Illustration:
BEEHIVE COKE OVENS
]
Brick ovens of the beehive shape were built at a later date where
considerable charcoal was to be made. These were operated on much the
same general principle as the _meillers_ or earth-covered piles,
described above. The fire was lighted at the bottom of the central
cavity of the corded wood, the only air at first coming from the top,
though later in the process a little was admitted through holes in the
walls. After about ten days, when gas ceased to come off, the kiln was
tightly closed for a period of twenty days more for the fire to die out
and the charcoal to cool.
By both of these processes valuable constituents were burned or driven
off by the heat and lost. These were mainly methyl alcohol, acetic acid,
and wood tar.
Modern industry so emphatically disapproves of any waste of materials
that apparatus has been devised to produce charcoal which allows of
recovery of the by-products at the same time. In northern Michigan,
which is practically the only district in the United States in which the
charcoal industry as an industry still survives, long steel tubes or
retorts are built with brick fire-boxes under each end, much as a
stationary boiler is set. Into these retorts are run steel cars loaded
with the wood. The retorts being closed, the heat drives or distills off
the moisture and gaseous compounds through pipes connecting them with
condensing apparatus. After about twenty hours the wood has been
charred, the doors of the kilns are suddenly opened and the cars are
rushed into other and similar retorts for cooling, while fresh loads of
wood replace them in the first.
[Illustration:
STANDARD BEEHIVE COKE OVEN
]
[Illustration:
BEEHIVE OVENS
]
As may be surmised vast quantities of wood and of wood-producing land
are required for extensive charcoal manufacture, and this is the most
serious problem for the manufacturer of charcoal. Several square miles
of timber land must be cut over each year and the wood efficiently
transported in order to operate a large plant profitably.
Pig iron as a _by-product_ is a rather novel idea, but that is
practically what the charcoal pig iron produced in our Lake Superior
region is. Several companies operate wood distillation plants for the
production of methyl alcohol, acetic acid, acetate of lime, etc., and
use their charcoal in the manufacture of charcoal pig iron from the ores
so close at hand.
The very low sulphur content and the small amount of ash have been the
great advantages possessed by charcoal over other solid fuels. Resulting
characteristics made charcoal pig iron a former favorite for manufacture
of certain articles such as chilled car wheels, etc., and it, therefore,
brought a higher price than coke pig iron. During recent years, however,
by careful selection of coal and improvements in the coking process the
sulphur and ash of coke have been so reduced that charcoal has not so
great an advantage as formerly. Charcoal iron to-day brings only about
$1.50 per ton more than coke iron; whereas, the differential a few years
ago was as great as $5.00 or $6.00 per ton.
Charcoal is quite fragile and structurally weak, so much so that blast
furnaces for its use cannot be built higher than sixty feet; whereas,
the great strength of coke allows them to be built to exceed one hundred
feet in height with correspondingly increased output. What this means
may be realized by every one conversant with the demands of modern
industry.
Coke
[Illustration:
CHARGING COAL INTO THE OVENS
]
As charcoal is completely charred wood, so coke for analogy’s sake may
be said to be completely charred coal, practically always of the
bituminous type. By “baking” bituminous coal at a cherry-red heat, its
volatile constituents are driven off as the well-known “coal-gas” of
almost every small town, and a strong, brittle and porous material or
coke residue is left. If the baking is done without any admission of air
to the retort, practically none of the coal burns and the “cake” or coke
which is left contains the ash of the original coal and what is known as
the “fixed carbon,” i.e., carbon which cannot be distilled or driven off
by heat alone, though it would burn were air admitted.
The gases or volatile constituents which are given off consist mainly of
moisture and a mixture of gaseous chemical compounds, which are known as
“hydro-carbons.” These contain that part of the carbon of the original
coal which does not remain as “fixed carbon” in the coke.
[Illustration:
QUENCHING AFTER COAL HAS BEEN COKED
]
Just why some coals will coke while others of apparently the same
composition as shown by the chemist’s analyses, will not, but instead of
the hard brittle mass will leave a heap of brown or black powder, is not
as yet definitely known. It is easy enough for chemists to determine
with accuracy the amounts of hydrogen, nitrogen, oxygen, carbon,
sulphur, and other elements; but it is a difficult and perhaps an
impossible matter to determine just how these elements are “hitched up”
in the very complex mineral, coal,—one of the most complex substances
which we know.
Various theories have been advanced in the attempt to explain the coking
quality. A bulletin of the United States Geological Survey claims that
the relative percentages of hydrogen and oxygen in the coal determines
it; others have held that it depends upon the compounds of a tarry or
asphaltic nature present. The fact remains that some coals coke without
trouble, while others do not coke at all. As yet the only real way to
tell whether a new variety of coal will or will not coke is to try it.
Since 1713, when Abraham Darby in England succeeded in introducing it as
a substitute for the fast disappearing charcoal for use in blast
furnaces, coke has become the standard fuel. It is very strong and will
bear up under the great weight of iron ore and limestone with which the
furnace is charged. So furnaces for use with coke may be built much
larger than those in which charcoal is to be the fuel. The porous nature
of coke allows it to burn rapidly with intense heat, so that the output
of an iron works is greatly increased through its use—a very desirable
thing in these days of big things. It has its disadvantages, of course,
mainly high sulphur, a deleterious substance for which molten iron,
unfortunately, has a voracious appetite, and a rather high percentage of
ash which must be fluxed out. But all in all, it is a very desirable
fuel for blast furnace and other metallurgical purposes, as is shown by
the fact that it is used in the production of about ninety-nine per cent
of all iron and steel now made.
[Illustration:
DRAWING THE COKE
]
What is known as the Appalachian coal region produces coal for more than
seventy-five per cent of the coke made in the United States. This region
includes the strip of territory extending from Western Pennsylvania and
Ohio down to Tennessee, Georgia, and Alabama. The famous Connellsville
district is a part of this region.
Illinois and Indiana have a great deal of coal, which, however, has
rather indifferent coking qualities. Almost constant experimentation has
been carried on in the attempt to induce these semi-coking coals to
coke. The best that has so far developed is the use of a considerable
percentage of them in admixture with coals of good coking qualities.
Such mixtures yield quite satisfactory coke.
The Beehive Oven Process
[Illustration:
LARGE PIECES OF COKE
]
In the old days there was no desire or incentive to avoid waste of coal
resources. If during the coking process some air got into the oven and
part of the coal was burned, or if all of the gas given off was wasted,
it did not matter. There was plenty more of coal and the thing desired
was to get the requisite coke in the quickest and cheapest way.
[Illustration:
WHERE COALS ARE PULVERIZED AND MIXED FOR COKING
]
In Western Pennsylvania, Ohio, and Virginia, were great beds of high
grade coking coal. In this region and particularly around Pittsburg,
numerous blast furnaces and steel mills grew up. The coke for these was
made in the most convenient way—in the wasteful beehive ovens.
[Illustration:
BATTERY OF BY-PRODUCT COKE OVENS, SHOWING GAS-COLLECTING MAIN
]
As the name signifies, these ovens or retorts are brick chambers shaped
like beehives. In the larger plants they are built either in single rows
against long hills or in double rows back to back. Over the tops of the
ovens in each row runs a car called a charging “lorry.” Coal is poured
from the bottom of this through a hole in the top of each oven while it
is still hot from the preceding charge. No air gets in except that
admitted through the hole in the oven top and a small slit left over the
one side door, through which the coke is drawn when the coking process
is finished. The heat of the oven starts the distillation of the
moisture and the volatile compounds which escape through the hole in the
oven top. The small amount of air admitted burns a little of the coal
and gas and raises the temperature of the oven to that required for
coking.
After 48 or 72 hours a spray of water is thrown in over the glowing coal
to quench the fire. The partially cooled coke is drawn through the open
door, sorted and loaded into cars for shipment.
Though this method of coking is a very wasteful one, it yet produces the
larger quantity of the coke made in the United States. However,
conditions are rapidly changing and it will not be many years before the
much less wasteful “by-product” process gains the ascendency. By 1914 it
had already come to produce about twenty-five per cent of the total coke
made here, and since that date the percentage has been rapidly
increasing.
The By-product Process
[Illustration:
TOP OF OVENS WITH CHARGING BIN AND LORRY AT FAR END
]
By this system of coking a greater yield of coke is obtained and most of
the by-products are saved. The value of the latter depends largely, of
course, upon local conditions, such as transportation, costs of the
material, cost of labor, and available market for the coke oven gas.
They are usually figured as having a value of $1.50 per ton of coal
coked, equivalent to a total of $71,000,000 per year for the coal coked
in the United States.
[Illustration:
LORRY FOR CHARGING COAL INTO OVENS
]
The ovens and apparatus required are considerably more expensive, but,
since this industry has developed in this country during the last
twenty-two years to a point where one-quarter of all of the coke
manufactured is made by the by-product process, there can be no doubt
that it is a profitable proposition and that eventually the wasteful
beehive ovens will be a thing of the past.
Practically all of the types of by-product coke ovens in use have been
developed in Germany or Belgium, where circumstances forced earlier
conservation of resources than in this country. The three best known
types are the Semet-Solvay, the Otto Hoffman, and the Koppers—the latter
a recent arrival. They differ mainly in details of construction and
operation.
[Illustration:
MACHINE FOR PUSHING COKE FROM OVENS
]
In a general way a “battery” of coke ovens consists of from 40 to 80
long narrow brick-walled chambers placed closely side by side with
heating flues or “checker-work” between them. The fire for the baking
process is in these flues, which are interconnected, and the heat
developed is sufficient to drive off the moisture and volatile
substances of the coal in the narrow chambers just on the other side of
the brick walls. Charging is done by a “lorry” as in the beehive
process. After from seventeen to twenty-four hours at a red heat, the
coke is “pushed” from the ovens, one after another, by an electric ram
which enters at one end. The 30 × 7 × 1½ foot block of glowing coke
emerges from the other end, where, breaking under its own weight into
good-sized pieces, it falls into a steel car on a track just beneath. A
spray of water quenches it and it is taken to the storage bins to be
sorted.
Rich coal-gas is the main by-product. That which comes off during the
first seven hours is the richest and has the greatest illuminating or
“candle” power. After washing free from dust, tar, ammonia, etc., the
gas is usually run into holders or tanks from which it is distributed
for use for illuminating or for heating purposes. That which comes off
during the latter part of the coking period has much less of those
constituents which give illuminating value. It has good heat value,
however, and as fuel is required for keeping the ovens up to the coking
temperature, this poorer gas from the coking chambers is switched into
and burns in the flues between the coking chambers as mentioned.
Thus the larger part of the gas is sold to customers, usually in the
city near which the ovens have been located, and the poorer part is
utilized in heating the ovens and the steam boilers which run the plant.
[Illustration:
QUENCHING CAR AWAITING ITS LOAD
]
The coal tar, which the German chemists have made so famous through its
manufacture into the almost endless variety of beautiful dyes, is
another of the by-products which is recovered by this, but burned or
lost in the beehive oven process. From a long main over the tops of the
ovens which connects the gas pipes, the tar flows along with the gas to
the scrubbing and gas cleaning plant, where by rather intricate
operations it is freed from other substances.
In this country much of the tar is used for building purposes, etc., and
some as fuel, but not much has been made into the chemical products for
which Germany is so famous. For a long time a few dyes and other
chemical compounds have been made here from coal tar. Since the early
days of the war in Europe and the cessation of imports of such materials
on this account, there has come about considerable expansion in their
manufacture here; but it is doubtful if the time is yet ripe for a
wholesale entry into the manufacture of these coal tar “derivatives,”
especially the very extensive variety of dyestuffs.
Naphthalene and benzol from which many other chemical compounds as well
as munitions of war can be made, are among the by-products.
[Illustration:
QUENCHING THE COKE
]
Most of the ammonia which the corner drug store sells, comes from the
by-product manufacture of coke. The largest part of the ammonia which is
produced in the process, however, is manufactured into sulphate of
ammonia, a well-known fertilizer.
Coal
Anthracite or hard coal has been used in certain districts in the United
States, especially in New Jersey and eastern Pennsylvania. It is not an
ideal fuel as it is too solid to burn rapidly, spalls or cracks under
heat and interferes with the blast. Since 1860 when coke became
available here much less coal has been used, though some is yet used in
admixture with coke. Some bituminous coals which contained little tarry
matter also have been used in this way.
Fluxes
Limestone, the rock which is ordinarily used for fluxing purposes, needs
no introduction to any of us. As the marble of statuary, the material of
which oyster and other sea shells and the white tombstones of our
cemeteries are composed, it is well known. Any of these varieties of the
material may be used for fluxing purposes, but usually it is limestone
which is quarried for the purpose or obtained as chippings or spalls
from building blocks.
[Illustration:
COKE GOING FROM QUENCHING CAR TO BINS
]
[Illustration:
LOADING COKE IN BOX CAR
]
The active agent, which produces the chemical or fluxing action in the
blast furnaces, is carbonate of calcium (lime) of which limestone
contains about 98 per cent. Dolomite is a mixture of carbonates of lime
and magnesium, about 53 per cent of the former and 45 per cent of the
latter, and is sometimes used in place of limestone. Fluor spar, a rock
composed of calcium and fluorine, is used in small quantities in some of
the metallurgical processes. It is a very powerful flux.
CHAPTER IV
THE BLAST FURNACE
Up the dark tower shoots the elevator with its “buggy” of coke. Its
speed is not conditioned to the comfort of man, who is not supposed to
be a passenger, except the occasional laborer whose duty as buggy-pusher
requires his presence on twelve-hour shifts at the top. So we, whose
exploratory proclivities have led us at the office to sign away our
lives for grant of a pass to the blast furnace, find our breath about
taken from us with the first mad dash into the darkness of the climb.
That stone tower had looked much more innocent from below.
But now the rickety elevator has as suddenly emerged into the light
again and stopped abruptly at the charging floor which extends across
the chasm to the top of the furnace.
As the smoke-begrimed buggy-pushers rush the buggy of coke across to the
furnace bell, we have opportunity to notice that we are a full hundred
feet above ground. Just here, seemingly so close that we can put our
hands on them, in a row, are the round steel tops of the four stoves
which are for the purpose of preheating the blast. The huge pipes, dust
arresters, tanks, and buildings, all so necessary to the plant, look
almost like a tangled mass from our high station, while the charging
floor upon which we stand, the shoulder-high steel fence around it, the
furnace top, the adjacent stoves and in fact everything for a half mile
around us, is colored yellow-red with iron dust. We understand the
reason for this when the buggies of ore which have succeeded the coke
are dumped into the funnel-shaped depression around the conical bell at
the center. As the huge bell is lowered and the charge slides in there
is considerable blowing out of the fine ore dust, which, in fact,
continually “oozes” out of all crevices under the heavy pressure of the
blast inside.
[Illustration:
HAND-FED BLAST FURNACE
]
Day and night, month in and month out, during the life of the fire-brick
lining of the furnace, this routine of charging, first coke, next the
theoretically correct charge of analyzed iron ores, then limestone, in
rotation goes on. From 6 A.M. to 6 P.M. and from 6 P.M. to 6 A.M. on
twelve-hour shifts, alternating gangs of laborers push the buggies
across to the furnace top, dump and return them to the elevator already
up with another load.
The incessant quiver of the iron plates beneath our feet with the
rumbling and groaning from the inside of this monster are disquieting
and the thought constantly recurs: “What if this powerful creature
should just now rebel, as quite occasionally occurred in the old days
when all of its moods had not been so well understood?” For this king of
metallurgical devices, though gentle and obedient as a lamb under proper
treatment, is a domineering fury when it has dyspepsia as occurs
whenever its attendants are remiss in their attentions to its diet.
“Those explosion doors just below the furnace top—are they in working
order and would they be adequate?” But whether, as in recorded
instances, the whole furnace top is torn off as evidence of its wrath,
or its displeasure is exhibited in a milder way, we much prefer to be
absent. The thought is disquieting and we are glad to leave.
[Illustration:
CINDER OR SLAG FLOWING INTO LADLES
]
[Illustration:
“FIREWORKS” AT THE CINDER-NOTCH
]
Unwilling to test again the elevator for the downward trip, we take to
the narrow iron stairway which leads from the top of the furnace to the
ground. But this is worse than the elevator, for the stair treads are
very narrow and made only of three slender iron rods. To our palpitating
hearts they seem to give very insecure foothold and the gaps show that
there is nothing but earth beneath us, and that a hundred feet below. To
make matters worse, before we creepingly get half way down some visitors
below have stopped to watch our slow and trembling steps and our nervous
clutch on the low “stingy” hand rail. We hear them innocently inquire of
one another why we move so slowly. We wish that we could appear brave,
especially before the women in the party, but we could not move with
greater alacrity if our lives depended upon it.
Once below again with our breath regained, things are more interesting.
The red-hot molten slag which has just been tapped out is running from
the furnace along a long trough into a ladle six feet high resting upon
a car on the railway track alongside the “cast house,” as the huge
structure which houses the lower part of the furnace is called. This
smoking, molten slag stream gives off a powerful sulphur smell and
throws a lurid glare over everything round about.
[Illustration:
THE SLAG DUMP
]
The furnace superintendent is just explaining to the other party that
No. 2 furnace has been “hanging” for a couple of days and is still
dangerous. “If you realize,” said he, “the great weight of coke, ore,
and limestone in that furnace, you can see what a splash it would make
if the clogged, bridged part with all above it should fall suddenly into
the molten pool in the ‘hearth’ of the furnace. Two years ago No. 1
broke out and the molten metal caught and burned to death one of our men
and injured several others. ‘Hanging’ does not occur when the furnace is
working right, but failure of the charge to come down evenly is very
serious sometimes. A blast furnace is like a coquette; she has to be
handled just so, and even then you cannot always be sure what she is
going to do next.
“Oh yes,—where does the iron come from? Well, we often read nowadays of
a man and his ‘affinity.’ Now the chemist has used that word ‘affinity’
for years to describe the liking or attraction of one chemical ‘element’
for another; in fact, that is where this recent colloquial use of the
word originated. Iron ore is nothing more nor less than metallic iron,
the element, chemically combined with oxygen, another element which
constitutes one-fifth of the air we breathe. Under conditions produced
in the blast furnace, though for centuries wedded to iron, oxygen
deserts him for her ‘affinity’ carbon, which is best known to you as
coke, coal, or charcoal. The iron, now free, becomes molten at the high
temperature encountered (about 2800° to 3000° F.) and descends into the
‘hearth’ or bottom of the furnace, while oxygen and her new partner
escape out of the top of the furnace in gaseous form. When molten iron
has accumulated in the hearth to the extent desired it is tapped out as
you will soon see.
[Illustration:
DIAGRAMMATIC SKETCH OF BLAST FURNACE
]
“The limestone charged has ‘affinity’ for dirt and certain other
impurities of the ore which it removes in molten form as the ‘cinder’ or
‘slag’ which is there running into the ladle. When cold, this cinder is
a dark greenish-black, glassy substance, which of recent years has come
to be used to a certain extent in the manufacture of Portland cement but
is mainly used for filling-in purposes. Some is crushed and utilized in
concrete mixtures and for road building. In Chicago considerable land
has been ‘made’ by dumping slag into the lake, and South Chicago is
reported as standing on a swamp which has been filled in with slag from
the steel works there.
[Illustration:
OLD-FASHIONED PIG BED
]
“This immense furnace is simply a strong steel shell lined two or three
feet thick with fire bricks. At the ‘bosh,’ which is the region where
the greatest heat is produced, hollow bronze plates are inserted among
the bricks of the lining through which circulating cold water keeps the
bricks from being fused.
“The hot gases which are led from the upper part of the furnace through
that brick-lined ‘downcomer’ are burning in three of those ‘stoves’ to
heat them, while cold, clean air from the blowing engines is coming
through the other stove, which, ten minutes ago, when it was put on
blast, was the hottest of the four. It is now giving up part of its
accumulated heat to the blast on its way to the furnace. Switching the
cold incoming air every little while from a partially cooled stove
through a hotter one while allowing the former to reheat, provides
continuous blast of a temperature of 800° to 1400° F. The ‘hot blast’
idea originated about 1830 with James Neilson, a gas engineer of
England, and its introduction revolutionized the blast furnace industry
and made the highly efficient modern practice possible.
[Illustration:
FURNACE AND SAND BED READY FOR IRON
]
“This big pipe above our heads which encircles the furnace is the
‘bustle pipe.’ It also has to be lined with fire bricks. The hot blast
is distributed by this ‘bustle pipe’ to the tuyères here—these L-shaped
pipes—which shoot it directly into the furnace. Through the peep-holes
in the tuyères you can get a glimpse of the dazzling interior of the
furnace. The blast of heated air is causing the coke to burn fiercely
there so that it melts the iron, which farther up in the furnace has
been forced to part from the oxygen, as I explained to you.”
[Illustration:
LAYOUT OF BLAST FURNACE PLANT
]
But now six men with a long steel bar are starting to break through the
two or three feet of clay with which the “tap hole” of the monster
furnace is plugged, and our informant hurries away.
[Illustration:
SKIP HOIST AT WORK. SKIP DUMPING INTO HOPPER
]
For ten minutes with strong sledge blows the tappers struggle to break
through the plug of burned clay. Meanwhile the monotonous whistle of the
heavy blast into and through the bustle pipe and tuyères goes on and the
discharge pipes of the water-cooling plates empty into the gutter around
the furnace bottom the water which has been circulating to keep the
inner bricks from fusing.
[Illustration:
SECTION OF BLAST FURNACE SHOWING FILLING ARRANGEMENT, BINS AND ORE
BRIDGE
]
And now a shout and the strong red glow throughout the cast house tell
us that the tap hole is open and the iron is running down the main
channel of the sand bed. Past the plugged entrances to the lateral
branches runs the molten iron stream to the end of the cast house nearly
one hundred feet distant where it divides, filling the laterals on each
side and from them running into many open molds arranged like the teeth
of a comb. Each of these molds is about five feet long. They form the
“pigs,” and the laterals what are known as “sows.” As each lateral and
its molds fill, the lateral ahead of it is opened and the process
repeated, laterals and pigs filling up simultaneously on opposite sides
of the main channel till the whole cast house floor is filled nearly up
to the furnace with the red smoking metal.
[Illustration:
SAND CAST PIG IRON
]
There are few sights more glorious than the cast house with bed just
filling with metal, and especially is it so at night. The strong
yellow-red light of the flaming metal issuing from the furnace and the
intense glow of that already in the bed illuminates everything in and
about the building. But already, before the furnace is empty, the
workmen are spraying with water the earliest cast pigs. Covering them
with a light layer of sand they venture upon them with thick-soled shoes
and break the “pigs” from the “sows” with sledge hammers.
This is the old-fashioned “sand cast” pig iron. After remelting in the
cupola furnaces of neighboring towns and casting into stove parts or
other forms it is known as “cast iron”; through “puddling” in
reverberatory or special furnaces it becomes “wrought iron”; after
decarbonizing treatment in steel furnaces of various design it is
changed into the wonderful material called “steel.”
Pig iron is thus the _intermediate_ or _semi-raw_ material from which
practically all of our various iron and steel products are made and the
transition product through which they pass.
[Illustration:
MACHINE CAST PIG IRON
]
But the romantic period of the hand-fed furnace and the gloriously
beautiful pig beds at casting time are rapidly passing; in fact, are
almost past. Modern “skip-hoists” carrying automatically dumped buckets
or cars charge the furnace more economically than even low-waged
laborers can do it. The two charging cars alternate, one filling at the
bottom in the stock house while the other is dumping through the double
bell at the top of the furnace. Furnaces are now tapped by power driven
drills which make quick work of a formerly difficult operation. Instead
of running it into the sand bed, the molten iron from the furnace is
nowadays run into ladles alongside the cast house as is the cinder which
was described above. If the metal is to be made into pigs it goes to the
pig casting machine, where the traveling iron molds very quickly convert
the entire cast into “chilled cast” pigs. At the top of the incline
these pigs which have been cooling under sprays of water fall from the
traveling molds into railroad cars below which deliver them to the
consumer.
[Illustration:
HOW PIG IRON IS NOW CAST INTO TRAVELING MOLDS
]
[Illustration:
UPPER END OF CASTING MACHINE WHERE PIGS ARE DUMPED FROM TRAVELING
MOLDS INTO RAILWAY CARS
]
In large steel works the greater part of the molten iron is not cast
into pigs at all but while yet molten is directly charged into the
open-hearth or Bessemer furnaces which convert it at once into steel of
which the greater part is made into plate, rails, or other shapes before
being allowed to cool. Even the gas is recovered nowadays. Its journey
through the “dust arrester” rids it of most of its dust, after which
filters and washers clean it thoroughly. That not required for the
heating of the stoves is used for firing the steam boilers about the
plant and as fuel for batteries of huge gas engines which in large
plants have been installed to generate low-priced electric current.
It should be noted that in modern practice iron is mined, loaded,
transported to the furnaces, unloaded, charged and made into pigs or
converted into steel and even into the finished products with
practically no hand labor, all operations being performed by machinery.
Though a “direct” process for converting the ore into wrought iron or
steel has been long sought, a method has never been found, except that
used in the very small way followed by the old iron-workers with their
crude furnaces. It has always proved commercially advantageous to make
pig iron in the blast furnace as an intermediate step and then by a
second step convert it into wrought iron, steel, etc. So the ore is
brought from the mines to the furnace, the coke and limestone arrive
from another region, and batteries of huge blast furnaces through the
country make from them the pig iron.
BLAST FURNACE DATA AND ANNUAL PIG IRON PRODUCTION
═════╤══════════╤══════════╤══════════╤════════════════════════════════
Year │ Average │ Average │ Average │ Tons Pig Iron Produced During
│Height[1] │ Cu. Ft. │ Daily │ Year
│ of Blast │ Capacity │Output in │
│ Furnace │ of Blast │Tons Each │
│ │ Furnace │ │
─────┼──────────┼──────────┼──────────┼──────────┬──────────┬──────────
„ │ „ │ „ │ „ │ United │ Great │ Germany
│ │ │ │ States │ Britain │ and
│ │ │ │ │ │Luxemberg
─────┼──────────┼──────────┼──────────┼──────────┼──────────┼──────────
1850 │ 30′│ 2000│ 29│ 565,000│ │
1860 │ │ │ │ 920,000│ │
1870 │ │ │ │ 1,865,000│ 5,963,000│ 1,391,000
1880 │ 70′│ 8200│ 117│ 3,835,000│ 7,749,000│ 2,729,000
1890 │ 90′│ 18200│ 360│ 9,000,000│ 7,904,000│ 4,658,000
1900 │ 100′│ 24000│ 600│13,790,000│ 9,003,000│ 7,550,000
1905 │90 to 100′│ 24000│ 600│23,000,000│ 9,746,000│10,988,000
1910 │90 to 100′│ 24000│ 600│27,300,000│10,380,000│14,495,000
1912 │90 to 100′│ 24000│ 600│30,000,000│ 9,037,000│17,869,000
1913 │90 to 100′│ 24000│ 600│31,000,000│10,654,000│19,292,000
─────┴──────────┴──────────┴──────────┴──────────┴──────────┴──────────
Footnote 1:
No advantage has been found in furnaces having a height of over 110
feet.
The chemical laboratory plays a very important rôle in iron making.
Analyses made of each car or boat load of ore by the furnace chemists
representing the buyer must check very closely the analyses made by the
mine chemists for the seller, as the price of every ton of ore is based
on its iron and its phosphorus contents and the percentages of certain
other constituents present. In calculating the “burden” or charges for
the furnace, each of these constituents is estimated in pounds actually
present per charge, losses or gains during the journey through the
furnace are allowed for, and by combining the various ores the charges
are so made up that the resulting iron will be of certain desired
composition. The closeness of actual composition obtained to calculated
results is startling.
Truly this is an age of efficiency.
Though technical information and statistics are not to be inflicted upon
our readers to any extent in this series of articles, it may not be
amiss to give one table of interesting figures which show the increase
in height and capacity of furnaces from 1850 to the present time. During
this period the annual production of pig iron in the United States has
risen from 565,000 to 31,000,000 long tons (2240 pounds). It will be
noted that since 1887, when we passed Great Britain, the United States
has been the champion pig iron producer of the world.
The record production of a single blast furnace to date was that of one
of the United States Steel Corporation’s furnaces at Duquesne, Penn.,
which produced 900 tons of pig iron in one day.
CHAPTER V
A GENERAL GLIMPSE AHEAD
We have arrived at the parting of the ways. From the vast beds of iron
ore, the coal fields and coke ovens, and from the quarries of limestone,
all roads have led to the blast furnace. This we have visited and we now
know how pig iron is made.
From this point the several paths diverge. One by one we are to follow
them to get acquainted with the interesting country which they traverse
and the regions to which they lead. However, before choosing any one of
these paths for our first trip, it will be to our advantage to pause, to
study for a moment our position and get a general view of the country
ahead of us. We should know the relative locations and importance of the
places we are going to visit, for only by getting a comprehensive idea
of the general plan of this ferrous (meaning iron) world, can we
understand to the best advantage the position of each of the main
products, wrought iron, steel, cast iron, malleable iron, etc., and
acquire a satisfactory knowledge of them. In the last chapter pig iron
was called the intermediate stage between the ore and the finished iron
product, and such the sketch given shows it to be. It is only as an
intermediate product that pig iron has value, for nowhere in the
commercial world has it a purpose except as a material to be chemically
and structurally transformed into other materials which may themselves
be used without further transformation. It is desirable that we fully
realize the position of this very important semi-raw material, pig iron,
before passing on to the study, one at a time, of the refined ferrous
products which _are_ susceptible of _direct use_ in our commercial life.
[Illustration:
ELECTRIC ARC, MICROSCOPE, AND CAMERA, PART OF METALLOGRAPHIC APPARATUS
]
From Table A (page 71) it will be seen that from blast furnace metal
several well-known products are formed by the various processes of
refinement. Each of these methods of purification may be said to result
in a certain general composition and structure which give to the
material formed its character and properties.
The Metallographic Method of Classification
By aid of the microscope it is possible actually to look into the
structure of these materials.
TABLE A
IRON AND STEEL PRODUCTION OF THE UNITED STATES FOR 1912
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ 3000 Furnaces. │ │ Bar Iron, Sheets. │
│ │ │ │ │ WROUGHT IRON. │ │ Pipe, Boiler Tubes, │
│ │ │ │↗│ 1,637,582 tons │→│Stay Bolts. Stock for│
│ │ │ │ │ (750,000 tons Pig │ │ Cementation and │
│ │ │ │ │ Iron used). │ │ Crucible Steel. │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ 102 Plants. │ │ Rails, Axles, Rods, │
│ │ │ │ │ BESSEMER STEEL. │ │ Wire, Nails. │
│ │ │ │↗│ 1,327,900 tons │→│ Structural Shapes. │
│ │ │ │ │(11,000,000 tons Pig│ │ Pipe, Bar Steel, │
│ │ │ │ │ used). │ │ Steel Castings. │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ 78 Plants. │ │ │
│ │ │ │ │ ACID OPEN-HEARTH │ │Rails, Plate, Axles. │
│ │ │ │↗│ STEEL. │→│ Steel Castings. │
│ │ │ │ │ 1,139,221 tons │ │ Miscellaneous. │
│ │ │ │ │ (500,000 tons Pig │ │ │
│ │ │ │ │ used). │ │ │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ 100 Plants. BASIC │ │Rails, Plate, Axles, │
│ IRON ORE │ │ │ │ OPEN-HEARTH STEEL. │ │ Rods. Structural │
│59,975,000│↖│ │↗│ 19,641,502 tons │→│Shapes. Pipe, Boiler │
│ TONS │ │ │ │(11,500,000 tons Pig│ │ Tubes, Bar Steel, │
│ │ │ │ │ used). │ │ Steel Castings. │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ │ │ Stove, Radiator, │
│ │ │466 BLAST │ │ │ │ Machinery Parts, │
│COKE USED │ │ FURNACES │ │ CAST IRON. │ │ Valves, Pipe │
│35,491,292│←│ PIG IRON │→│ 6,750,000 tons │→│Fittings, etc., Bath │
│ TONS │ │ MADE │ │(5,000,000 tons Pig │ │ Tubs, Sinks, │
│ │ │29,726,937│ │ used). │ │ Carwheels, │
│ │ │ TONS │ │ │ │ Brakeshoes, Rolls, │
│ │ │ │ │ │ │ Misc. Castings. │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ │ │ Railway Car and │
│ CHARCOAL │ │ │ │ MALLEABLE IRON. │ │ Agricultural │
│35,436,017│↙│ │↘│ 1,000,000 tons │→│ Machinery Castings, │
│ BUSHELS │ │ │ │ (750,000 tons Pig │ │ Pipe Fittings, │
│ │ │ │ │ used). │ │ Miscellaneous │
│ │ │ │ │ │ │ Castings. │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│LIMESTONE │ │ │ │ 108 Plants. │ │Tool Steels, Ordnance│
│15,092,166│↙│ │↘│ CRUCIBLE STEEL. │→│Materials, Bar Steel,│
│ TONS │ │ │ │ 121,517 tons. │ │ Castings. │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ 14 Plants. │ │ Rails, Bar Steel, │
│ │ │ │↘│ ELECTRIC STEEL. │→│ Castings. │
│ │ │ │ │ 18,309 tons. │ │ │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
┌──────────┬─┬──────────┬─┬────────────────────┬─┬─────────────────────┐
│ │ │ │ │ 4 Plants. │ │ │
│ │ │ │↘│ OTHER STEEL │→│ Tool Steels, Bar │
│ │ │ │ │ PROCESSES. │ │Steel, Miscellaneous.│
│ │ │ │ │ 2853 tons. │ │ │
└──────────┴─┴──────────┴─┴────────────────────┴─┴─────────────────────┘
* Figures for Pig Iron Used are Estimates, no Conclusive Statistics
being available.
[Illustration:
PART OF A CHEMICAL LABORATORY WHERE 6,000 SAMPLES A YEAR ARE ANALYZED
]
By cutting in any direction through a piece of metal or alloy, polishing
the surface exposed very clean and smooth and then etching (corroding)
slightly with acid, the exposed grains of the metal may be seen when
sufficiently magnified. Not only may the grains of metal be seen, but
certain of the other constituents which are present are visible.
Photographs, also, can be taken by attaching a camera to the microscope.
This method of analysis, which is known as “metallography,” has proved
as valuable an aid to the metallurgist as it proved to the geologist
when applied to the study of rocks and geological specimens.
[Illustration:
MACHINE FOR DETERMINING STRENGTH OF IRON AND STEEL BARS
]
The metallography of wrought iron, cast iron, malleable iron and steel
differentiates them to us with considerable accuracy, as is shown by a
glance at the accompanying photomicrographs, as photographs taken
through the microscope are called.
For our immediate purpose of gaining a general knowledge of the relative
positions of these products, this method of analysis probably cannot be
excelled.
After the processes of manufacture of these materials have been taken up
one by one in later chapters, the photomicrographs will be even better
understood than now, as will the differences of chemical composition and
physical properties of the alloys, such as strength, hardness,
brittleness, forging quality, etc. The photomicrographs are given at
this time to show that the materials are structurally very different and
to aid in the general classification.
To make them comparative, all have been taken at the same magnification
of seventy diameters; i.e., the microscope has made everything shown
just seventy times as large as it actually was in the alloy.
[Illustration:
No. 198. PHOTOMICROGRAPH OF SAND CAST PIG IRON. THE THICK BLACK LINES
ARE GRAPHITE FLAKES
]
As stated before, the alloy _pig iron_ normally contains from 3 to 5½
per cent of carbon. This was absorbed during the journey through the
blast furnace. As long as the iron was molten all of this carbon was in
the “combined” form; i.e., in chemical combination with the iron itself.
Cold iron, however, cannot retain in the chemically combined form as
much carbon as does molten iron, so, during the solidification and
cooling of the alloy, more or less of its carbon was precipitated, i.e.,
thrown out of solution and from chemical combination with the iron, the
amount depending mainly upon the speed of the cooling. It appeared then
as the “free” carbon (crystalline graphite) which remained distributed
throughout the alloy and may be seen as the jet black flakes in
photomicrograph No. 198.
Every pure metal is supposed to be composed of crystals or grains which
would have been of the true cubic form if the severe internal pressure
during solidification and cooling had not distorted them.
Photomicrograph No. 99b represents quite well a pure metal. It is that
of an extremely mild steel made by special methods in the open-hearth
steel furnace. It is so highly refined that it can hardly be called
steel at all but is often called “_open-hearth iron_” or “_ingot iron_.”
It is probably the purest iron on the market in commercial quantities
to-day. While in the chemical laboratory iron of considerably greater
purity can be made, for a commercial product this is remarkably pure,
seldom containing more than ¼ per cent of elements other than the metal,
iron.
[Illustration:
No. 99b. OPEN-HEARTH IRON. PROBABLY THE PUREST COMMERCIAL IRON PRODUCT
]
The boundary lines of the crystals or grains may be plainly seen. Each
grain should show practically white. The dark parallel lines, the dots,
and the grayish portions result from inequalities in the polishing and
etching.
[Illustration:
No. 1d. SECTION OF WROUGHT IRON CUT LENGTHWISE OF THE BAR. BLACK
PATCHES AND FILAMENTS ARE “SLAG” OR “CINDER”
]
After noting the appearance of photomicrograph No. 99b, which is of a
nearly pure iron, one need have no difficulty in realizing that pig iron
and the steels are alloys and not simple metals. The truth is that of
all alloys some of the well-known iron products which we are studying
are by far the most complicated, much more so than are the nonferrous
alloys, which include the brasses, bronzes, babbitts, German silver,
etc.
[Illustration:
PHYSICAL TEST ROOM WHERE 15,000 SPECIMENS ARE TESTED EACH YEAR
]
This should not worry us, however, for we shall not attempt to follow
them into their complications.
[Illustration:
No. 3b. STEEL CONTAINING .10 PER CENT OF CARBON. THE CARBON IS IN THE
BLACK PATCHES
]
The important point just now is to observe the crooked black flakes of
crystalline graphite in this photomicrograph No. 198. It is largely
because of these flakes of brittle, soft graphite that pig iron and the
cast irons are so fragile. One has no difficulty in realizing that these
flakes, which cut in every direction through the metal, make it
structurally weak, especially toward a sudden blow.
No. 1d shows a typical section of _wrought iron_ cut lengthwise of the
rolled bar. It will be noted that, as in photomicrograph No. 99b, there
are no graphite flakes.
In the process of wrought iron manufacture practically all of the carbon
of the original pig iron is burned out, leaving little besides the iron
itself and some viscous cinder or slag. In the rolling or hammering out
of the resulting white-hot “bloom,” the slag enclosures which remain
after the squeezing process are extended lengthwise through the bar.
Upon observing with the microscope any prepared section of wrought iron
which has been cut lengthwise of the bar the filaments of slag may be
plainly seen, all parallel or practically so. When such filaments of
slag can be discerned in a longitudinal section it is practically an
absolute indication that the material in question is wrought iron.
[Illustration:
No. 22c. STEEL WITH .50 PER CENT OF CARBON
]
[Illustration:
No. 36a. STEEL WITH 1.98 PER CENT OF CARBON
]
Photomicrograph No. 3b is that of _mild steel_ containing .10 per cent
(⅒ per cent) of carbon. Here we have neither the graphite flakes of No.
198 nor the slag filaments of No. 1d. We can plainly see the boundary
lines of the grains. The irregular dark patches which are evenly
distributed throughout are the defining features of steel. In what might
be called a chemical-mechanical combination, these dark patches contain
all of the small percentage of carbon which gives to carbon steel its
definite properties.
During the manufacture of this alloy all but a small amount of carbon is
eliminated by burning it out, as happens with wrought iron. But the
steel is _molten_ or _fluid_ when finished and the slag which has been
formed floats on top and is also eliminated, which does not occur with
wrought iron, which is thick and pasty at its finishing temperature.
[Illustration:
No. 74. GRAY CAST IRON. THE CROOKED BLACK LINES ARE GRAPHITE FLAKES
]
Therefore, steel contains no graphite and no slag but has only the small
percentage of carbon which was purposely put back to give to it its
valuable properties.
[Illustration:
No. 92d. SEMI-STEEL, A STRONGER GRAY CAST IRON
]
Photomicrograph No. 22c is typical for steel which contains .50 per cent
(½ per cent) of carbon. The irregular patches containing the carbon are
much larger and more frequent. It will be seen, therefore, that through
metallography the various iron alloys, to a considerable extent, may be
analyzed as well as classified.
Photomicrographs Nos. 74 and 92d represent soft and stronger grades of
ordinary _gray cast iron_ respectively. It will be noted at once that
both much resemble pig iron in structure, as of course they should, for
simple remelting in the cupola does not effect much modification in
composition or structure.
Occasionally castings are made from molten iron direct from the blast
furnace, but such practice is not very satisfactory and is little done.
It forms probably the only exception to the statement made above that
pig iron has no useful purpose in the commercial world except as
something to be transformed by some refining process into another
material.
[Illustration:
No. 132. GRAY CAST IRON 200 YEARS OLD
]
[Illustration:
No. 109. MALLEABLE CAST IRON BEFORE ANNEALING
]
The remelting for the well-known cast iron is usually of such selected
brands of pig iron and cast scrap as will produce cast iron best adapted
to the purposes intended. The resulting alloy still contains 3 per cent
or 3½ per cent of carbon.
No. 132 is interesting. It is a photomicrograph of a piece of cast iron
which is approximately 200 years old. From the standpoint of the
metallurgist it is the same as other photomicrographs of cast iron, the
difference in appearance resulting probably from casting conditions,
etc.
_Malleable cast iron_ is made much as is gray cast iron except that it
is brought to such a composition that sections of castings made from the
melt show a white fracture when broken. Castings of gray iron of course
show a gray fracture. The former are extremely hard and are as brittle
as glass until they have gone through a careful long anneal or heat
softening process. By maintaining them at cherry-red heat away from air
for sixty hours or more and cooling slowly, they become “malleable”;
i.e., not brittle at all but capable of considerable distortion without
cracking.
[Illustration:
No. 35. MALLEABLE CAST IRON ANNEALED
]
From the viewpoint of malleability, malleable iron may be considered to
occupy a position between gray cast iron and steel.
Photomicrographs Nos. 109 and 35 are those of malleable iron before and
after the annealing treatment. The former shows the typical structure of
_white cast iron_, while the latter plainly shows the minute lumps of
pure carbon and the surrounding grains of pure iron metal, the two
having become divorced through the annealing process. Note that the
large amount of carbon in this, the “temper carbon” form, does not make
the alloy brittle through cutting of the grains as does the crystalline
graphite form of carbon.
The above gives very briefly the most essential points in the
classification of the irons and steels from the structural standpoint.
True it has not entered into the vast complications of the higher carbon
or tool steels which are those which will take a “temper”; i.e., the
tool steel’s quality of hardening by quenching in water from a cherry
red heat. The simpler points of these will be taken up later. But enough
has been given that we now understand something of the relative
positions of the great main products, some reasons therefor, and their
general structures.
[Illustration:
NO. 8. BAR ROLLED FROM SCRAP; CONTAINS BOTH WROUGHT IRON AND STEEL
]
It has been seen that their micrographs quite definitely differentiate
them and probably no one will have difficulty in recognizing and naming
such specimens. As testing this it may be interesting to note
photomicrograph No. 8. Two different iron alloys made up the material
from which this photomicrograph was taken. Apparently the bar was one
made by heating and rolling together scrap metals. Such material is on
the market. The photomicrograph shows that some of the scrap used was
wrought iron and some of it mild steel of about .08% carbon.
Classification by Chemical Analysis and by Physical Tests
So far not much has been said about composition except that upon it to a
great extent depends the structure and physical properties of the alloy.
Composition and physical characteristics as well as structures are
necessary to a fair
TABLE B—CHEMICAL COMPOSITION AND PHYSICAL PROPERTIES
═══════════════╤═══════╤═════════╤════╤══════╤═══════════╤═══════════
│ Per │Per Cent │Per │ Per │ Beginning │ Tensile
│ Cent │Graphitic│Cent│ Cent │ of │Strength[3]
│Silicon│ Carbon │ │Total │Freezing[2]│
│ │ │ │Carbon│ │
───────────────┼───────┼─────────┼────┼──────┼───────────┼───────────
1. Sand Cast │ 2.50│ 3.75│ .25│ 4.00│ 2100│
Pig Iron │ │ │ │ │ │
2. Machine │ 2.50│ 3.00│1.00│ 4.00│ 2100│
Cast Pig │ │ │ │ │ │
Iron │ │ │ │ │ │
───────────────┼───────┼─────────┼────┼──────┼───────────┼───────────
3. Open-Hearth│ .03│ .00│ .02│ .02│ 2740│ 50,000
Iron │ │ │ │ │ │
4. Wrought │ Slag│ .00│ .05│ .05│ 2740│ 52,000
Iron │ │ │ │ │ │
│ │ │ │ │ │
5. Mild Steel │ .05│ .00│ .10│ .10│ 2740│ 55,000
│ │ │ │ │ │
│ │ │ │ │ │
│ │ │ │ │ │
6. Medium │ .05│ .00│ .25│ .25│ 2720│ 65,000
Steel │ │ │ │ │ │
7. Rail Steel │ .05│ .00│ .60│ .60│ 2680│ 90,000
8. Low Carbon │ .15│ .00│ .75│ .75│ 2660│ 100,000
Tool │ │ │ │ │ │
Steel │ │ │ │ │ │
9. Medium │ .15│ .00│1.00│ 1.00│ 2630│ 120,000
Carbon │ │ │ │ │ │
Tool │ │ │ │ │ │
Steel │ │ │ │ │ │
10. High Carbon│ .15│ .00│1.25│ 1.25│ 2600│ 135,000
Tool │ │ │ │ │ │
Steel │ │ │ │ │ │
11. Very High │ .15│ .00│1.50│ 1.50│ 2560│ 124,000
Carbon │ │ │ │ │ │
Tool │ │ │ │ │ │
Steel │ │ │ │ │ │
12. High Steel │ │ .00│1.75│ 1.75│ 2530│
│ │ │ │ │ │
13. White Iron │ │ .00│2.50│ 2.50│ 2460│
│ │ │ │ │ │
14. White Cast │ .70│ .10│2.65│ 2.75│ 2400│ 41,000
Iron │ │ │ │ │ │
│ │ │ │ │ │
15. Annealed │ .70│ 2.70│ .05│ 2.75│ │ 40,000
Malleable│ │ │ │ │ │
Cast Iron│ │ │ │ │ │
│ │ │ │ │ │
16. Cast Iron │ 1.00│ 1.00│2.00│ 3.00│ 2330│ 35,000
for │ │ │ │ │ │
Chilled │ │ │ │ │ │
Castings │ │ │ │ │ │
17. Semi-Steel │ 1.75│ 2.80│ .40│ 3.20│ 2300│ 35,000
│ │ │ │ │ │
│ │ │ │ │ │
18. Gray Cast │ 2.00│ 3.10│ .30│ 3.40│ 2200│ 25,000
Iron │ │ │ │ │ │
│ │ │ │ │ │
│ │ │ │ │ │
│ │ │ │ │ │
19. Soft Gray │ 2.50│ 3.30│ .15│ 3.45│ 2200│ 23,000
Cast Iron│ │ │ │ │ │
│ │ │ │ │ │
│ │ │ │ │ │
───────────────┴───────┴─────────┴────┴──────┴───────────┴───────────
═══════════════╤═════════════╤══════════╤═════════════════
│Elongation[4]│ Welding │ Principal Uses
│ │Properties│
│ │ │
│ │ │
───────────────┼─────────────┼──────────┼─────────────────
1. Sand Cast │ │ │Further Refining.
Pig Iron │ │ │
2. Machine │ │ │Further Refining.
Cast Pig │ │ │
Iron │ │ │
───────────────┼─────────────┼──────────┼─────────────────
3. Open-Hearth│2½″ │ Good │Bars, pipe,
Iron │ │ │ sheet.
4. Wrought │2¼″ │ Fine │Bars, pipe,
Iron │ │ │ boiler tubes,
│ │ │ stay bolts.
5. Mild Steel │2½″ │ Good │Bars, pipe, wire,
│ │ │ sheet,
│ │ │ shafting,
│ │ │ tubes.
6. Medium │2¼″ │ Good │Bars, plate,
Steel │ │ │ structural.
7. Rail Steel │1¾″ │ Fair │Rails, gears.
8. Low Carbon │1¼″ │ Fair │Hammers, cold
Tool │ │ │ chisels, saws,
Steel │ │ │ springs.
9. Medium │1″ │ Poor │Lathe tools,
Carbon │ │ │ chisels,
Tool │ │ │ drills, dies,
Steel │ │ │ springs.
10. High Carbon│1⅛″ │ Slight │Lathe tools,
Tool │ │ │ chisels, files,
Steel │ │ │ saws.
11. Very High │ ¼″ │ Slight │Razors, lancets,
Carbon │ │ │ graving tools,
Tool │ │ │ saws for steel.
Steel │ │ │
12. High Steel │0 │ None │Dies for wire
│ │ │ drawing.
13. White Iron │0 │ None │Dies for wire
│ │ │ drawing.
14. White Cast │0 │ None │For
Iron │ │ │ malleableizing,
│ │ │ carwheels.
15. Annealed │ ½″ │ None │Railway and
Malleable│ │ │ agricultural
Cast Iron│ │ │ castings,
│ │ │ fittings.
16. Cast Iron │0 │ None │Rolls, gears,
for │ │ │ brakeshoes.
Chilled │ │ │
Castings │ │ │
17. Semi-Steel │0 │ None │Gears, steam
│ │ │ cylinders,
│ │ │ valves.
18. Gray Cast │0 │ None │Machine parts,
Iron │ │ │ grates,
│ │ │ radiators,
│ │ │ valves, soil
│ │ │ pipe.
19. Soft Gray │0 │ None │Stoves,
Cast Iron│ │ │ hollowware,
│ │ │ pipe fittings,
│ │ │ misc.
───────────────┴─────────────┴──────────┴─────────────────
Footnote 2:
In degrees Fahrenheit. For our purposes, the same as the _melting
points_ of the alloys.
Footnote 3:
Pounds required to pull apart lengthwise a bar one inch square.
Footnote 4:
Number of inches that a bar eight inches long will stretch before it
breaks.
[Illustration:
IRON AND STEEL TEST PIECES AND INSTRUMENTS USED IN MEASURING THEIR
SIZE, ELASTIC LIMIT AND ELONGATION
]
understanding of the subject. There is given therefore, a table showing
approximate comparative values of chemical compositions and physical
properties of the alloys under discussion.
It should be distinctly understood that the figures given in Table B are
_approximate_ only and are intended to be average, or rather, perhaps,
typical.
There are all sorts of conditions which in practice modify the figures
given in the table, and criticism may be maintained justly against some
of the too specific statements which here it was necessary to make. The
classification is given with considerable hesitation and only because,
arranged in this way, it brings out existing relationships which
otherwise would escape notice and which we cannot afford to overlook.
But please do not gain the impression that these alloys are divided into
distinct classes. There are no dividing lines at all. One group merges
into the next so gradually that it is impossible to tell where the one
ends and the other begins.
It is to be hoped that no one will make himself miserable by trying to
digest these rather formidable figures of Table B all at one sitting.
They are given mainly for comparison and for reference. It is suggested
that after noting carefully the similarities and differences to which
attention is called, they be reserved until the processes of manufacture
of the various alloys are taken up one by one. Reference to these
figures on those occasions should be profitable.
The main points to be noted at this time are:
1. Open-hearth iron is practically pure iron, having no constituents or
slag inclusions which materially affect its properties.
2. Wrought iron, for all practical purposes, is pure iron except for its
content of slag. It is the only one of the iron family which does
normally contain slag.
3. Neither open-hearth iron nor wrought iron contains carbon in
appreciable quantities.
4. The distinguishing and active element of the steel family is carbon.
With increase of carbon the hardness of the alloy increases as does its
tensile strength, but the ductility (elongation or stretch) decreases.
5. Other conditions being equal, the more carbon the alloy contains the
more easily it melts; i.e., at lower temperature. So the purer irons
such as open-hearth iron, wrought iron, and mild steel (i.e., steel with
low carbon, usually under 0.15 per cent) have relatively high and the
cast irons lower melting points.
TABLE C—PERCENTAGES OF THE SO-CALLED “METALLOIDS” BY WEIGHT AND BY
VOLUME
═══════════════════╤═══════════╤══════════╤═════════╤══════════
│ Silicon │Manganese │ Sulphur │Phosphorus
│ │ │ │
───────────────────┼────┬──────┼────┬─────┼───┬─────┼────┬─────
│Wt. │ Vol. │Wt. │Vol. │Wt.│Vol. │Wt. │Vol.
───────────────────┼────┼──────┼────┼─────┼───┼─────┼────┼─────
Gray Cast Iron │2.50│=10.0=│ .70│ =.7=│.09│=.36=│ .75│=3.2=
Semi-Steel │1.75│ =7.0=│1.00│=1.0=│.10│=.40=│ .35│=1.5=
Malleable Cast Iron│ .70│ =2.8=│ .50│ =.5=│.15│=.60=│ .17│ =.7=
Cast Steel │ .30│ =1.2=│ .50│ =.5=│.05│=.20=│ .04│=.17=
Mild Steel │ .05│ =.2=│ .40│ =.4=│.04│=.16=│ .03│=.13=
Open-hearth Iron │ .03│ =.1=│ .02│=.02=│.01│=.06=│ .01│=.06=
Wrought Iron │1.20│ =5.0=│ .08│=.08=│.01│=.04=│ .15│=.65=
───────────────────┴────┴──────┴────┴─────┴───┴─────┴────┴─────
═══════════════════╤═══════════╤═══════╤══════════
│ Total │Iron[5]│ Total
│ Carbon │ │Metalloids
───────────────────┼────┬──────┼───────┼───┬──────
│Wt. │ Vol. │ Wt. │Wt.│ Vol.
───────────────────┼────┼──────┼───────┼───┼──────
Gray Cast Iron │3.45│=12.1=│ 92.5 │7.5│=26.4=
Semi-Steel │3.20│=11.2=│ 93.6 │6.4│=21.1=
Malleable Cast Iron│2.75│ =9.6=│ 95.7 │4.3│=14.3=
Cast Steel │ .35│ =1.2=│ 98.8 │1.2│ =3.3=
Mild Steel │ .10│ =.35=│ 99.4 │ .6│ =1.2=
Open-hearth Iron │ .02│ =.07=│ 99.9 │ .1│ =.3=
Wrought Iron │ .05│ =.17=│ 97.7 │2.3│ =5.9=
───────────────────┴────┴──────┴───────┴───┴──────
Footnote 5:
These alloys contain small amounts of other elements so these
percentages of iron are a little high, though approximately correct.
Note the purity (high percentage of iron) of the open-hearth iron.
6. In the cast irons, the carbon occurs not in one only but in two
different forms; i.e., as graphitic carbon, commonly called graphite
(Gr. C.) and the combined form (C. C.). The sum of these is usually
between 3.00 per cent and 3.50 per cent. It is not so much the total
amount of the carbon that causes the differences in structure and
physical properties which have been noted in 1 and 2 and in 16 and 17
above, as it is the _relative proportions_ in which these two varieties
occur.
[Illustration:
EXHIBITION CASE SHOWING FOUR WELL-KNOWN IRON ALLOYS WITH THEIR
METALLOIDS
]
7. No one knows just when, with increase of carbon, steel ceases to be
steel and becomes white cast iron. There is no definite dividing line
either in chemical or physical properties. The changes are extremely
gradual throughout the scale. Aided by the microscope, modern physical
chemistry has disclosed the fact that alloys of iron with carbon
“freeze” from molten to solid condition according to two different laws.
The change from one to the other occurs somewhere between 1.7 per cent
and 2.2 per cent of carbon as is described in Chapter XXII. This is our
only basis for calling alloys with less than 2 per cent of carbon,
steels, and those with greater amounts, cast irons.
8. For our immediate purposes the other “metalloids” or constituents are
of secondary importance and will not be taken up now. From this it must
not be understood that they can be slighted by the metallurgist and
furnace man in his work. They cannot. Every one of them is of importance
and must be accounted for in the final product or trouble results.
Volumetric Analysis of the Iron Alloys
There is a way in which we may visually get a very intimate idea of the
relative composition of these alloys.
The cabinet of which a photograph is given is partitioned into four
sections. Each one of these contains a bar and six specimen jars. As you
may or may not be able to read from the labels, the bars, all of exactly
the same size, are soft cast iron, semi-steel (a stronger cast iron),
annealed malleable iron and cast steel. The six jars above each bar
contain the exact amounts of the various constituents other than iron
which are in the bar beneath.
As none of the constituents except manganese are as heavy as iron, their
volumes per unit of weight are correspondingly greater. Putting it into
approximate figures we have the percentages by weight and by volume
shown in Table C.
This means, of course, that _of the cast iron plates of your cook stove
or steam or water radiators fully one-quarter (26 per cent by volume) is
not iron at all_ but brittle substances of little or no strength. These
elements, silicon, sulphur, phosphorus, and carbon, are commonly called
“metalloids.” While the first three named are not in “free” form in the
alloy and therefore allow of some doubt as to just the space they
require, we have good reason to suppose that the figures given are not
far from correct.
With such a volume of weakening constituents and particularly with the
graphite flakes cutting through and separating the iron grains as the
photomicrographs show, can one wonder that cast iron is fragile—more so
than steel or wrought iron?
To sum up, naming only the most familiar alloys and the two or three
qualifying features of each which stand forth with particular boldness,
we have:
_Pig Iron_—Very High Carbon. Brittle.
_Gray Cast Iron_—High Carbon. Brittle.
_Malleable Cast Iron_—High Carbon. Made Malleable by Annealing.
_Wrought Iron_—Slag. Little or no Carbon. Very Malleable without
Annealing.
_Mild Steel_—Very Low Carbon. No Slag. Very Malleable without Annealing.
_Carbon Tool Steel_—Medium Carbon. No Slag. Of Medium Malleability.
So steel which is not called “iron” at all is a very pure metal in
comparison with gray and malleable cast iron and usually has a larger
percentage of the chemical element, iron from which all are derived,
than has the well-known wrought iron itself.
CHAPTER VI
WROUGHT IRON
We of America, and especially of the West, never have been particularly
devoted to the study of our genealogies. However, it is likely that most
of us at one time or other in our mind’s eye have seen that little
country town back in Massachusetts or New York State, whence came our
forebears. Since those days of long ago, when, with you upon his knee,
grandfather waxed reminiscent and related tales of his boyhood, haven’t
you many times wished that Father Time could carry you back with him a
hundred and fifty years and allow you for a few hours to walk among
those good people with their quaint dress and customs? How interested
you would be in the relatives and friends whose queerly transcribed
verses, bearing date of a century and a half ago, adorn the yellow pages
of your great aunt’s autograph album, which is one of your treasures!
To the present rather unsentimental world we admit of much the same sort
of reverent feeling as we traverse the paths, centuries old, of the
wrought iron region. Here is something which links us with the
antiquities and we “take off our hats and tread lightly” over the lands
and the centuries in and through which this primal material, wrought
iron, has been produced.
But we come back to a plain statement of the case. Let not the fact be
overlooked that it is wrought iron which in some form or other has been
made during the forty or more centuries that iron has been known. It
undoubtedly was the pioneer of the iron family and through all of the
centuries it has maintained its importance. From it as a base during the
earlier centuries were made the steels for which the ancients were so
famous, and similar practice has prevailed from those early times up to
the present day.
[Illustration:
WROUGHT IRON BAR Steel has no “fiber” and can not be split in this
way.
]
We say that the iron made by the ancients was in reality a variety of
what we now term wrought iron, for it fulfilled three of the principal
requirements for wrought iron, viz., it was not necessarily melted
during production, it was a malleable metal, and it contained cinder or
slag, but practically no carbon.
Early iron and steel, of course, were comparatively rare, so much so as
to be available only for implements of war and for particular purposes.
Moreover, all of the steel made was of the high carbon, hard variety,
none of it being of the low carbon sort which we know as the soft or
mild steels. The latter have all come since the invention of the
Bessemer process in 1855 and the Siemens-Martin (the open-hearth)
process of a few years later.
As you will remember the next development in the iron industry was the
use of the larger blast furnace and much more fuel, with higher
temperatures and the production of cast iron which, by reason of the
absorption of considerable carbon from the fuel, was fluid enough to run
out of the furnace. And, as you also know, this blast furnace metal has
come to be the great intermediate product in what has come to be known
as the _Indirect Process_ of making iron and steel.
[Illustration:
PICKLING IN WEAK ACID EXPOSES THE “FIBERS” OF WROUGHT IRON
]
As pig iron contains 3½% or more of carbon, while wrought iron has none
or comparatively little of this embrittling element, any process for
converting the pig iron into wrought iron must eliminate the carbon.
Following the advent of pig iron as a commercial product several
furnaces and processes were developed to turn it into wrought iron. All
of these were based upon the elimination of the carbon by _oxidation_,
which means the burning of the carbon in presence of oxygen of the air.
The best known ones were the Walloon or Swedish Lancashire process, the
South Wales process, the Finery Fire, the Running-Out Fire and the
Charcoal Finery or Knobbling process. The Walloon furnace, largely used
in Sweden, is shown in the illustration on page 94.
While by the process generally used to-day wrought iron is more easily
and cheaply produced, it must be said that by the processes above named
has been made as fine iron as has ever been produced. The Sheffield
manufacturers, whose high grade steel made by the crucible process, is
so widely and favorably known for cutlery, tools, etc., in many cases
yet demand the Walloon process iron made from high grade Swedish ores as
the starting point for their product.
[Illustration:
BAR IRON WILL STAND SEVERE BENDING EVEN AFTER IT HAS BEEN NICKED
]
[Illustration:
SWEDISH WALLOON FURNACE
One of several types of furnaces that preceded the Reverberatory. Some
of them are still used.
]
In these furnaces which consisted mainly of a shallow hearth filled with
glowing charcoal, with tuyères for blast supply, the pigs of iron were
heated until molten. At high temperatures the metalloids of pig iron
will readily burn in a blast of air. After the air blown over and upon
the molten metal has burned out most of the carbon, the main metalloid,
the melting point of the purified metal becomes so much higher that the
heat of the furnace is not sufficient to keep it molten. It becomes more
and more pasty and stiff therefore. This is what the iron maker calls
“coming to nature.” It is the signal that the carbon is about gone and
that he must be careful or the iron will suffer in quality. At this
stage he sees to it that the mass of pasty iron is well protected by
glowing charcoal until it is removed to be hammered or worked into a
bar.
This in general is the process which was used from about the fourteenth
century up to 1783 when Cort invented the reverberatory furnace which
has since been the type generally used.
In the processes just referred to, all very similar, it should be noted
that the iron was _in contact_ with the fuel, which, therefore, _had to
be charcoal_, the fuel with little or no sulphur.
[Illustration:
CORT’S REVERBERATORY FURNACE
This is the type of furnace generally used to-day.
]
Charcoal was an expensive fuel, and, moreover, there was an insufficient
supply because of the great destruction of forests necessary for its
production. Naturally the thing to do was to substitute coal, which was
plentiful. But the sulphur of the coal spoiled the iron.
This proved to be a great barrier until 1783 when Henry Cort of England
succeeded in making wrought iron in a new type of furnace wherein the
iron was refined in one compartment while the fuel was made to furnish
its heat from another; i. e., the fuel and the metal _were not in
contact_ and the refined metal did not suffer from the sulphur content
of the coal.
The figure illustrating Cort’s furnace plainly shows how this was
accomplished and it represents almost as well the furnace used to-day.
In the one-hundred and thirty-three years that have elapsed since it was
designed, his furnace has been changed only in certain details, and but
two important changes have been made in his process—the use of an iron
bottom instead of the sand bed by S. B. Rogers in 1804 and the
introduction of “pig boiling” by Joseph Hall in 1830.
Cort’s process is known as “dry puddling” and his trouble was the
excessive loss of iron, due to his use of the sand bottom and the
absence of a proper cinder. The loss was said to have been from 50% to
70% of the iron charged; i. e., it took about 2 tons of pig iron to make
one ton of wrought iron. Because of the great demand for iron and the
fact that he was using such a cheap fuel, coal, his process at that time
was a success financially.
[Illustration:
EARLY IRON ROLLS
While Cort did not originate the idea, it was he who first made the
rolling process successful, and, therefore, he is given credit for
the invention.
]
But Cort did not stop here. He saw the desirability of a quicker and
more economical method of reducing the “blooms” or balls of iron into
bars or other finished shapes than the hammering process up to that time
used. He accomplished this by the use of power driven rolls, such as
those shown in the cut.
These two inventions of Cort’s were epoch making, though of the two the
more important one was the invention of the rolls from which has
developed the modern rolling mill.
There remains to be described in a little more detail the making of
wrought iron as practiced to-day. The puddling furnace used has a grate
upon which is built the coal fire. The long flame passes over the fire
wall and is deflected by the roof down upon the charge of pig iron piled
upon the “fettling” or lining of iron oxide (iron ore or mill scale)
over the air or water cooled iron plates which form the bottom and the
sides of the hearth.
With a long iron bar the “puddler” (the expert attendant) turns the pigs
until they have melted down into the bath of slag or cinder charged and
continually being formed by the chemical union of iron from the ore or
pig and some of the sand and other impurities present. This cinder,
which is largely a silicate of iron, is a protection for the bath of
molten iron and its use prevents excessive oxidation and loss of metal.
During the melting of the charge the heat is kept as high as possible
and the molten iron is “puddled,” i. e., stirred, by the “puddler” or
his helper with a “rabbler” or iron bar. In order to take out the
phosphorus and sulphur, which for best results should be removed before
the carbon is eliminated, the heat of the furnace is lowered somewhat as
soon as all of the pig has melted, and some iron oxide is mixed into the
“bath” of molten iron and cinder. Most of the phosphorus and sulphur are
chemically acted upon and pass into the cinder which covers the iron.
Soon the mass begins to boil or seethe and small blue flames break
through the cinder covering. This indicates that the carbon is being
oxidized by the oxygen of the iron ore which was added, the oxygen, as
in the blast furnace, having a greater “affinity” for carbon than it has
for the iron.
This “pig boiling” goes on for twenty or thirty minutes, the “puddler”
meanwhile “rabbling” the charge in order to hurry the reactions and to
make sure that all parts of the bath of molten metal are uniformly
exposed to the oxidizing conditions.
[Illustration:
THE MAKING OF WROUGHT IRON TO-DAY. CHARGING THE PIG IRON
]
Soon the metal begins to “come to nature” and little lumps of pure iron
here and there through the bath stiffen up into little pasty balls. Some
may be seen sticking out through the cinder covering of the bath and
others must be torn loose from the bottom with the rabbler. This
“balling” period lasts from fifteen to twenty minutes, during which time
all of the iron has “come to nature.”
[Illustration:
THE COAL PILE AND FIRE BOX OF A REVERBERATORY FURNACE
]
[Illustration:
TURNING THE PIGS TO INSURE EVEN MELTING
]
The puddler quickly separates into two or three white-hot balls the 400
pounds or so of spongy iron. These balls, full of and dripping with
cinder, are seized, one at a time, with long tongs, removed from the
furnace and rushed to the rotary squeezer through which they are twisted
and turned, ever becoming longer and smaller in diameter until they
emerge from the other and narrower side much compacted and with but
little of the cinder which they originally carried. Without being given
time to cool, the blooms are seized and shoved into the “muck rolls,”
whence after a few passes they emerge as long flat bars, very rough and
imperfect in appearance.
After shearing into short lengths, many pieces of this “muck bar,” as it
is called, are made into “box piles” and tied together with wires. These
are charged into the furnace of the finishing mill. After coming to a
white heat the box piles go to the finishing rolls where they are rolled
into bars, rods, plates, or other shapes desired. By repeated cutting,
piling, heating, and rolling, double refined and other high grades of
wrought iron are made, each repiling and rerolling, of course, producing
a more compact and better product.
[Illustration:
PUDDLING THE MELTED CHARGE
]
[Illustration:
CONSIDERABLE CINDER OVERFLOWS DURING THE “BOILING” STAGE
]
Wrought iron has a “fiber,” as may be seen from two of the illustrations
presented. In “coming to nature” small particles of iron crystallize out
as they become purer. These measure perhaps ¹⁄₃₂″ or ¹⁄₁₆″ in diameter.
As it goes to the squeezer the ball of “sponge” is made up of such
grains of iron loosely welded together with the interstices filled with
cinder. The squeezer, and later the rolls, elongate the particles of
iron into threads, which, welded together, make the bar.
It is thought by some that films of cinder, too thin to be seen under
the microscope, surround each fiber of iron and that these afford
protection from rusting and give to wrought iron the excellent welding
quality that it possesses.
[Illustration:
DRAWING ONE OF THE BALLS FROM THE FURNACE
]
[Illustration:
ON THE WAY TO THE “SQUEEZER”
]
Steel has no fiber and for this reason it cannot be split as was the
wrought iron bar shown in the illustration of page 92.
It will have been noticed that only small amounts of iron can be refined
at one time. This, indeed, has been the unfortunate part of wrought iron
manufacture, for it may readily be seen that production of any such
material in lots as small as a quarter ton results in labor costs which
are almost prohibitive in these days of machine-made goods. Not only is
the output of a furnace small but much skill and judgment are necessary
for the production of a high grade product. Very sturdy and strong men,
too, are required as puddlers, for the work is heavy and the extremes of
heat and cold to which they are exposed necessitate men of rugged
health.
[Illustration:
CROSS-SECTION OF A “SQUEEZER”
]
This material in bar iron, engine stay bolts, butt and lap-welded pipe
and certain other products has long held a high place. Though not as
strong as steel, its very excellent welding properties and comparative
freedom from “crystallization” and treacherous breakage under long
continued vibration or sudden jar have fostered its application in such
products as stay bolts, chain-links, cable hooks and others where
failure might have serious consequences. Too, it is thought by many that
pipes, sheets and other articles of wrought iron resist the corrosive
influences of moist air, soil, etc., particularly well. The cinder films
in which the fibers are supposed to be encased are given credit for such
protective influence.
[Illustration:
“BOX PILES” READY FOR THE RE-HEATING FURNACE
]
Though the product has always been a favorite with iron users, the
industry has suffered during the last sixty years by reason of the high
cost of manufacture, which has very largely restricted the application
of wrought iron to certain uses for which first cost is not a main
factor.
The production of wrought iron rails has rapidly dwindled since the year
1880, when they began generally to be replaced by rails made from
Bessemer steel.
[Illustration:
THE BALL GOING INTO THE “SQUEEZER”
]
[Illustration:
SHEARING THE MUCK BAR INTO SHORT LENGTHS FOR “PILING”
]
[Illustration:
THE BLOOM FROM THE SQUEEZER GOES TO THE “MUCK” ROLLS WHICH ROLL IT
DOWN INTO “MUCK BAR”
]
[Illustration:
THE RE-HEATED “BOX PILES” BEING ROLLED INTO “SKELP” FOR PIPE, IN THE
FINISHING MILLS
]
[Illustration:
CROSS PILING GIVES CROSS FIBERS IN THE FINISHED BAR—A DESIRABLE
QUALITY
]
Of recent years, mild steel has been the great competitor of wrought
iron. With marvelous energy, skill, and much capital the manufacturers
of Bessemer and open-hearth steels have adapted their products very well
to the needs of the iron user, while the enormous tonnages turned out in
short time by use of ingenious furnaces and other devices has resulted
in a low cost of production.
Had any of the several mechanical puddling furnaces devised for the
manufacture of wrought iron proved really successful, things might be
more rosy commercially for this very excellent material.
According to the 1916 Statistical Report of the American Iron and Steel
Institute, the recent yearly production in this country of wrought iron
and steel merchant bars, plates and sheets, and skelp for pipe in gross
tons has been:
════╤═══════════════════╤═══════════════════╤═══════════════════
│ Merchant Bars │ Plate and Sheets │ Skelp for Pipe
────┼─────────┬─────────┼─────────┬─────────┼─────────┬─────────
│ Iron │ Steel │ Iron │ Steel │ Iron │ Steel
────┼─────────┼─────────┼─────────┼─────────┼─────────┼─────────
1905│1,322,439│2,271,162│ 72,156│3,460,074│ 452,797│ 983,198
1906│1,481,348│2,510,852│ 74,373│4,107,783│ 391,517│1,137,068
1907│1,440,356│2,530,632│ 74,038│4,174,794│ 444,536│1,358,091
1908│ 685,233│1,301,405│ 54,033│2,595,660│ 297,049│ 853,534
1909│ 952,230│2,311,301│ 76,202│4,158,144│ 370,151│1,663,230
1910│1,074,163│2,711,568│ 91,118│4,864,366│ 350,578│1,477,616
1911│ 835,625│2,211,737│ 89,427│4,398,622│ 322,397│1,658,276
1912│ 944,790│2,752,324│ 75,044│5,800,036│ 327,012│2,119,804
1913│1,026,632│2,930,977│ 64,729│5,686,308│ 312,746│2,189,218
1914│ 563,171│1,960,460│ 56,590│4,662,656│ 264,340│1,718,091
1915│ 657,107│3,474,135│ 20,253│6,057,441│ 262,198│2,037,266
1916│ 993,948│5,625,598│ 13,303│7,440,677│ 355,445│2,572,229
────┴─────────┴─────────┴─────────┴─────────┴─────────┴─────────
There is considerable so-called wrought iron on the market to-day which
is not truly wrought iron, by which we mean iron “puddled” from pig
iron.
Bushelled Iron
After heating a mixture of thin sheet or other soft steel and wrought
iron scrap to a welding heat in a reverberatory furnace, it may be
balled and put through the squeezer, muck rolls, etc., as was the true
wrought iron made by puddling. This manipulation of scrap is known as
the bushelling process and the product as “bushelled iron” or “scrap
bar.” By using scrap bar for the outer layers and old wrought iron bars
cut to length for the interior, box piles are made, which, heated and
rolled, make very good material, though not as good as puddled iron.
Certain grades on the market, e. g., common bar iron, contain more or
less of this bushelled iron, but the better grades, refined wrought
iron, double refined wrought iron, engine and stay-bolt iron, are
usually the pure puddled product.
As with the latter, repeated shearing, piling, and rolling improve the
quality.
Bushelled iron is largely the result of an endeavor to reduce the cost
of production of wrought iron. The material has a legitimate place and
considerable of it is used.
CHAPTER VII
CEMENTATION AND CRUCIBLE STEELS
In the early days practically the only steels recognized—certainly the
only ones desired—were of the high carbon or hardening variety. These
were required for the manufacture of swords and other implements of war,
for tools, etc., most of which had to have hard and sharp cutting edges.
When softer and less brittle metal was desired, wrought iron was
available, but in all probability high carbon steel was the material
most largely used.
Having but the two iron alloys and these of very different properties,
it was not difficult to distinguish between them. A piece of metal could
be heated to redness and plunged into cold water. If it became glass
hard when cooled in this way it was thereby proved to be steel; if still
soft, it was iron.
But the problem is not so simple to-day. Medium, mild and yet softer
steels, and other alloys which have steel characteristics have appeared
and are used in immense quantities. Their advent introduced considerable
complication.
It will be well, therefore, before taking up our subject, “Cementation
and Crucible Steel,” and the several steels which are to follow, to make
sure that we all understand, as well as we may, what is “steel” as
defined to-day, what are the best known varieties, and what are their
characteristics?
For a rough classification it is safe for us to divide the steel world
into four general divisions as follows:
1. The harder, high carbon steels used for tools, dies, etc.
2. The mild and medium steels of which wire, rod, bar, plate, pipe and
structural shapes for bridges, ships and “sky scrapers” are made.
[Illustration:
HARDENING A PIECE OF TOOL STEEL. READY TO QUENCH
]
3. Alloy steels, to which some metal such as nickel, manganese or
chromium gives definite properties and the name.
4. Those other modern materials which are known as “self-hardening” and
“high-speed steels.”
[Illustration:
BOWKNOT MADE FROM PIECE OF STEEL PIPE
]
The two classes last named are not simple iron-carbon alloys and their
properties are less directly derived from and do not so plainly depend
upon carbon. Metallurgically, then, they are not steels in the exact
former sense of the word; but as they do require carbon—though perhaps
in lesser amount, are made by regular steel processes, have most of the
characteristics of steel and are used for the same general purposes,
they are undoubtedly entitled to the appellation “steel.” However, to
distinguish, they are usually termed “alloy steels.”
We are just now concerned only with the steels of classes one and
two—the carbon steels. As explained in a previous chapter, these are
alloys of iron with not more than 2 per cent of carbon.
[Illustration:
HIGH CARBON TOOL STEEL (1.25 PER CENT C) AS CAST
(Magnification 70 diameters)
]
[Illustration:
LOW CARBON TOOL STEEL (.50 PER CENT C) ANNEALED
(Magnification 70 diameters)
]
[Illustration:
LOW CARBON TOOL STEEL (.50 PER CENT C) AS CAST
(Magnification 70 diameters)
]
[Illustration:
MEDIUM CARBON TOOL STEEL (.86 PER CENT C) AS CAST
(Magnification 400 diameters)
]
Carbon is the element the presence of which confers upon iron the
ability to harden when _cooled suddenly_ from a cherry-red heat, as by
quenching in water or oil. If the steel contains less than four-tenths
of one per cent of carbon it has little or no hardening power under this
treatment; but steel with six-tenths of one per cent or more of the
element, has the wonderful property of being slightly malleable when in
the annealed state, but extremely hard and brittle after this sudden
cooling—leads a dual life, so to speak.
[Illustration:
LOW CARBON TOOL STEEL (.50 PER CENT C) HARDENED
(Magnification 100 diameters)
]
At any time, hardened steel may be returned to its former condition of
softness by the well known process of annealing, wherein it is reheated
to the same cherry-red heat and _slowly cooled_.
At the will of the blacksmith or metal worker alternate hardening and
softening may be repeated a great many times without apparent
deterioration.
Various degrees of hardness also, may be obtained according to (1), the
percentage of carbon in the steel, and (2), the completeness and
suddenness of the cooling.
As considerable brittleness and internal strain in the metal necessarily
follow hardening, the hardness is usually “tempered” or “let down” by a
careful reheating to a much lower temperature, usually 425 to 550
degrees Fahrenheit. From this temperature a second quenching “fastens”
the temper at whatever of the original hardness the steel retains at the
temperature chosen by the smith for the second quenching. Much of the
brittleness is in this way relieved. The smith calls it “toughening” the
steel. Tools so treated are much less liable to break.
The steels that will harden (we will call them “carbon tool steels”),
range ordinarily from the .60 per cent carbon variety, used for hammers,
cold chisels, etc., to those containing 1.50 per cent of carbon which
are selected for razors, scalpels, and other tools requiring high
temper. Each one of these many grades is susceptible of a wide variety
of temper in the hands of a capable man, who must select his steel and
give to it the most desirable temper for the work for which the tool is
designed.
[Illustration:
MILD STEEL PIPE (.10 PER CENT C)
(Magnification 70 diameters)
]
Blacksmiths and other tool makers become extremely proficient in judging
steels and the proper temperature at which each should be hardened and
“drawn” (tempered). They judge temperatures solely by the color of the
steel when heated. Every five or ten degree change imparts a slightly
different shade as the steel grows hotter in the forge fire or cooler
when about to quench.
Observation of a good blacksmith at work and a few minutes’ conversation
with him about his “art” will give one greater knowledge and
appreciation of the carbon tool steels than volumes of writings
concerning them. Along with it will come more respect for the skill of
these clever men whose handiwork is never exhibited in salons and about
whom the world hears little, though indebted to them for a great measure
of its civilization and prosperity.
[Illustration:
HIGH CARBON TOOL STEEL IS EXTREMELY BRITTLE WHEN HARDENED AND HAS VERY
LITTLE MALLEABILITY WHEN ANNEALED
]
What and how much would be possible without machines and proper tools?
[Illustration:
QUARTER-INCH MILD STEEL PLATE WITH DOUBLE FOLD. FOLDED COLD WITHOUT
SLIGHTEST CRACK
]
About sixty years ago steels of much lower carbon content appeared. They
have been made softer and softer until we have what we now know as the
“mild” steels and even the almost or practically carbonless material
which we called “open-hearth iron” or “ingot iron” in a former chapter.
These have not the hardening property but they possess softness,
ductility and freedom from brittleness which the higher carbon steels
always lack. For such real evidences of our Twentieth Century
civilization as the great bridges, ships, buildings, etc., they are
indispensable, for they are easily cut, bent and otherwise worked into
shape, and they combine pliability with sufficient strength for the
service intended. Such steels are desirable, for when overloaded they
bend before they break, thus giving warning of the danger.
These mild and medium steels are of immense importance industrially. Of
the 31,000,000 tons of steel made in the United States during 1912
probably 99 per cent was of the soft and medium varieties.
It has been said that “the exception proves the rule.” Cementation steel
is the exception to the rule which we gave in Chapter VI that steel is
always melted during its manufacture.
If a thin piece of bar iron be packed in powdered charcoal and heated at
low red heat for some time, the metal, after cooling, will be found to
have acquired the hardening property. In other words by _absorption of
carbon_ it will have become steel with all of the characteristics of
that material. Neither the iron nor the carbon by which it was
surrounded have melted, yet in some way carbon has penetrated into the
iron and if the heating has been sufficiently long, carbon will be found
at the center of the bar. But _always_ there will be more carbon in the
outer layers of the bar than in those farther inside, i. e., it will be
found in diminishing amounts as we approach the center.
[Illustration:
SHELBY SEAMLESS STEEL TUBING CRUSHED ENDWISE
]
Just how and when the cementation process for making steel, to be now
described, was discovered is not known. It may have been the result of
the non-uniform working of the larger blast furnaces which were
developing in Continental Europe during the Thirteenth century. From the
German “natural steel” which was probably the steely product too rich in
carbon for the wrought iron which they intended to make and much too
poor in carbon to be the fluid cast iron which with the growing height
and heat of the blast furnace they later did make, may have come the
idea. More likely, a piece of thin wrought iron was accidentally left
imbedded in glowing charcoal until it had absorbed some carbon.
[Illustration:
A CRUCIBLE MELTING ROOM. “MELTING HOLES” ARE BENEATH THE SQUARE COVERS
ON THE FLOOR AT THE LEFT. NOTE THE NEW CRUCIBLES DRYING ON THE
SHELVES, AND THE INGOT MOLDS AT THE RIGHT
]
The first mention of cementation steel appears to have been by an
Italian metallurgist, Vannuccio Biringuccio, who, in 1540, described the
making of steel by heating billets of soft iron for a long time in
molten cast iron. The modern method, the heating of wrought iron in
powdered charcoal, was certainly known in the sixteenth century and this
method of cementation has been practiced in France, England, Belgium and
Germany since the seventeenth century.
[Illustration:
A SHEFFIELD (ENGLAND) CEMENTATION FURNACE
]
Reaumur, the Frenchman, whose process of making cast iron soft by
annealing bears his name and is still used in Europe, was the first to
study and understand to any extent the cementation process. Publication,
about 1722, of his complete directions for cementing iron gave great
impetus to the manufacture of steel by this process. Fate, however, was
unkind and his own nation, France, by reason of her small production of
suitable iron for the work, was unable to profit greatly through his
discoveries. Sweden, England and Germany were benefited to a much
greater extent.
During the early years many were the secret and wonderful mixtures and
compounds offered for this work, but of them all carbon in some form was
the only necessary element.
Finely divided or powdered charcoal or bone dust has been mostly used.
[Illustration:
HUNTSMAN CRUCIBLE FURNACE—ORIGINAL TYPE
]
[Illustration:
ONE TYPE OF OIL-FIRED CRUCIBLE FURNACE
]
Sheffield, England, steel makers, have been very successful in the
manufacture of cementation steel. Their usual method is to pack flat
strips of best Swedish Walloon iron in charcoal in rectangular stone
boxes about four feet wide, three feet high and fourteen feet long.
Alternate layers of small-sized charcoal and thin iron bars are piled in
these boxes until they are filled, the bars not being allowed to touch
one another. When full, top slabs are luted on to the boxes to make them
airtight.
Fire is kindled in the firebox below and the heat gradually raised until
furnace and boxes are cherry-red in color. This heat is maintained for
seven to eleven or more days, depending upon the hardness desired, i.e.,
the amount of carbon they desire absorbed. The furnace is closed and
allowed to cool slowly, which requires another seven or more days.
Upon unpacking the furnace the bars are found to be brittle and of a
steely fracture instead of the soft malleable material which was put in.
They have become high carbon steel.
Expert workmen are able to judge very closely the hardness of the steel
by looking at the fracture and they sort the bars in this way, piling
bars of similar hardness together.
[Illustration:
HUNTSMAN COKE-FIRED CRUCIBLE FURNACE—MODERN TYPE
]
Bars thus made show many blisters on the surface and the steel became
known as “blister steel” on this account. The reason for these blisters
was not discovered until along about 1864, when the well-known English
metallurgist, Percy, proved that the blisters were caused by the
chemical action of carbon on the slag contained in the wrought iron. The
gases formed produced the blistering of the bar. That this is the
explanation is proved by the fact that bars of mild steel or iron
without slag do not blister.
Blister bars heated to a forging heat and drawn out under the hammer or
rolled into bar steel are known as “spring steel”, or “plated bars.”
As in wrought iron manufacture, a cutting to length, repiling, heating,
welding and again drawing down by hammering or rolling produces much
more homogeneous and reliable steel. Piled and reworked steel of this
sort became known as “shear” steel because blades of shears for cropping
woolen cloth were always made in this way.
Many of us will recognize in the cementation process an extended “case
hardening.” Case hardening is very largely resorted to by iron and steel
workers, who in a few hours can give a hardened and long-wearing thin
outer layer of steel to a piece of iron or soft steel after it has been
forged or machined into the desired shape.
[Illustration:
SIEMEN’S GAS-FIRED CRUCIBLE FURNACE—REGENERATIVE SYSTEM
One pair of Checker-work Chambers, k. h., is being heated by the hot
outgoing flame and waste gases while the other pair is heating
incoming gas and air. They are worked alternately.
]
This shear steel was largely made and was quite satisfactory, until, as
described before, Huntsman, a Sheffield clock maker, conceived the idea
of melting together in a pot or crucible blister bars or bars of shear
steel. This he did to equalize the carbon content and give uniformity of
product which had never been attainable through the cementation process
alone.
From that date (1740) to this the crucible process has undergone only
minor alterations and to-day it produces the highest grades of steel
which we have. Practically all of the high grade tool steels are
produced by this process.
Nor has Huntsman’s form of furnace been greatly changed, as the
illustrations prove. Though gas and oil as well as coal are, in many
cases, used as the fuel, the general design of the furnace has remained
the same.
For a century crucibles were made from clay molded to form, slowly dried
and very carefully burned. Usually each steel maker made his own
crucibles. They could be used but three times, becoming so thin and
tender after use for three batches of steel that they were not safe for
a fourth. Graphite crucibles are now very largely used. They withstand
the severe heat much better and can be used five or six times. The
expense item for either clay or graphite crucibles is a large one.
[Illustration:
THE STALWART MELTERS
]
After filling with small pieces of blister or shear steel the crucibles
are entirely surrounded by coal or coke in the furnace pit. The fire is
so regulated that the steel is not too quickly melted. Fresh coal or
coke must be put in around the crucibles two or even three times.
When he thinks the steel should be molten, the expert attendant known as
the “melter” quickly removes the tight fitting cover of the crucible and
with an iron rod determines whether any unmelted pieces remain.
After complete melting the steel must be “killed,” else it will boil up
in the mold upon pouring and leave a spongy or insufficiently solid
“ingot” or block of steel. This “killing” of steel is a rather peculiar
phenomenon. It is accomplished by allowing the steel to remain quiet in
the furnace for another half hour or so. Undoubtedly the quieting is the
result of the escape of the gases or impurities which are contained in
the charge, and absorption of the chemical element, silicon, from the
walls of the crucible.
We have met this element, silicon, before in our metallurgical journey
and we will likely meet it several times again. To the metallurgist it
is secondary in importance only to carbon.
[Illustration:
PULLING THE CRUCIBLE
]
When the steel has been properly melted and killed it is ready to pour.
An assistant lifts the cover from the melting hole, the “puller-out”
seizes the crucible just below the bulge with circular tongs and pulls
it from the coke which surrounds it. The slag is skimmed off the top and
the steel poured into iron molds forming small “ingots,” usually from 2
to 4 inches square and two feet or more long.
Every part of the process, even the pouring, must be done with extreme
skill and care or the product suffers.
After liberation from their molds, the ingots are heated and either
rolled or hammered down to the sizes desired for tools, etc.
As stated before, crucible steel necessarily is an expensive material
both on account of high labor and crucible costs. For this reason, many
have resorted to the process used in the very small way mentioned for
the manufacture of Wootz steel—the melting of wrought iron bar or soft
steel in a crucible with carbon.
In the Wootz process chopped wood and green leaves were used. Nowadays
charcoal is substituted or there is added the proper amount of cast iron
to give the desired amount of carbon to the wrought iron or soft steel
charged. During the melting the iron takes up the charcoal and alloys
with it.
[Illustration:
“TEEMING” OR POURING INTO INGOTS. THE INGOTS LATER ARE FORGED OR
ROLLED INTO BARS FROM WHICH THE TOOLS ARE MADE
]
Proper amounts of silicon, manganese, and other beneficial materials are
also charged, which become either part of the alloy itself or have a
cleaning or fluxing action upon it.
Steels made in this way are practically, though perhaps not quite, as
good as steels made by melting together the properly selected
cementation bars. The method has come to be very generally used on
account of its directness and because it eliminates the long and
expensive preliminary cementation process.
When Bessemer and open-hearth steels made their appearance in the market
an attempt was made to use them instead of wrought iron as the base for
high grade crucible steels. Though seemingly pure enough, apparently
purer even than wrought iron, these metals were not able to compete with
wrought iron for this purpose. For some reason, not yet satisfactorily
explained, these new materials which are made in 15, 35 and 50–ton
batches, when used as a base, do not give as high quality tool steel as
puddled wrought iron, which is slowly and laboriously made in 500–pound
lots. Considerable of these materials are utilized but it is for a
somewhat lower grade of crucible steel.
For many years mild steels for castings have been quite largely made by
the crucible process. They are among the best but the crucible and labor
costs are usually too great to allow crucible steel castings to compete
in present markets.
CHAPTER VIII
BESSEMER STEEL
The “Manufacture of Malleable Iron and Steel without Fuel” was the
startling title of a scientific paper read in 1856 before the British
Association for the Advancement of Science. This was the announcement to
the world of Henry Bessemer’s invention of the process for making iron
and steel which led to the greatest commercial development the world has
seen.
To those of us who have had little or no experience along manufacturing
lines the announcement seems strange enough, but metallurgists,
engineers and manufacturers who know how serious is the matter of fuel
bills realize at once how revolutionary the claim of Bessemer must have
seemed to men of those days.
As occurs with so many new things the idea was scoffed at; Bessemer’s
scheme was one purporting to give “something for nothing” and—well, it
could not be.
It was ridiculous!
And why should it not have seemed strange when we consider that up to
that time fuel had been required in all metallurgical processes. In the
old Catalan furnace and the types that preceded it, in the Finery Fire,
the Walloon and the several other refining furnaces fuel had to be
provided without stint. The lowest proportion that seventy years of
experiment and practice had brought about in Cort’s puddling process was
one ton of coal per ton of iron, while the blast furnace required at the
least four-fifths of a ton of coke for each ton of pig iron produced.
[Illustration:
KELLY’S FIRST TILTING CONVERTER
]
Whether Bessemer, an Englishman of French descent, or William Kelly, an
American of Irish descent, of Eddyville, Ky., first conceived the idea
of the “pneumatic” process is a moot question. Considerable evidence
substantiates the claim that the latter first hit upon the scheme and
during the ten years between 1846 and 1856 had considerable success with
its development. Perhaps Bessemer had heard of Kelly’s experiments.
There is no proof that he did. Whether he did or not, the fact remains
that he quite independently and very fully developed the process in
England, and with great business sagacity and energy made it the success
that it is.
As fortune has withheld from Kelly and from this country credit which
was deserved, it is desirable to tell briefly the part which he had in
the development of this process that with a single furnace converts pig
iron into steel at the rate of a thousand tons in 24 hours and first
made mild steel available as a building material.
In 1846 Kelly, with a brother, bought the Suwanee Iron Works, near
Eddyville, Ky. After about a year they encountered the same difficulty
that charcoal iron manufacturers usually have encountered—the failure of
the supply of fuel. This difficulty Kelly, a better inventor than
business man, apparently had not foreseen. His business was threatened
unless some other way of refining his iron was found.
[Illustration:
CRUCIBLE WITH WHICH BESSEMER’S FIRST EXPERIMENTS WERE CONDUCTED
]
One day while watching the operation of his Finery Fire he noticed that
the blast of air from the tuyère made the molten iron where it impinged
very much whiter and apparently hotter than the rest. Like other iron
makers, he had always supposed that a blast of cold air chilled molten
iron.
It appears that Kelly was not long in surmising the truth. In a few days
he had rigged up a crude apparatus and made soft iron from which a
horseshoe and a horseshoe nail were fashioned by a blacksmith.
[Illustration:
FIXED CONVERTER OF 1856 WITH SIX TUYÈRES ABOUT THE SIDES
]
Being conservatives, Kelly’s customers were not slow in informing him
that they did not want iron made by anything other than the “good old
process” and he was obliged to accede to their demands or lose their
trade.
Like Galileo, however, he had not really surrendered. In the woods near
by he built and experimented with seven successive “converters,” as the
furnaces are called in which Bessemer steel is made.
Upon learning that Bessemer of England had been granted a United States
patent (1856), Kelly came before the patent office and proved that he
had several years before used the same process. The priority of his
invention was acknowledged, and a patent was granted to him also (1857).
[Illustration:
BOTTOM BLOWING TILTING CONVERTER
]
Financial troubles and finally bankruptcy handicapped him. However, the
Cambria Steel Co., of Johnstown, Pa., became interested and let him
experiment with his process at the company’s plant. Here in 1857 he
built his first “tilting” converter. His first public demonstration
resulted in failure and ridicule, but a few days later he was
successful. Steel makers bought interests in his patent, which at its
expiration in 1870 was renewed by the United States Patent Office, while
renewal of Bessemer’s patent was refused.
[Illustration:
IN 1858 BESSEMER ERECTED HIS FIRST CONVERTER OF THE FORM GENERALLY
USED TO-DAY
]
The Kelly Pneumatic Process Company, which was organized to operate
under Kelly’s patents, built a converter at an iron works at Wyandotte,
Michigan. Here the first pneumatic process steel ever made in this
country in other than an experimental way was “blown” in 1864.
Meanwhile Alexander L. Holley, an American engineer, had obtained for
another American company the right to manufacture steel here under
Bessemer’s patents. He built a plant at Troy, New York, which began
making steel in 1865.
[Illustration:
EVEN THE DETACHABLE BOTTOM—TO FACILITATE REPAIRS—WAS THOUGHT OF AND
PATENTED BY BESSEMER—1863
]
It was soon decided to merge the interests of the two companies and in
1866 this was done, the process thereafter being known as the Bessemer
Process. During the early years of the process here Holley became very
well known. As consulting engineer he designed practically all of the
Bessemer plants which were built during the first ten or fifteen years.
To the majority of the people of the United States to-day Kelly and his
parallel part in the great invention are practically unknown, and thus
not only he but the United States is without credit which should be
ours.
Fortunately Kelly did not entirely fail to profit financially as so many
times is the case with inventors. He received a total of about $500,000.
Bessemer’s return from his process is said to have approximated
$10,000,000 and he was knighted by the British sovereign.
More intimate details regarding Kelly and his work may be found in
_Munsey’s Magazine_ for April, 1906, where H. Casson gives information
which he received direct from several of the men who knew and worked
with Kelly.
While apparently not the originator of the process, Bessemer is without
any doubt entitled to most of the credit he received. There is no proof
that he had heard of Kelly’s experiments when he began his own or that
he was aided by Kelly’s discoveries. He worked out the details of the
process independently, as had Kelly, and it was Bessemer who put it on a
commercial basis.
As has occurred with other new processes Bessemer’s first licensees were
not particularly successful. When those who had bought the right to use
his process had failed in their efforts to use it, and become
discouraged as most of them did, he quietly bought back their rights and
went ahead with his development of the process. Perhaps no man ever
exhibited more perseverance in continuing experiments and development
under very discouraging conditions than did Henry Bessemer. He had
faith.
[Illustration:
SECTIONAL VIEW OF A MODERN CONVERTER SHOWING AIR DUCT AND TUYÈRES
]
He had a genius for invention and was thorough in his experimental work.
Practically no type of converter has since been brought out that he did
not think of and try, and the process has been modified in but one or
two important particulars in the years that have passed.
The essential part of the Bessemer process is the blowing of air through
molten cast iron to remove the metalloids by which cast iron differs
from steel and wrought iron, as has been explained before.
This being the essential point, and at first thought the lack of fuel
seeming so peculiar, we must describe what happens during the Bessemer
“blow.”
[Illustration:
POURING CHARGE OF MOLTEN PIG IRON INTO CONVERTER
]
Technically speaking, the metalloids are “oxidized.” Oxidation is the
chemical uniting of oxygen, generally from the air, which has 21 per
cent of this element, with another element or material such as iron,
silicon, carbon, wood, coal, etc. If the oxidation is slow as in the
“rusting” of iron, the resulting heat dissipates as fast as it is
generated and the change is hardly noticeable. If, however, the reaction
occurs rapidly and with vigor enough, we say that the material “burns.”
The latter sort of oxidation is what we call “combustion.”
The affinity between the metalloids and oxygen has been noted by us
before, but in those cases most of the oxygen came from a different
source.
In the wrought iron process most of it was furnished by the iron ore or
scale which was stirred into the metal, or by the slag which covered the
“bath.” In the Bessemer, or as it was first known in America, “Kelly’s
air blowing process,” the oxygen of the air blown through the molten
metal directly oxidizes or burns out the carbon, silicon, and manganese.
The extremely rapid oxidation of these furnishes the heat.
The iron, then, furnishes its own fuel and _no outside combustible is
needed_.
How can this be?
In every ton of molten cast iron there are approximately 70 pounds of
carbon, 25 pounds of silicon, and 15 pounds of manganese or a total of
about 2000 pounds of these metalloids in the fifteen-ton charge of
molten metal which goes into the ordinary steel plant converter.
We know that if burned in a furnace this ton of high grade fuel would
generate much heat. Burned _inside_ of the mass of molten metal it
generates exactly that same amount of heat and the heat is applied with
such rapidity, directness and efficiency that the molten iron which had
a temperature of 2300° F., say, when charged, in nine or ten minutes has
become steel with a temperature of about 3000° F. simply through this
rapid oxidation of its 4 to 6 per cent of metalloids.
How the blast under 15 to 30 pounds per square inch is applied through
little nozzles in the bottom of the modern “converter” and the several
types of vessels with which Bessemer experimented in the course of his
investigations are shown in the illustrations.
Nor is it necessary that the air be blown through the metal. Air blown
upon its surface accomplishes practically the same purpose, and in many
of the steel foundries of to-day smaller converters of this
“surface-blown” type are used for producing steel for castings. The
large steel plants, however, use the larger “bottom-blown” converter.
Two or three of these vessels, working with proper metal from the
“mixer,” produce an immense tonnage of steel each 24 hours.
The “mixer” is quite necessary. It is a large vessel or furnace holding
and keeping hot from 75 to 300 or more tons of metal from the blast
furnace. It mixes and equalizes irons of various compositions, so that
the converters have the advantage of uniform and hot metal with which to
work.
In addition it is made to perform a “refining” service. By mixing into
the metal a quantity of manganese, considerable of the sulphur present
(a deleterious substance) is removed.
The fifteen or twenty minute blowing of 15 tons of metal in the big
egg-shaped converters of a steel plant presents a spectacle which, when
once observed, will never be forgotten.
One sees a little “dinky” engine come shooting into the converter
building with its ladle of molten iron from the “mixer.” With America’s
time saving routine not a single minute is lost while emptying the metal
into the converter, now in a horizontal position. Almost before the
ladle is out of the way, the converter swings to the upright position
with the blast already on, for otherwise the metal would flow into the
tuyère holes at the bottom.
[Illustration:
COMPARISON OF INGOTS
A. From Four Pot Crucible Furnace: Each Heat 400 Pounds in 4 Hours or
100 Pounds an Hour, Each Heat Pours 4 Ingots 3 × 3 × 36″. B. From
Fifteen Ton Bessemer Converter: 30,000 Pounds in 20 Minutes or
90,000 Pounds an Hour, Each Heat Pours 6 Ingots 19 × 20 × 62″. C.
From Fifty Ton Open-Hearth Furnace, 100,000 Pounds in 8 Hours or
12,500 Pounds an Hour, Each Heat Pours 6 Ingots 24 × 32 × 72″.
]
Reddish-brown smoke and a shower of sparks come from the converter.
These gradually develop into a flame.
The blast shows considerable partiality in selecting for its first
attention the metalloids silicon and manganese, in preference to the
iron itself or any other of the metalloids present. After from three to
five minutes half of the silicon and manganese have been burned out. If
the temperature of the metal and other conditions have become right the
carbon then begins to burn. This gives a change in the nature of the
flame which becomes large and of a dazzling whiteness.
The metal is hot—very hot—so much so that pieces of cold steel often
must be dropped in to cool it somewhat. This is known as “scrapping” the
charge.
An experienced blower can judge through every period of the operation of
the condition of his metal and just how things are progressing.
After some minutes the flame begins to waver and later “drops”; i.e.,
there is scarcely a flame at all. This signal, which is very definite to
an experienced man, cannot be lightly disregarded. Oxygen has affinity
for iron as well as for the metalloids and it is only because of its
greater love for silicon, manganese and carbon that it has thus far
largely neglected the iron. With the metalloids mentioned out of the
way, as they are when the drop occurs, the iron will begin to burn. Were
the “blowing” continued we would shortly have no iron left, but in its
place a mass of iron oxide and slag.
Thus we see that during the first minutes of the blow, more than
one-half of the silicon and manganese are burned. The remainder of these
and all of the carbon are removed in the subsequent five or six minutes.
At the end of this short blowing period we have practically pure iron.
[Illustration:
TWO CONVERTERS IN OPERATION AND A THIRD POURING
]
The metal is not yet in condition to pour well, however, largely because
of the dissolved air and gases which it holds. Something akin to the
“killing” of the steel which we observed in the crucible process must be
accomplished or ingots from it will be spongy. And, having practically
no carbon, it is not yet “steel.”
Bessemer, knowing that the finished steel should contain carbon, tried
to stop the blow long enough before the drop of the flame to leave
exactly the desired amount of this element. He found this difficult to
do and therefore uncertain. It was found to be far better to blow until
the drop of the flame and then put back sufficient carbon to give the
proper composition.
An English metallurgist named Mushet discovered that addition of
manganese ridded the metal of injurious gases and oxides and what is
known as “red-shortness.” After a period of difficulty without it
Bessemer acknowledged the necessity of manganese and adopted its use. It
had before this been used in crucible steel.
Upon turning down the converter at the drop of the flame, the blast is
turned off and a smaller ladle is run in on a track above. This brings a
molten mixture of irons, usually known as “spiegel” or “spiegeleisen”
which contains just enough carbon, manganese and silicon to give to the
whole of the molten metal in the converter the metalloids needed to make
of it steel of the composition desired. This addition also accomplishes
the “deoxidation” of the metal. By deoxidation we mean that the iron is
relieved of the oxygen and gases which have remained as a result of the
blast. This is necessary in order to give proper fluidity for pouring
and the best physical properties to the finished steel.
After “recarburization,” as this addition of manganese-silicon-carbon
metal is called, the steel and slag are quickly poured out into a ladle
waiting below from which the steel is “teemed” (i.e., poured), through a
“nozzle” or hole in the bottom into ingot molds arranged on trucks on
the railroad track which runs through the building.
[Illustration:
TEEMING THE FINISHED STEEL INTO THE INGOT MOLDS
]
When the molds have been filled and a strong crust develops on the steel
the cars are pulled to the “stripper” where the molds are removed,
leaving the white-hot ingots standing on the cars.
The ingots mentioned in the chapter on Cementation and Crucible Steel
were usually small enough that one pot of 100 pounds of metal filled the
mold. A four pot furnace therefore produced 400 pounds. Now for the
first time, we are talking in _tonnage_ figures. Instead of a batch of
steel making four 3″ × 3″ × 36″ ingots of 100 pounds each, the ordinary
“heat” of Bessemer steel from the 15–ton converter gives six or seven
ingots about 18″ × 20″ × 60″ in size. Each of these weighs about two
tons. The total is 30,000 pounds.
From the stripper the ingots go to the gas-fired soaking pits where the
molten interiors of the ingots gradually solidify by cooling while the
outer crusts are reheated. After equalizing the temperatures of
exteriors and interiors in this way, the ingots are white-hot again and
ready for rolling.
[Illustration:
MOLDS BEING STRIPPED FROM INGOTS
]
The purpose for which the steel is intended, of course, determines the
shapes and sizes into which the ingots are rolled. For rails they are
rolled down directly, each ingot making about six rails, of
thirty-three-foot length. For most other purposes the ingots are rolled
in the slabbing mill into billets or slabs which are of intermediate
shapes and sizes which are reheated and further rolled down into axles,
bars, shapes, wire or other products.
Meanwhile the converter which we saw emptied has not been idle. The
American steel engineer has genius for mechanical efficiency and all
parts of a great steel plant are so co-ordinated that enormous
quantities of material can be handled with not a moment lost between
trips. Almost before the ladle of steel had swung away from the
converter’s mouth, any remaining slag was dumped from the converter by
further tipping, the vessel returned to receiving position and the ladle
car, back again from the mixer, poured in the next charge.
Thus blow after blow is made without loss of time.
Repairs are allowed to take no longer than is absolutely necessary. When
the lining around the tuyères gets too badly cut by the action of the
air and metal the bottom is removed, another one is quickly substituted
and the steel making goes on.
Blowers, ladlemen, cranemen, pourers, patchers, vesselmen, sample boys
and the other workmen are relieved by their “partners” at the end of
each shift, each man of necessity working until relieved—twelve,
twenty-four, or even thirty-six hours, for there must be no delay. So
day and night, through the entire week from Monday morning at six, when
they begin, until the next Sunday morning at six, when the plant shuts
down for a brief spell, the converters go on turning out three heats per
hour or four to five hundred per week each.
It has been mentioned that most of Bessemer’s first licensees failed
with the new process. The reasons for this were various, but one in
particular was the attempt of many to use metal of high phosphorus
content. Bessemer soon discovered that no phosphorus was removed during
the “blow” and that, as phosphorus in quantity over one-tenth of one per
cent was detrimental to steel, it was necessary to use raw material
which had little of this element.
This could be done, but it barred many pig irons otherwise good.
Fortunately Swedish and many English irons had low phosphorus. Germany’s
vast beds of high phosphorus ores, however, were useless for the
purpose.
For twenty years this situation existed, during which time many
metallurgists endeavored to make the process applicable to irons which
contained high phosphorus. After long study and many experiments the
problem was solved by Sidney Thomas, an English metallurgist. With a
cousin, Percy Gilchrist, he made hundreds of blows with a toy converter
holding only eight pounds of iron.
Bessemer’s linings had been of sand, clay and other earths which are
known chemically as “acid” materials. By using “basic” materials such as
limestone, dolomite, etc., for the converter lining and additions of
limestone or burnt lime to the charge before and during the blow to make
and keep the slag “basic,” Thomas was able to make the phosphorus burn
after the carbon had been removed. Therefore, a three or four minute
“after blow” following the “drop” of the carbon flame took out the
phosphorus,—again, with generation of heat.
So there are two varieties of the process—the acid Bessemer and the
basic Bessemer, but the former, only, is used in this country as we have
few high phosphorus ores. The analogous open-hearth processes, which are
next to be described, are both used in this country with the basic
open-hearth greatly in the lead.
However, the basic Bessemer process of Thomas and Gilchrist is credited
with making Germany’s great industrial development possible.
════╤════════════════════════════════════╦═══════════════════════════════════
Year│ TABLE NO. 1 ║ TABLE NO. 2
│ Materials Used for Rails[6] ║ Total Steel Made by Processes[6]
────┼──────────┬────────────┬────────────╫─────────────┬────────────┬────────
│ Wrought │ Bessemer │Open-Hearth ║ Bessemer │Open-Hearth │Crucible
│ Iron │ Steel │ Steel ║ Steel │ Steel │ Steel
────┼──────────┼────────────┼────────────╫─────────────┼────────────┼────────
1849│ =21,710=│ │ ║ │ │
1850│ =39,360=│ │ ║ │ │
1855│ =124,000=│ │ ║ │ │
1860│ =183,000=│ │ ║ │ │ No Data
1865│ =318,000=│ │ ║ │ │
1867│ =410,000=│ 2,280│ ║ =2,679=│ │
1868│ =445,970=│ 6,450│ ║ =7,589=│ │
1869│ =521,370=│ 8,620│ ║ =10,714=│ 893│
1870│ =523,000=│ 30,360│ ║ =37,500=│ 1,339│
1875│=448,000=↘│ 260,000│ ║ =335,000=│ 8,080│ 35,180
1880│ 441,000│ ↘=852,000=│ 12,160║ =1,074,000=│ 110,850│ 64,660
1885│ 13,000│ =959,000=│ 4,280║ =1,515,000=│ 133,000│ 57,600
1890│ 14,000│ =1,868,000=│ 3,590║ =3,689,000=│ 513,000│ 71,200
1895│ 5,810│ =1,300,000=│ 700║ =4,909,000=│ 1,137,000│ 68,700
1900│ 695│ =2,384,000=│ 1,330║ =6,685,000=│ 3,398,000│ 100,500
1905│ 318│ =3,192,000=│ 183,000║ =10,941,000=│ 8,971,000│ 102,200
1906│ 15│ =3,391,000=│ 186,000║ =12,276,000=│ 10,980,000│ 127,500
1907│ 925│ =3,380,000=│ 253,000║=11,668,000=↘│ 11,550,000│ 131,000
1908│ 71│ =1,349,000=│ 572,000║ 6,117,000│↘=7,837,000=│ 63,600
1909│ │ =1,767,000=│ 1,257,000║ 9,331,000│=14,494,000=│ 107,400
1910│ 230│=1,884,000=↘│ 1,751,000║ 9,413,000│=16,505,000=│ 122,300
1912│ │ 1,100,000│↘=2,105,000=║ 10,328,000│=20,780,000=│ 121,500
1913│ │ 818,000│ =2,528,000=║ 9,546,000│=21,600,000=│ 121,200
1914│ │ 324,000│ =1,526,000=║ 6,221,000│=17,175,000=│ 89,900
1915│ │ 327,000│ =1,775,000=║ 8,287,000│=23,679,000=│ 113,800
1916│ │ 440,000│ =2,270,000=║ 11,059,000│=31,415,000=│ 129,700
────┴──────────┴────────────┴────────────╨─────────────┴────────────┴────────
Footnote 6:
In United States—long tons of 2,240 pounds.
The well-known “Thomas Slag” which is in demand as a fertilizer on
account of its phosphorus content is the by-product of the basic-lined
converter.
An idea of what the invention of the Bessemer process meant to railroad
development alone may be gained by studying for a moment Table No. 1.
Wrought iron was our first material for rails, but, being very soft, it
did not give long service. But a short time was required for Bessemer
steel to displace it for rails when steel became available. The greater
uniformity, strength and hardness of the alloy gave such excellent
wearing properties that few rails of iron were laid after the year 1880.
During recent years rails have been made of greater and greater strength
and hardness to keep pace with the fast increasing weight, speed and
frequency of railroad trains, steel being susceptible to much
modification of properties.
Now it appears that Bessemer steel is giving way to other products which
show even superior properties.
What happened in the railroad world to a great extent has happened
elsewhere, as the figures of Table No. 2 show. They are a barometer
which indicates what has been our industrial development and our advance
in civilization.
CHAPTER IX
THE OPEN-HEARTH PROCESS
Bessemer’s was a wonderful process, but the time seemed to be ripe for
great development along metallurgical lines, and the method of
converting pig iron into steel which he devised soon had a competitor
which was destined eventually to take the lead in steel production. Many
years passed before the tonnage turned out annually by Bessemer’s
process was equaled by that of the new, but as shown in the last chapter
the Siemens-Martin or open-hearth process in 1907 produced the greater
tonnage. It has since retained its lead and probably will continue to do
so.
As far back as 1845 John Marshall Heath took out a patent for a process
for making steel patterned after the old puddling process. In a way he
may therefore be said to have devised or forecast the open-hearth
process, but because of the great obstacles that had to be surmounted in
getting a furnace that would fulfill the requirements he was unable to
carry out his scheme. You will remember that in the puddling furnace the
purified metal became pasty because of its high melting point. Because
of the great heat required it was not until the invention of the
regenerative system by C. W. Siemens in 1860 that the open-hearth
process was possible. Siemen’s furnace was the first one that could keep
the iron molten. It was in Birmingham, England, that the first
successful open-hearth furnace was used.
[Illustration:
EARLY TYPE OF GAS PRODUCER, REGENERATORS, AND OPEN-HEARTH FURNACE.
COURSE TAKEN BY AIR, GAS, AND PRODUCTS OF COMBUSTION ARE PLAINLY
SHOWN, AS ARE THE VALVES THAT REVERSE DIRECTION OF FLOW
]
While not as speedy nor as prolific a producer as the Bessemer process
and far less spectacular, the open-hearth has several advantages.
The acid Bessemer was always handicapped because pig iron with less than
0.1 per cent of phosphorus was necessary. The majority of ores carry
more than this amount. The basic Bessemer requires pig iron containing
not less than 2 per cent of phosphorus. The vast quantities of material
which contain percentages of phosphorus between these limits are useless
as far as the Bessemer process is concerned.
To be successfully used the pig iron must be further limited as to
composition. It must have sufficient silicon, manganese, and carbon to
give the heat required for Bessemerizing, as the burning of these
metalloids has to be depended upon for the conversion to steel and to
give proper fluidity to the finished alloy.
Then, too, the large amount of air forced through to a certain extent
“over-oxidizes” the bath and some of the gases are mechanically retained
by the steel no matter how complete the deoxidation. There also is loss
of metal due to unavoidable “spitting,” for the rapid streams of air
mechanically carry some metal and slag with the flame out of the vessel.
On the other hand, for the open-hearth process can be used pig iron of
widely varied character and composition and, further, large percentages
of low-priced steel scrap can be utilized in the charges; as no air is
blown through the metal and little comes in contact with it, the
conversion takes place quietly and smoothly and with much less loss by
oxidation, the yield of steel usually being from 90 to 97 per cent of
the metal charged as against 83 to 87 per cent which is the yield by the
Bessemer process; besides giving less over-oxidation and gases in the
metal, the slowness of the conversion is an advantage, as control is
very easy, and, when desired, samples for test may be taken. From his
tests the melter can be quite certain when he taps out the steel that it
is of the composition desired.
[Illustration:
SECTION THROUGH TYPICAL STATIONARY OPEN-HEARTH FURNACE, SHOWING
CONSTRUCTION OF FURNACE, LINING, BATH AND AIR AND GAS PORTS
]
The melting in an open-hearth furnace is done largely by indirect or
radiated heat, and it is not intended that the flame shall impinge too
directly upon the surface of the bath.
[Illustration:
BOXES OF STEEL SCRAP AND ELECTRIC CHARGING MACHINE IN FRONT OF
CHARGING DOORS AT REAR OF FURNACES
]
Except during the melting down of the pig iron and other materials
charged in the furnace, the flame and air take little part in the actual
elimination of the metalloids. Their main function is to furnish the
heat necessary. Being used so indirectly—mostly by radiation from the
roof and walls—very great heat must be used and much would be wasted if
special precautions were not taken to save it. The bath must be kept hot
enough to remain molten after purification of the metal, which we were
unable to accomplish in the wrought iron puddling furnace.
Under each end of the rectangular furnace are two chambers built up with
checker-work of fire brick. These sets are in duplicate and each has one
chamber for air and one for gas.
[Illustration:
CHARGING MACHINE WITH BOX OF SCRAP HALF WAY INTO FURNACE
]
Thus an open-hearth furnace will be seen to occupy a sort of hollow
square, the furnace proper forming one side, the regenerative chambers
two sides, with the chimney and flues the remaining side. “Reversing”
valves force the incoming gas and air to travel each through its
respective hot regenerating chamber up through the ports and into the
furnace where they unite and burn with a very hot flame. The hot gases
leave through similar ports in the other end of the furnace and on their
way to the chimney heat the checker-work in the regenerative chamber.
Every fifteen or twenty minutes the valves are reversed and the
direction of flow is changed. In this way the incoming gas and air are
preheated and in the furnace burn with a very much hotter flame than
would cold gas with cold air. No blast is required, the draft caused by
the chimney being sufficient.
For protection of the roof from the great heat developed and the metal
of the bath from too great oxidation, the air ports usually are located
above the gas ports. The streams of air, while protecting the roof from
the flame, at the same time are prevented from directly impinging upon
and too strongly oxidizing the metal of the bath.
The diagrammatic sketches given show roughly a furnace, regenerative
chambers, ports, etc.
[Illustration:
CHARGING “HOT” METAL
]
The original intention was to melt pig iron and reduce it; i. e., burn
out the silicon, manganese, and carbon by action of the flame and
addition of iron ore. This was the process worked out by Siemens in
England. In France, P. and E. Martin altered the method by diluting
molten pig iron in the Siemens furnace by melting and dissolving in it
steel scrap. It was soon found that a combination of the two methods was
better than either one alone and the open-hearth process acquired its
name—the Siemens-Martin—in this way.
In the United States about 20,000,000 tons of steel are made annually by
the basic open-hearth process while only 1,100,000 tons are produced by
the acid open-hearth process.
The two processes are practically the same except that by the basic
process the phosphorus as well as the silicon, manganese, and carbon are
reduced or eliminated. In order to take out the phosphorus, additions of
lime (i. e., calcium oxide or calcium carbonate) are made just as
occurred with the basic Bessemer process.
Should we use lime in a furnace having an acid lining, much of the lime,
which is a “base,” would react with the “acid” (silica) bricks of the
lining, and, becoming neutralized, would not do its work. So, as in the
basic Bessemer process, we here have to use either “basic” or “neutral”
lining.
The material generally used is burnt magnesium carbonate which is known
as “magnesite.” Dolomite, which is a combination of the carbonates of
calcium and magnesium, is sometimes used. Chrome bricks, the usual
neutral material, are rather too expensive for extensive use. The best
magnesite comes from Austria and is usually not very cheap. As acid
materials (those of silica or clay) are cheaper and mechanically
stronger, a compromise is ofttimes effected by using basic materials for
the furnace bottom and acid bricks for the sidewalls and roof. A few
rows of chrome bricks may be put in to form a neutral dividing line just
at and above the edge of the bath where the action of the slag is the
most severe. It also serves to keep the basic and acid materials apart
and from reacting with each other.
At the commencement of charging, limestone or sometimes burnt lime is
shoveled in upon the bottom or “hearth” of the white-hot furnace.
When cold metal is charged, the pigs of iron are conveyed into the
furnace by the melter and his helpers by means of long handled flat iron
tools called “peels.” This is followed by charging some or all of the
scrap or iron which is to be made a part of the charge.
Even in the smaller 15 or 25–ton furnaces hand charging takes a great
deal of time, sometimes as much as six or eight hours, and the labor
cost as well as the heat loss is therefore excessive. Modern machine
charging which requires not more than an hour is therefore highly
desirable.
[Illustration:
ROW OF OPEN-HEARTH FURNACES SHOWING PIT OR TAPPING SIDE
]
During the melting down of the pig iron with the scrap that has been
charged, the air and flame burn out about half of the silicon and
manganese of the metal. To remove the remainder of these and the carbon
of the charge, additions are made from time to time of sufficient ore to
keep the bath “boiling.” This phenomenon results from the giving off of
carbon monoxide gas formed from the oxygen of the iron ore and the
carbon of the metal, just as happened when the puddler in the
manufacture of wrought iron used iron ore in his furnace. The covering
of slag which forms and protects the bath from the flame undoubtedly
transfers oxygen from the furnace gases to the bath and this helps to
burn out the carbon.
The lime charged unites with the phosphorus of the iron and takes it
into the slag which covers the bath. If necessary, further additions of
lime may be made from time to time during the melting and the “working
down” (elimination of the metalloids) of the charge. As long as the slag
is kept basic it retains the phosphorus, but should it turn acid the
iron of the bath would take the phosphorus back again.
These reactions are all chemical, just as much so as are the burning of
wood and coal and the thousands of reactions which are brought about in
chemical laboratories.
Additions of ore are made from time to time and the bath rabbled.
Samples are taken now and then with a long handled iron spoon or ladle
and these are poured into molds to form small bars of steel, which,
after quenching, are broken.
[Illustration:
OPEN-HEARTH FURNACE “TAPPING”
]
The melter has become very proficient in judging the composition of the
metal of the bath from the fracture of these broken test pieces. By
means of the samples taken he watches the elimination of the metalloids.
When he thinks the reactions have progressed far enough he takes a last
sample which is rushed to the chemist who makes a hurried “control”
analysis for carbon and phosphorus, the metal being held in the furnace
meanwhile. If the results of this analysis show the bath to have the
desired composition the steel is poured. If the reactions have not been
complete, the chemist’s report shows that the carbon and perhaps the
phosphorus are still too high, in which case the charge must be still
further worked down.
Some melters are able to make fairly uniform and satisfactory steel
without a chemist, but for best results a chemical laboratory is
desirable.
When ready to tap, the big ladle is suspended from a crane under the
spout of the furnace. With a tapping bar the plug of clay is removed
from the tap hole and the molten steel gushes out into the ladle. The
slag which has covered the bath is the last to drain out. Many times
this will overflow the ladle, making a beautiful cascade as it pours
over the sides all around to the floor beneath. Especially at night is
this a glorious sight.
[Illustration:
TEEMING THE STEEL INTO INGOT MOLDS
]
Recarburization is not done to the same extent as it is in the Bessemer
process. As the open-hearth elimination of carbon is slower and under so
much better control, the furnace usually is tapped when the carbon has
been reduced to the percentage desired in the finished steel. When it is
necessary to add carbon it is done sometimes by adding pig iron to the
bath and sometimes by throwing a weighed amount of coal or coke in the
ladle as the steel is going in. Molten iron and steel have strong
appetites for carbon and dissolve it very readily. Ferro-manganese is
used to prevent red-shortness and to deoxidize the metal. This also is
usually put into the ladle as too much loss would occur were it added in
the furnace.
While the furnace is again being charged through the charging doors at
the rear, the steel is teemed through the nozzle of the big ladle into
the waiting ingot molds. These go to the stripper, to the soaking pits,
and then to the rolls of the blooming mills just as did the Bessemer
ingots.
[Illustration:
AT THE “STRIPPER”
]
In the acid-lined furnace no attempt is made to reduce the phosphorus.
It would be futile. Therefore the materials charged must be very low in
phosphorus and sulphur. No lime additions are made, the flame simply
melts down the pig iron and scrap, the iron oxide later is added from
time to time to keep up the boil until the test bars show that the
carbon as well as the silicon and manganese have been eliminated as
fully as is desired. The metal is then tapped as described above.
Three or more hours are usually required to melt down cold charges. The
elimination of the remainder of the silicon, manganese, and the carbon
requires about four or five hours more. So for each heat the open-hearth
furnace requires from eight to twelve hours, depending largely upon the
speed of charging and melting.
Of late years the difficulties attending the use of molten metal from
the blast furnace in place of cold pig iron have been largely
surmounted. The use of uniform metal from the “mixer,” which was
described in the article on the Bessemer process, has aided the
open-hearth process also. Of course, when molten metal is added none of
its silicon and manganese is reduced by the flame as occurred with the
cold metals during the melting down, so the molten metal charged is
usually low in these elements to compensate. By use of “hot” (molten)
metal the time necessary to produce a “heat” of steel is considerably
shortened.
The first and perhaps the majority of furnaces yet building are
“sta
Read full text (200,001 characters)
Fields
| author | La Verne W. Spring |
|---|---|
| language | English |
| chars | 492220 |
| source_url | https://www.gutenberg.org/ebooks/73090 |
Cite this record
MLA
"Non-technical chats on iron and steel, and their application to modern industry." Project Gutenberg, n.d., https://gutenberg.go-v.org/record/73090.
Chicago
"Non-technical chats on iron and steel, and their application to modern industry." Project Gutenberg. n.d.. https://gutenberg.go-v.org/record/73090.
APA
Project Gutenberg. (n.d.). Non-technical chats on iron and steel, and their application to modern industry. https://gutenberg.go-v.org/record/73090